Material characterization of seven photovoltaic backsheets using seven accelerated test conditions

Soňa Uličná, Rachael L. Arnold, Jimmy M. Newkirk, Archana Sinha, Kent Terwilliger, Laura T. Schelhas, Peter Pasmans, Christopher Thellen, David C. Miller

Abstract

A variety of polymeric backsheet materials can be found in fielded photovoltaic (PV) modules, mostly based on fluoropolymer and polyethylene terephthalate (PET) materials. Cost reduction and sustainability considerations drive the recent development of alternative backsheet materials and designs [1]. In some fielded PV installations, polymeric materials are susceptible to environmental degradation in the form of backsheet cracking. To prevent backsheet degradation that can result in a module failure, thorough laboratory reliability testing is needed. Here, we studied the durability of seven commercial and experimental PV backsheets through accelerated stress testing using seven photolytic, hygrometric, and custom tests with the goal to understand if novel fluoropolymer-free backsheets are sufficiently environmentally durable to be commercialized. We divided the mechanisms observed during aging into two categories: core degradation and surface degradation. Although core degradation due to hydrolysis was observed in all commercial PET-, and polyamide (PA)-based backsheets aged with 85 °C/85 % relative humidity, this test is unlikely to be field relevant. Photo-oxidative reactions on the exposed surface during UV weathering affected all seven backsheets regardless of the outer layer polymer material and additives. This degradation was limited to the outermost micrometers of the surface, except for backsheets containing PA-12, which resulted in surface cracking. A custom test combining UV with water spray caused the most severe backsheet degradation, including surface erosion and loss of insulating properties in polyolefin (PO)- and PA-based backsheets. This highlights the importance of combined accelerated stress testing to screen for complex backsheet degradation mechanisms. We also showed that, with material and design optimization, coextruded experimental PO-based backsheets have the potential to be a durable alternative to commercial PET- and fluoropolymer-based PV backsheets.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Photovoltaic System Optimization Techniques · Silicon and Solar Cell Technologies · Photovoltaic Systems and Sustainability

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (38)

Show source-provided references
1. Chunduri
2. A comparative life cycle assessment of end-of-life treatment pathways for photovoltaic backsheets10.1002/pip.3003 ↗
3. Life cycle assessment of photovoltaic module backsheets
4. Towards validation of combined-accelerated stress testing through failure analysis of polyamide-based photovoltaic backsheets
5. A comparison of emerging nonfluoropolymer-based coextruded PV backsheets to industry-benchmark technologies10.1109/JPHOTOV.2021.3117915 ↗
6. World map of the Köppen-Geiger climate classification updated10.1127/0941-2948/2006/0130 ↗
7. Palmiotti · 2023 · 2023
8. BACKFLIP: identification of materials and changes upon aging of emerging fluoropolymer-free and industry-benchmark PV backsheets
9. Al Hasan · 2023 · 1
10. IEC TS 62788-7-2, “Measurement procedures for mateials used in photovoltaic modules - Part 7-2: environmental exposures - accelerated weathering tests of polymeric materials,”
11. IEC 61215-2, “crystalline silicon terrestrial photovoltaic (PV) modules—design qualification and type approval- Part 2: test procedures,”
12. Tearing and reliability of photovoltaic module backsheets10.1002/pip.3144 ↗
13. GSAS-II: the genesis of a modern open-source all purpose crystallography software package10.1107/S0021889813003531 ↗
14. Measurement procedures for mateials used in photovoltaic modules - Part 2: polymeric materials used for frontsheets and backsheets
15. IEC 61730-2, “Photovoltaic (PV) module safety qualification - Part 2: requirements for testing,”
16. Polyethylene terephthalate degradation under natural and accelerated weathering conditions10.1016/j.eurpolymj.2020.109873 ↗
17. Physicochemical aspects of the environmental degradation of poly(ethylene terephthalate)10.1016/0141-3910(94)90074-4 ↗
18. FT-IR study of the effect of hydrolytic degradation on the structure of thin PET films10.1016/S0141-3910(99)00104-4 ↗
19. Physical aspects of the hydrolysis of polyethylene terephthalate10.1016/0141-3910(89)90114-6 ↗
20. Evaluation of temperature and humidity on PV module component degradation
21. Photolysis of poly(ethylene terephthalate)10.1002/pol.1967.150050308 ↗
22. A study of degradation mechanisms in PVDF-based photovoltaic backsheets10.1038/s41598-022-18477-1 ↗
23. Microstructure changes during failure of PVDF-based photovoltaic backsheets10.1002/pip.3605 ↗
24. Limits of UV-light acceleration on the photooxidation of low-density polyethylene10.1016/j.polymdegradstab.2020.109443 ↗
25. Combining theory and experiment to study the photooxidation of polyethylene and polypropylene10.1021/jp035427h ↗
26. Failure analysis of a new polyamide-based fluoropolymer-free backsheet after combined-accelerated stress testing10.1109/JPHOTOV.2021.3090152 ↗
27. Error analysis of aged modules with cracked polyamide backsheets10.1016/j.solmat.2019.110194 ↗
28. Backsheet Chalking - theoretical background and relation to backsheet cracking and insulation failures
29. Moisture‐induced plasticization of amorphous polyamides and their blends10.1002/app.1988.070360301 ↗
30. Hydrolytic ageing of polyamide 11. 1. Hydrolysis kinetics in water10.1016/S0032-3861(02)00583-9 ↗
31. Molecular weight distribution and mass changes during polyamide hydrolysis10.1016/S0032-3861(97)00414-X ↗
32. Effect of molecular weight and hydration on the tensile properties of polyamide 12
33. Standard · 2018
34. Hydrolysis kinetics of condensation polymers under humidity aging conditions10.1016/j.polymdegradstab.2013.04.001 ↗
35. IEC 60721-2-1:2013, “Classification of environmental conditions - Part 2-1: environmental conditions appearing in nature - temperature and humidity,”
36. Quantitative analysis of degradation mechanisms in 30-year-old PV modules10.1016/j.solmat.2019.110019 ↗
37. Degradation in photovoltaic encapsulant transmittance: results of the second PVQAT TG5 artificial weathering study10.1002/pip.3551 ↗
38. Advancing reliability assessments of photovoltaic modules and materials using combined-accelerated stress testing10.1002/pip.3342 ↗