journal article·2022-08

How to accelerate natural weathering of polymeric photovoltaic backsheets – A comparison with standardized artificial aging

Bettina Ottersböck, Gernot Oreski, Gerald Pinter

Publisher page

Abstract

The weathering performance of polymeric backsheets is most accurately assessed by outdoor exposure to natural weathering and examination of their performance characteristics by observing changes in properties. The main drawback of natural weathering is the long exposure time. Therefore, also existing qualification tests for photovoltaic (PV) components suggest accelerated artificial aging tests. This should lead to similar materials degradation as long-term outdoor exposures cause. However, it is necessary to establish connections between field performance of polymer products and accelerated materials durability testing in order to better predict the service life of a polymer product. Therefore, the main focus of this work was to evaluate the effect of natural and artificial aging on multilayer backsheet films for PV modules. For this reason, different backsheet films were naturally and artificially aged. Subsequently the optical, chemical, mechanical and thermal properties were characterized. In general, only some changes in properties after up to 3000 h of accelerated aging can be correlated with natural weathering for 2.5 years. The degradation mechanism of the polymeric part during natural weathering has to be considered when trying to simulate natural aging conditions in order to choose the right parameters for artificial aging. Thus, the right test design for artificial aging tests is highly important, as well as the consideration of the degradation mechanisms when trying to simulate natural aging conditions.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Photovoltaic System Optimization Techniques · Silicon and Solar Cell Technologies · Photovoltaic Systems and Sustainability

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (44)

Show source-provided references
1. Moisture transport, adhesion, and corrosion protection of PV module packaging materials10.1016/j.solmat.2006.04.003 ↗
2. 2014
3. Degradations of silicon photovoltaic modules: a literature review10.1016/j.solener.2013.07.005 ↗
4. Study on the degradation of different types of backsheets used in PV module under accelerated conditions10.1016/j.solmat.2013.09.036 ↗
5. Reflection and durability study of different types of backsheets and their impact on c-Si 5PV6 module performance10.1016/j.solmat.2015.11.038 ↗
6. Review of degradation and failure phenomena in photovoltaic modules10.1016/j.rser.2022.112160 ↗
7. Aging mechanisms of polymeric films for PV encapsulation10.1016/j.solener.2005.02.008 ↗
8. Ultra-violet degradation behavior of polymeric backsheets for photovoltaic modules10.1016/j.solener.2014.06.027 ↗
9. Influence of the environment during a photodegradation of multilayer films10.1002/app.44075 ↗
10. Relation between degradation of polymeric components in crystalline silicon PV module and climatic conditions: a literature review10.1016/j.solmat.2018.12.027 ↗
11. A comparison of key PV backsheet and module performance from fielded module exposures and accelerated tests10.1109/JPHOTOV.2014.2305472 ↗
12. Degradation of photovoltaic backsheets: comparison of the aging induced changes on module and component level10.1002/app.42093 ↗
13. Comparison of different microclimate effects on the aging behavior of encapsulation materials used in photovoltaic modules10.1016/j.polymdegradstab.2017.03.010 ↗
14. Degradation of photovoltaic backsheets: comparison of the aging induced changes on module and component level10.1002/app.42093 ↗
15. Wypych · 2008
16. A comparison of key PV backsheet and module performance from fielded module exposures and accelerated tests10.1109/JPHOTOV.2014.2305472 ↗
17. Error analysis of aged modules with cracked polyamide backsheets10.1016/j.solmat.2019.110194 ↗
18. Correlation study of damp heat and pressure cooker testing on backsheets10.1002/app.44230 ↗
19. E. Parnham, A. Seaman, A. Whitehead, W. Brennan, E. Ashford, Yellowing of PV backsheets in accelerated tests can be used as a realistic indication of possible field failures-fact or fiction?, in: 32nd European Photovoltaic Solar Energy Conference and Exhibition.
20. 2005
21. Comparison of accelerated UV test methods with Florida exposure for photovoltaic backsheet materials EU PVSEC 2017
22. IEC TS 62788 Measurements Procedures for Materials Used in Photovoltaic Modules-Part 7-2: Environmental Exposures - Accelerated Weathering Tests of Polymeric Materials.
23. Understanding backsheet durability through field studies and accelerated stress testing
24. Properties and degradation behaviour of polyolefin encapsulants for photovoltaic modules10.1002/pip.3323 ↗
25. DIN, Normausschuss Kunststoffe (FNK), DIN EN ISO 4892-2 - Kunststoffe - Künstliches Bestrahlen Oder Bewittern in Geräten: Teil 2: Xenonbogenlampen.
26. 2006
27. Fluorescent UV instrument
28. Aging characterization of multi-layer films used as photovoltaic module backsheets
29. Structure and basic properties of photovoltaic module backsheet films10.1016/j.solmat.2015.09.060 ↗
30. Monitoring the degradation of stabilization systems in polypropylene during accelerated aging tests by liquid chromatography combined with atmospheric pressure chemical ionization mass spectrometry10.1016/j.polymdegradstab.2013.06.015 ↗
31. Field study and analysis of backsheet degradation in 450MW+ PV installations
32. PV array differential backside exposure conditions: backsheet degradation and site design
33. Differential degradation patterns of photovoltaic backsheets at the array level10.1016/j.solener.2018.01.072 ↗
34. Hu · 2016
35. Thermo-mechanical characterisation of fluoropolymer films for concentrated solar thermal applications10.1016/j.solmat.2014.08.013 ↗
36. Natural and artificial weathering tests of polymer films used in solar applications
37. Encapsulation of PV modules using ethylene vinyl acetate copolymer as a pottant: a critical review10.1016/0927-0248(95)00150-6 ↗
38. The influence of the additive composition on the photochemical degradation of EVA
39. 6 - degradation processes and mechanisms of encapsulants
40. Hydrolysis kinetics of condensation polymers under humidity aging conditions10.1016/j.polymdegradstab.2013.04.001 ↗
41. The effect of ultraviolet stabilizers on the photodegradation of poly(ethylene terephthalate)10.1016/S0141-3910(01)00214-2 ↗
42. 2015
43. Study of hygrothermal ageing of glass fibre reinforced PET composites10.1016/j.polymdegradstab.2005.01.025 ↗
44. Ehrenstein · 2004