Degradation-related defect level in weathered silicon heterojunction modules characterized by deep level transient spectroscopy
Source abstract
Abstract
Commercial silicon heterojunction photovoltaic modules, known as amorphous-silicon-based heterojunction with intrinsic thin-film layer (HIT) modules, show average degradation after 10 years in the field. HIT modules weathered outdoors in Colorado and Florida display mostly uniform decreases in intensity when mapped with photoluminescence (PL) imaging compared to a control module. Flash-table-based current-voltage curves show that degradation is dominated by voltage loss. Samples are cored from each of the modules, and deep level transient spectroscopy (DLTS) detects three electron-trap defect states in all modules with activation energies of electron emission from the defects of 0.07, 0.16, and 0.50 eV. DLTS measurements on the weathered modules show an additional deep-level, electron-trap defect state with an activation energy of 0.51 eV and a trap density of approximately 10 12 cm −3 . The capture rate is measured using varying short filling pulse times, and the resulting capture cross section is estimated to be 1.1x10 −16 cm 2 . The development of the weathering-related defect level correlates to decreases in carrier lifetime, PL intensity, and module voltage. Various depths of the space charge region are probed with increments in applied reverse bias and filling-pulse bias. This DLTS depth profiling shows a trend of trap density increasing with less applied reverse bias, suggesting that the weathering-related defect increases carrier recombination toward the interface between the bulk silicon wafer and the junction-forming amorphous-silicon passivation layers.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Silicon and Solar Cell Technologies · Thin-Film Transistor Technologies · Photovoltaic System Optimization Techniques
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (37)
Show source-provided references
1. Tourino Jacobo
2. Masuko · 2014
3. Review—development history of high efficiency silicon, heterojunction solar cell: from discovery to practical use10.1149/2162-8777/abdfb6 ↗
4. Progress on the intrinsic a-Si:H Films for interface passivation of silicon heterojunction solar cells: a review10.1016/j.jnoncrysol.2021.121166 ↗
5. High efficiency module degradation—from atoms to systems
6. Device physics underlying silicon heterojunction and passivating‐contact solar cells: a topical review10.1002/pip.2959 ↗
7. Multifunctional process to improve surface passivation and carrier transport in industrial n-type silicon heterojunction solar cells by 0.7% absolute,”
8. Study of hydrogen influence and conduction mechanism of amorphous indium tin oxide for heterojunction silicon wafer solar cells: hydrogen influence and conduction mechanism of amorphous ITO10.1002/pssa.201532221 ↗
9. Current losses at the front of silicon heterojunction solar cells,”10.1109/JPHOTOV.2011.2174967 ↗
10. Silicon heterojunction system field performance10.1109/JPHOTOV.2017.2765680 ↗
11. Long-term performance and reliability of silicon heterojunction solar modules
12. Insights into the degradation of amorphous silicon passivation layer for heterojunction solar cells10.1002/pssa.201800705 ↗
13. Zhang · 2020 · 814
14. Jordan · 2020
15. Blood · 1992
16. Schroder · 1990
17. Capacitance study of inversion at the amorphous-crystalline interface of n-type silicon heterojunction solar cells10.1063/1.3663433 ↗
18. Deep level transient spectroscopy measurements of silicon heterojunction cells
19. Capacitance study of carrier inversion at the amorphous/crystalline silicon heterojunction passivated by different thicknesses of i-layer10.1016/j.apsusc.2014.03.187 ↗
20. Effects of oxygen related thermal donors on the performance of silicon heterojunction solar cells10.1016/j.solmat.2018.02.006 ↗
21. Stability of silicon heterojunction solar cells having hydrogen plasma treated intrinsic layer
22. Kinetics of bulk lifetime degradation in float‐zone silicon: fast activation and annihilation of grown‐in defects and the role of hydrogen versus light10.1002/pssa.202000436 ↗
23. Fast photoluminescence imaging of silicon wafers
24. Photoluminescence imaging of silicon wafers10.1063/1.2234747 ↗
25. An accurate method for calibrating photoluminescence-based lifetime images on multi-crystalline silicon wafers10.1016/j.solmat.2014.06.004 ↗
26. Photoluminescence based open circuit voltage and effective lifetime images re-interpretation for solar cells: the influence of horizontal balancing currents10.1016/j.solmat.2014.07.035 ↗
27. A novel method for characterizing temperature sensitivity of silicon wafers and cells
28. Deep level transient fourier spectroscopy (DLTFS)--a technique for the analysis of deep level properties10.1016/0038-1101(88)90071-8 ↗
29. Development of coring procedures applied to Si, CdTe, and CIGS solar panels10.1016/j.solener.2017.11.071 ↗
30. Advances in coring procedures of silicon photovoltaic modules
31. Laser cutting and micromachining for localized and targeted solar cell characterization
32. Model for a-Si:H/c-Si interface recombination based on the amphoteric nature of silicon dangling bonds10.1103/PhysRevB.76.035326 ↗
33. Defect states and carrier capture processes in a-Si:H.”10.1016/0022-3093(84)90322-3 ↗
34. Measurement of the density of gap states in hydrogenated amorphous silicon by space charge spectroscopy10.1103/PhysRevB.25.5285 ↗
35. Dangling-bond relaxation and deep-level measurements in hydrogenated amorphous silicon10.1103/PhysRevB.48.8667 ↗
36. Milnes · 1973
37. Interface states study of intrinsic amorphous silicon for crystalline silicon surface passivation in HIT solar cell10.1088/1674-1056/26/4/048104 ↗