Correlation between damp-heat test and field operation for electrode corrosion in photovoltaic modules
Source abstract
Abstract
In order to determine the correlation between damp-heat test and field exposure, the degradation mode related to corrosion in photovoltaic modules was investigated in detail based on the change in acetic acid concentration in the ethylene-vinyl acetate encapsulant on the light-receiving side and power retention rate during combination tests that varied temperature, relative humidity, and a new factor, the light intensity. The estimated activation energy for acetic acid generation was relatively high at 0.65 eV in the absence of light; however, it decreased to 0.08 eV under illumination. The correspondence between damp-heat test and field exposure was approximately equivalent to 1000 h of damp-heat test and 3–6 years of field exposure in humid areas. The relationship between the acetic acid concentration and the recovered power retention rate was approximately −0.002% per μg/g, even for modules with high acetic acid resistance. This suggests that an acetic acid concentration of 10000 μg/g can serve as a benchmark for the power lifetime, at which point the power falls below 80%. The power transition prediction was derived from a combination of acetic acid concentration prediction and this relationship. In climates hotter and more humid than Cfa classification, the lifetime is anticipated to be within 20 years, if no efforts are made to improve the reliability of the cell or encapsulant. For long-term reliability of modules operated in humid regions, the use of a single polyolefin layer as the light-receiving side encapsulant or appropriate assessment by the acceleration test is required.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Photovoltaic System Optimization Techniques · Solar Thermal and Photovoltaic Systems · Building Energy and Comfort Optimization
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (76)
Show source-provided references
1. Modeling of rates of moisture ingress into photovoltaic modules10.1016/j.solmat.2006.04.002 ↗
2. Acetic acid production and glass transition concerns with ethylene-vinyl acetate used in photovoltaic devices10.1016/j.solmat.2006.10.009 ↗
3. The role of encapsulant moisture permeability in the durability of solar photovoltaic modules
4. Outdoor weathering of PV modules — effects of various climates and comparison with accelerated laboratory testing
5. Degradation mechanism investigation of extended damp heat aged PV modules
6. Damp heat versus field reliability for crystalline silicon
7. Investigation of damp heat degradation mechanisms and correlation to an accelerated test procedure (HAST)
8. Degradation mechanism analysis of damp heat aged PV modules
9. Acetic acid production, migration and corrosion effects in ethylene-vinyl-acetate- (EVA-) based PV modules
10. Failure modes after damp heat tests on PV modules
11. Improved performance encapsulation film based on polyolefin
12. Origin of damp-heat induced cell degradation10.1016/j.solmat.2013.03.022 ↗
13. The effect of moisture on the degradation mechanism of multi-crystalline silicon photovoltaic module10.1016/j.microrel.2013.07.047 ↗
14. Effect of temperature and humidity on the degradation rate of multicrystalline silicon photovoltaic module10.1155/2013/925280 ↗
15. Correlation between moisture ingress and performance in photovoltaic modules
16. Degradation mechanism of photovoltaic modules by extended damp-heat or thermal-cycle test
17. Investigation of acetic acid corrosion impact on printed solar cell contacts10.1109/JPHOTOV.2015.2395146 ↗
18. Electrical detection of gap formation underneath finger electrodes on c-Si PV cells exposed to acetic acid vapor under hygrothermal conditions
19. Changes of solar cell parameters during damp-heat exposure10.1002/pip.2793 ↗
20. Performance evaluation of PV modules after accelerated testing followed by four years of field exposure in hot-humid climate of Florida
21. Effect of soldering on the module degradation along bus bar in DH test and PCT for crystalline Si PV modules
22. Development of highly efficientlong-term reliable crystalline silicon solar cells and modules by low-cost mass production10.7567/JJAP.57.08RB22 ↗
23. Comparison of glass/glass and glass/backsheet mini-modules by accelerated test
24. Analysis of acetic acid generation in PV modules
25. Corrosion mechanism analysis of the front-side metallization of a crystalline silicon PV module by a high-temperature and high-humidity test10.35848/1347-4065/ab8274 ↗
26. Investigation of degradation mode spreading interconnectors by pressure-cooker testing of photovoltaic cells10.1109/JPHOTOV.2019.2950079 ↗
27. Impact of acetic acid exposure on the screen-printed tellurite-based silver contacts
28. Corrosion testing of solar cells: wear-out degradation behavior10.1016/j.solmat.2022.111974 ↗
29. Crystalline silicon photovoltaic module degradation: galvanic corrosion and its solution10.1016/j.engfailanal.2022.106329 ↗
30. Impact of acetic acid exposure on metal contact degradation of different crystalline silicon solar cell technologies10.1016/j.solmat.2022.112089 ↗
31. PV module lifetime in humid areas: are 2000 h of damp heat tests sufficient for 25 years of life?
32. Influences of different backsheet on PV module reliability and durability in high humidity environment for the EU PVSEC 2019
33. Comparison of degradation mechanism of PV modules between under long term field exposure at hot-humid environment and under DH tests
34. Analysis of the degradation of monocrystalline silicon photovoltaic modules after long-term exposure for 18 years in a hot-humid climate in China
35. Analysis of electroluminescence and infrared thermal images of monocrystalline silicon photovoltaic modules after 20 years of outdoor use in a solar vehicle10.1016/j.solener.2018.07.055 ↗
36. Evaluation of temperature and humidity on PV module degradation- in field degradation analysis of crystalline silicon module
37. Comparison and analysis of performance and degradation differences of crystalline-Si photovoltaic modules after 15-years of field operation10.1016/j.solener.2019.08.051 ↗
38. Corrosion growth of solar cells in modules after 15 years of operation10.1016/j.solener.2020.05.016 ↗
39. Analysis of long-term performance and reliability of PV modules under tropical climatic conditions in sub-Saharan10.1016/j.renene.2020.08.021 ↗
40. Spectroscopic investigation of long-term outdoor-exposed crystalline silicon photovoltaic modules10.1016/j.jphotochem.2020.112891 ↗
41. Degradation analysis of photovoltaic modules after operating for 22 years. A case study with comparisons10.1016/j.solener.2021.04.026 ↗
42. Differences in c-Si solar cell metallization and susceptibility to series resistance degradation
43. Photovoltaic module failures after 10 years of operation in the tropics10.1016/j.renene.2021.05.145 ↗
44. Degradation of crystalline silicon photovoltaic modules installed in different climates
45. A study of module degradation from a 10-year installation in the urban tropical environment
46. Comparative degradation analysis of accelerated-aged and field-aged crystalline silicon photovoltaic modules under Indian subtropical climatic conditions10.1016/j.rineng.2022.100674 ↗
47. Degradation of monocrystalline silicon photovoltaic modules from a 10-year-old rooftop system in Florida10.1109/JPHOTOV.2023.3238278 ↗
48. H. Kanno, J. Irikawa, Y. Nakamura, H. Hashimoto, M. Taguchi, Key technologies for achieving high reliability and cost effectiveness in HJT module, in: Proc. PVRW (2022) Poster session E.2.4. https://www.nrel.gov/docs/fy22osti/82935.pdf (accessed 18 April 2024).
49. Characterization of front contact degradation in monocrystalline and mc-Sicrystalline silicon photovoltaic modules following damp heat exposure10.1016/j.solmat.2021.111468 ↗
50. Differences in printed contacts lead to susceptibility of silicon cells to series resistance degradation10.1109/JPHOTOV.2022.3150727 ↗
51. Correspondence: bill of materials variation and module degradation in utility-scale PV systems10.1109/JPHOTOV.2022.3209610 ↗
52. Guiding principle for crystalline Si photovoltaic modules with high tolerance to acetic acid10.7567/JJAP.57.04FS06 ↗
53. Degradation of bifacial PERC and Al-BSF cell minimodules with white and clear encapsulant combinations in modified damp heat
54. Chunduri
55. Migration of Sn and Pb from solder ribbon onto Ag fingers in field-aged silicon photovoltaic modules10.1155/2015/257343 ↗
56. Analysis of the electrochemical reactions and ions migration for crystalline silicon solar module under high system voltage10.1016/j.solener.2021.07.050 ↗
57. Study on mitigation method of solder corrosion for crystalline silicon photovoltaic modules10.1155/2014/809075 ↗
58. Simulation of water ingress into PV-modules: IEC-testing versus outdoor exposure10.1016/j.solener.2015.03.007 ↗
59. Quantitative determination of moisture content in solar modules by short-wave infrared reflectometry10.1109/JPHOTOV.2019.2938108 ↗
60. A reaction-diffusion formulation to simulate EVA polymer degradation in environmental and accelerated ageing conditions10.1016/j.solmat.2017.02.014 ↗
61. Uber einige meteorologische begriffe
62. The effect of ethylene content on the interaction between ethylene-vinyl alcohol copolymers and water: (I) Application of FT-IR spectroscopy to determine transport properties and interactions in food packaging films10.1016/j.polymertesting.2005.09.018 ↗
63. Study of the influence of water sorption in pure components and binary blends of high barrier ethylene-vinyl alcohol copolymer and amorphous polyamide and nylon-containing ionomer10.1016/S0032-3861(01)00496-7 ↗
64. Effect of humidity on mechanical, thermal and barrier properties of EVOH films10.1016/j.memsci.2017.06.031 ↗
65. Measurement and simulation of moisture ingress in PV modules in various climates10.1109/JPHOTOV.2023.3323808 ↗
66. Photovoltaic reliability model development and validation
67. Degradation analysis of solar photovoltaic modules: influence of environmental factor
68. Assessment of uncertainties and variations in PV modules degradation rates and lifetime predictions using physical models10.1016/j.solener.2021.01.071 ↗
69. Comprehensive model for humidity testing correlation
70. Review of statistical and analytical degradation models for photovoltaic modules and systems as well as related improvements10.1109/JPHOTOV.2018.2870532 ↗
71. Modeling outdoor service lifetime prediction of PV modules: effects of combined climatic stressors on PV module power degradation10.1109/JPHOTOV.2019.2916197 ↗
72. Methodology of Köppen-Geiger-Photovoltaic climate classification and implications to worldwide mapping of PV system performance10.1016/j.solener.2019.08.072 ↗
73. Global climate data processing and mapping of degradation mechanisms and degradation rates of PV modules10.3390/en12244749 ↗
74. Acetic acid permeation through photovoltaic backsheets: influence of the composition on the permeation rate10.1016/j.polymertesting.2017.04.025 ↗
75. Durable polyolefin encapsulants in aged photovoltaic modules10.1016/j.jphotochem.2022.114015 ↗
76. Corrosion behavior of crystalline silicon solar cells10.1016/j.microrel.2017.01.006 ↗