Influence of emitter position of silicon heterojunction photovoltaic solar cell modules on their potential-induced degradation behaviors
Source abstract
Abstract
Abstract Potential-induced degradation (PID)-test results of modules fabricated from the rear- and front-emitter silicon heterojunction (SHJ) solar cells were compared to clarify the influence of the emitter position of SHJ photovoltaic (PV) cell modules on their PID behaviors. The PID tests were performed by applying a bias of −2000 V to the shorted interconnector ribbons from the front surface of the cover glass, at 85 °C. In the initial stage, both modules showed the same degradation characterized by a reduction in the short-circuit current density (Jsc). After the first-stage degradation, the rear-emitter SHJ PV modules exhibited subsequent degradation characterized by a significant reduction in the Jsc and open-circuit voltage (Voc), due to the enhancement of the minority-carrier recombination in the front surface region of the n-type crystalline silicon base. The front-emitter SHJ PV modules, on the other hand, showed a reduction in the fill factor (FF), in addition to moderate reductions in Jsc and Voc. The FF reduction of the front-emitter SHJ PV modules is considered to be caused by the enhancement of the recombination in the front surface region of the n-type crystalline-silicon base as the region corresponds to the pn junction interface of the front-emitter configuration. The moderate reductions in both Jsc and Voc may be due to further progression of the first-stage degradation. These findings are essential for understanding the mechanism of PID in SHJ PV cell modules.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Silicon and Solar Cell Technologies · Photovoltaic System Optimization Techniques · Integrated Circuits and Semiconductor Failure Analysis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (37)
Show source-provided references
1. High-efficiency silicon heterojunction solar cells: a review10.1515/green-2011-0018 ↗
2. Development status of high-efficiency HIT solar cells10.1016/j.solmat.2010.04.030 ↗
3. The approaches for high efficiency HIT solar cell with very thin (<100 μm) silicon wafer over 23%
4. 24.7% record efficiency HIT solar cell on thin silicon wafer10.1109/JPHOTOV.2013.2282737 ↗
5. Impact of carrier recombination on fill factor for large area heterojunction crystalline silicon solar cell with 25.1% efficiency10.1063/1.4937224 ↗
6. Achievement of more than 25% conversion efficiency with crystalline silicon heterojunction solar cell10.1109/JPHOTOV.2014.2352151 ↗
7. Silicon heterojunction solar cell with interdigitated back contacts for a photoconversion efficiency over 26%10.1038/nenergy.2017.32 ↗
8. High-efficiency heterojunction crystalline Si solar cells10.7567/JJAP.57.08RB20 ↗
9. SEMI PV Group Europe
10. Potential-induced degradation in photovoltaic modules: a critical review10.1039/C6EE02271E ↗
11. Potential induced degradation of solar cells and panels
12. Potential induced degradation of solar cells and panels
13. Characterization of multicrystalline silicon modules with system bias voltage applied in damp heat
14. The role of stacking faults for the formation of shunts during potential-induced degradation of crystalline Si solar cells10.1002/pssr.201307090 ↗
15. Explanation of potential-induced degradation of the shunting type by Na decoration of stacking faults in Si solar cells10.1016/j.solmat.2013.06.015 ↗
16. Potential-induced degradation in photovoltaic modules based on n-type single crystalline Si solar cells10.1016/j.solmat.2015.04.037 ↗
17. Progression of rapid potential-induced degradation of n-type single-crystalline silicon photovoltaic modules10.7567/APEX.9.112301 ↗
18. Potential induced degradation of n-type crystalline silicon solar cells with p+ front junction10.1002/ese3.146 ↗
19. Influence of surface structure of n-type single-crystalline Si solar cells on potential-induced degradation10.1016/j.solmat.2017.03.018 ↗
20. Potential induced degradation of N-type bifacial silicon solar cells: an investigation based on electrical and optical measurements10.1016/j.solmat.2017.04.007 ↗
21. Changes in the current density-voltage and external quantum efficiency characteristics of n-type single-crystalline silicon photovoltaic modules with a rear-side emitter undergoing potential-induced degradation10.1016/j.solmat.2016.03.003 ↗
22. The surface polarization effect in high-efficiency silicon solar cells
23. Potential-induced degradation at interdigitated back contact solar cells10.1016/j.egypro.2014.08.015 ↗
24. Potential-induced degradation for encapsulated n-type IBC solar cells with front floating emitter10.1016/j.egypro.2015.07.050 ↗
25. Electrochemical corrosion of SnO2: F transparent conducting layers in thin-film photovoltaic modules10.1016/S0927-0248(02)00363-X ↗
26. Potential-induced degradation of thin-film Si photovoltaic modules10.7567/JJAP.56.04CS04 ↗
27. Similarity of potential-induced degradation in superstrate-type thin-film CdTe and Si photovoltaic modules10.7567/1347-4065/aafe67 ↗
28. Potential-induced degradation of CuIn1−xGaxSe2 thin film solar cells10.1109/JPHOTOV.2013.2253833 ↗
29. Potential-induced degradation of Cu(In,Ga)Se2 photovoltaic modules10.7567/JJAP.54.08KC13 ↗
30. Survey of potential-induced degradation in thin-film modules10.1117/1.JPE.5.053083 ↗
31. Elucidating PID degradation mechanisms and in situ dark I–V monitoring for modeling degradation rate in CdTe thin-film modules10.1109/JPHOTOV.2016.2598269 ↗
32. PV module durability testing under high voltage biased damp heat conditions10.1016/j.egypro.2011.06.154 ↗
33. Study on PID resistance of HIT PV modules
34. 600 hour potential induced degradation (PID) testing on silicon, CIGS, and HIT modules
35. Reduction in the short-circuit current density of silicon heterojunction photovoltaic modules subjected to potential-induced degradation tests10.1016/j.solmat.2016.12.027 ↗
36. Comprehensive study of potential-induced degradation in silicon heterojunction photovoltaic cell modules10.1002/pip.3006 ↗
37. Influence of hygrothermal stress on potential-induced degradation for homojunction and heterojunction crystalline Si photovoltaic modules10.35848/1347-4065/ab9a8a ↗