Is TOPCon ready for EVA? Insights from damp heat testing of glass-backsheet modules
Source abstract
Abstract
Tunnel oxide passivated contact (TOPCon) technology currently dominates the photovoltaic market, and the industry is now focused on enhancing their cost-effectiveness while ensuring their durability in harsher environments. TOPCon modules commonly use a glass–glass bill of materials that incorporates polyolefin elastomer and co-extruded polyethylene encapsulants. Though, for cost and weight reduction, the use of polymer backsheets and lower-cost encapsulants is appealing. This study investigates the performance of glass-backsheet (G-B) TOPCon modules fabricated with two types of silver/aluminum (Ag/Al) pastes: conventional firing with standard Ag/Al paste and low-Al-content Ag paste combined with laser-assisted firing (LAF). The modules, encapsulated with ethylene vinyl acetate (EVA), were subjected to damp-heat testing. Our findings indicate that solar cells with Ag/Al paste exhibit lower stability compared to low Al-content Ag paste; however, acid-rich moisture conditions contribute to glass-frit failures in both types of pastes. Additionally, the rear-side metal contacts, particularly those containing tellurium (Te) compounds, are susceptible to degradation in such environments. Based on these degradation mechanisms, we conclude that further investigation is required to allow for the wider adoption of EVA in TOPCon modules, particularly when a polymer backsheet is used. Ongoing research is essential to optimize these materials and enhance the cost-effectiveness and reliability of TOPCon technology for future applications. • EVA-based GB TOPCon modules with Ag/Al paste lost ∼37% power after 1,000h DH, mainly from FF degradation. • Using low-Al Ag paste with LAF cut power loss to ∼6.2% after 1,000h DH, showing improved thermal stability. • Front-side failure was due to Al oxidation and frit corrosion; rear-side failure involved Te compound breakdown. • Acetic acid from EVA hydrolysis accelerated contact corrosion and delamination at both front and rear interfaces.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Planetary Science and Exploration · Space Exploration and Technology · Spacecraft Design and Technology
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (48)
Show source-provided references
1. Fischer · 2024
2. Bi-layer in-situ phosphorus doped poly-Si films by PECVD for blistering-free high-efficiency industrial TOPCon solar cells10.1016/j.solmat.2024.112771 ↗
3. Investigation of the Ag–Si contact characteristics of boron emitters for n-tunnel oxide-passivated contact solar cells metallized by laser-assisted current injection treatment10.1002/solr.202400268 ↗
4. Tube‐type plasma‐enhanced atomic layer deposition of aluminum oxide: enabling record lab performance for the industry with demonstrated cell efficiencies >2410.1002/pip.3607 ↗
5. Atomic scale controlled tunnel oxide enabled by a novel industrial tube‐based PEALD technology with demonstrated commercial TOPCon cell efficiencies > 24%,10.1002/pip.3627 ↗
6. Unlocking the potential of boronsilicate glass passivation for industrial tunnel oxide passivated contact solar cells10.1002/pip.3519 ↗
7. Ultrathin silicon oxide prepared by in-line plasma-assisted N2O oxidation (PANO) and the application for n-type polysilicon passivated contact10.1016/j.solmat.2019.110389 ↗
8. Blistering-free polycrystalline silicon carbide films for double-sided passivating contact solar cells10.1016/j.solmat.2022.111586 ↗
9. An industrially viable TOPCon structure with both ultra-thin SiOx and n+-poly-Si processed by PECVD for p-type c-Si solar cells10.1016/j.solmat.2019.109926 ↗
10. Design rules for high-efficiency both-sides-contacted silicon solar cells with balanced charge carrier transport and recombination losses10.1038/s41560-021-00805-w ↗
11. Tunnel oxide passivating electron contacts as full‐area rear emitter of high‐efficiency p‐type silicon solar cells10.1002/pip.2960 ↗
12. Improving the performance of industrial TOPCon solar cells through the insertion of intrinsic a-Si layer10.1016/j.solmat.2024.113024 ↗
13. Buyer aware: three new failure modes in TOPCon modules absent from PERC technology10.1016/j.solmat.2024.112877 ↗
14. Damp-heat endurance investigation of PV modules based on n-type bifacial passivated contact cells
15. Y. Ye et al., "Damp-Heat Stability Investigation of Glass-Backsheet Modules Based on Topcon Solar Cells," Available at: SSRN 4986461.
16. Unveiling the origin of metal contact failures in TOPCon solar cells through accelerated damp-heat testing10.1016/j.solmat.2024.113188 ↗
17. Enhancing the reliability of TOPCon technology by laser-enhanced contact firing10.1016/j.solmat.2024.112846 ↗
18. Laser‐enhanced contact optimization on iTOPCon solar cells10.1002/pip.3598 ↗
19. Investigation on Effects of the Laser‐Enhanced Contact Optimization Process With Ag Paste in a Boron Emitter for n‐TOPCon Solar Cell10.1002/pip.3854 ↗
20. Microscale contact formation by laser enhanced contact optimization10.1109/JPHOTOV.2021.3129362 ↗
21. Investigation of monocrystalline p-type PERC cells featuring the laser enhanced contact optimization process and new LECO paste10.1063/5.0056380 ↗
22. Degradation stability of solar cells after laser enhanced contact optimization (LECO)10.1063/5.0089704 ↗
23. Q.ANTUM NEO with LECO exceeding 25.5 % cell efficiency10.1016/j.solmat.2024.113110 ↗
24. Al-induced variation to Ag crystal orientation of Ag–Al pastes during metallization10.1016/j.solmat.2024.112814 ↗
25. Towards understanding the characteristics of Ag–Al spiking on boron-doped silicon for solar cells10.1016/j.solmat.2015.11.032 ↗
26. Structural investigation of printed Ag/Al contacts on silicon and numerical modeling of their contact recombination10.1109/JPHOTOV.2016.2591318 ↗
27. PV encapsulant formulations and stress test conditions influence dominant degradation mechanisms10.1016/j.solmat.2023.112319 ↗
28. Corrosion effects in bifacial crystalline silicon PV modules; interactions between metallization and encapsulation10.1016/j.solmat.2023.112321 ↗
29. Moisture ingress in photovoltaic modules: a review10.1016/j.solener.2021.06.055 ↗
30. The causes and effects of degradation of encapsulant ethylene vinyl acetate copolymer (EVA) in crystalline silicon photovoltaic modules: a review10.1016/j.rser.2017.06.039 ↗
31. Chemical and mechanical interfacial degradation in bifacial glass/glass and glass/transparent backsheet photovoltaic modules10.1002/pip.3602 ↗
32. Impact of acetic acid exposure on metal contact degradation of different crystalline silicon solar cell technologies10.1016/j.solmat.2022.112089 ↗
33. 2016
34. AZtec wave–a new way to achieve combined EDS and WDS capability on SEM10.1017/S1431927620013422 ↗
35. Zhou · 2023 · 2023
36. Formation of Ag/Al screen-printing contacts on B emitters10.1109/JPHOTOV.2014.2364117 ↗
37. Current conduction mechanism of front-side contact of N-type crystalline Si solar cells with Ag/Al pastes10.1109/JPHOTOV.2013.2292350 ↗
38. Firing behavior of lead-containing and lead-free metallization silver paste for monocrystalline silicon solar cells10.1016/j.solmat.2023.112439 ↗
39. Understanding the influence of tellurium oxide in front Ag paste for contacting silicon solar cells with homogeneous high sheet resistance emitter10.7567/JJAP.56.08MB07 ↗
40. Effect of Te-based glass on contact formation and electrical properties in Si solar cells10.1016/j.jallcom.2020.154500 ↗
41. Effect of TeO2-based lead-free glass on contact formation of front side silver metallization for monocrystalline silicon solar cells10.1016/j.solmat.2022.111585 ↗
42. Tellurium‐based screen‐printable conductor metallizations for crystalline silicon solar cells10.1002/pip.3185 ↗
43. Development of a low temperature silver paste for high efficiency screen-printed solar cells
44. Encapsulation of PV modules using ethylene vinyl acetate copolymer as a pottant: a critical review10.1016/0927-0248(95)00150-6 ↗
45. Characterization of ethylene vinyl acetate (EVA) encapsulant: effects of thermal processing and weathering degradation on its discoloration10.1016/0927-0248(92)90013-F ↗
46. Acetic acid production and glass transition concerns with ethylene-vinyl acetate used in photovoltaic devices10.1016/j.solmat.2006.10.009 ↗
47. Modeling of rates of moisture ingress into photovoltaic modules10.1016/j.solmat.2006.04.002 ↗
48. The oxides and oxyacids of tellurium10.1021/cr60244a003 ↗