Alleviating contaminant-induced degradation of TOPCon solar cells with copper plating

Xutao Wang, Chandany Sen, Xinyuan Wu, Yuan-Chih Chang, Haoran Wang, Muhammad Umair Khan, Bram Hoex

Abstract

With the development of silicon (Si) solar cell technology, the tunnel oxide passivated contact (TOPCon) architecture has become the dominant industrial technology in the solar market. At the same time, concerns are raised about the long-term stability of TOPCon photovoltaic modules. The front side metallization of TOPCon solar cells is reported to be susceptible to corrosion as identified during cell and module level damp-heat (DH) testing. In this work, we use copper (Cu) plating on screen-printed (Ag paste with up to 3 % Al) TOPCon solar cells to address this problem. The plated cells show an improved performance due to the higher fill factor, indicating the potential of reducing the silver (Ag) consumption and material cost without sacrificing the solar cell efficiency. NaCl was chosen as a representative contaminant to assess the reliability at the cell level after 6 h of DH. The Cu-plated TOPCon solar cells showed only a ∼11.5% rel drop in efficiency, compared to ∼80% rel reduction in efficiency for the as-received cells. We also show that the Cu plating process results in a considerably denser contact, which hinders the penetration of contaminants. Consequently, the method presented in this work enhances the stability of photovoltaic technology with corrosion-sensitive contacts during field operation, thus contributing to an increase in lifetime and reduction in levelized cost of electricity. • ∼1 μm Cu was plated on the front grid of TOPCon cells with Al-containing front Ag-paste to improve reliability. The increased fill factor enabled ∼0.09% abs higher efficiency of as-plated cells. • Over 80% rel efficiency degradation occurred in non-plated TOPCon cells after 6 hours of DH testing due to increased R s and V oc drop, while plated cells showed only ∼11.5% rel efficiency loss. • Bare cells showed a 10-fold contact resistivity increase after 0.5 hours of DH testing, indicating metal-Si contact corrosion, while plated-Cu retained 1–2 orders lower contact resistivity after 2 hours of DH testing. • SEM and EDS analysis illustrated that plated-Cu can fill the voids of screen-printed contact and make the contact denser, which hinders the contaminant penetration and alleviates contact degradation.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Silicon and Solar Cell Technologies · Photovoltaic System Optimization Techniques · solar cell performance optimization

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (55)

Show source-provided references
1. 2024
2. Crystalline silicon (c-Si)-Based tunnel oxide passivated contact (TOPCon) solar cells: a review10.3390/en16020715 ↗
3. The application of poly-Si/SiOx contacts as passivated top/rear contacts in Si solar cells10.1016/j.solmat.2016.09.015 ↗
4. Fundamentals, present status and future perspective of TOPCon solar cells: a comprehensive review
5. Atomic scale controlled tunnel oxide enabled by a novel industrial tube-based PEALD technology with demonstrated commercial TOPCon cell efficiencies > 2410.1002/pip.3627 ↗
6. Detailed review on c-Si/a-Si:H heterojunction solar cells in perspective of experimental and simulation10.1016/j.mee.2022.111884 ↗
7. Nanocrystalline silicon thin film growth and application for silicon heterojunction solar cells: a short review10.1039/D0NA00791A ↗
8. Long-term performance and reliability of silicon heterojunction solar modules10.1002/pip.3688 ↗
9. Silicon heterojunction solar cells: techno-economic assessment and opportunities10.1016/j.joule.2022.02.009 ↗
10. Trina Solar claims record-breaking efficiency of 26.58% for TOPCon solar cell
11. M. Woodhouse, D. Feldman, R. Fu, K. Horowitz, D. Chung, On the path to SunShot: the role of advancements in solar photovoltaic efficiency, Reliability, and Costs, (n.d.).
12. The value of efficiency in photovoltaics10.1016/j.joule.2019.07.028 ↗
13. The value of stability in photovoltaics10.1016/j.joule.2021.10.019 ↗
14. Reassessment of the limiting efficiency for crystalline silicon solar cells10.1109/JPHOTOV.2013.2270351 ↗
15. The degradation of multi-crystalline silicon solar cells after damp heat tests10.1016/j.microrel.2014.07.071 ↗
16. Potential induced degradation in c-Si glass-glass modules after extended damp heat stress10.1016/j.solener.2023.03.013 ↗
17. Origin of damp-heat induced cell degradation10.1016/j.solmat.2013.03.022 ↗
18. Raman spectroscopic analysis of encapsulants in aged photovoltaic modules10.1016/j.jphotochem.2021.113721 ↗
19. Four failure modes in silicon heterojunction glass-backsheet modules10.1016/j.solmat.2023.112358 ↗
20. Impact of acetic acid exposure on metal contact degradation of different crystalline silicon solar cell technologies10.1016/j.solmat.2022.112089 ↗
21. Corrosion effects in bifacial crystalline silicon PV modules; interactions between metallization and encapsulation10.1016/j.solmat.2023.112321 ↗
22. Damp-heat endurance investigation of PV modules based on n-type bifacial passivated contact cells
23. Accelerated damp-heat testing at the cell-level of bifacial silicon HJT, PERC and TOPCon solar cells using sodium chloride10.1016/j.solmat.2023.112554 ↗
24. Enhancing the reliability of TOPCon technology by laser-enhanced contact firing10.1016/j.solmat.2024.112846 ↗
25. Buyer aware: three new failure modes in TOPCon modules absent from PERC technology10.1016/j.solmat.2024.112877 ↗
26. Unveiling the origin of metal contact failures in TOPCon solar cells through accelerated damp-heat testing10.1016/j.solmat.2024.113188 ↗
27. Diffusion processes for integrated waveguide fabrication in glasses: a solid-state electrochemical approach10.1016/0009-2509(95)00115-L ↗
28. Analysis of the electrochemical reactions and ions migration for crystalline silicon solar module under high system voltage10.1016/j.solener.2021.07.050 ↗
29. Supercharging cell-level potential-induced degradation (PID) testing using a salt-enriched hybrid polymer layer10.1016/j.solmat.2023.112479 ↗
30. Effects of SiOx barrier layer prepared by plasma-enhanced chemical vapor deposition on improvement of long-term reliability and production cost for Cu-plated amorphous Si/crystalline Si heterojunction solar cells10.1016/j.solmat.2016.12.029 ↗
31. Addressing sodium ion-related degradation in SHJ cells by the application of nano-scale barrier layers10.1016/j.solmat.2023.112604 ↗
32. Failure modes of silicon heterojunction photovoltaic modules in damp heat environment: sodium and moisture effects10.1016/j.solmat.2024.113190 ↗
33. Unveiling the degradation mechanisms in silicon heterojunction solar cells under accelerated damp-heat testing10.1016/j.solmat.2024.113325 ↗
34. Chemical characteristics and trends of Indian summer monsoon rainfall: a review10.4209/aaqr.220019 ↗
35. Chemical composition of the haze in Malaysia 200510.1016/j.atmosenv.2013.05.024 ↗
36. An empirical equation of state for hydrothermal seawater (3.2 percent NaCl)10.2475/ajs.285.8.725 ↗
37. Moisture induced degradation in field-aged multicrystalline silicon photovoltaic modules10.1016/j.solmat.2023.112407 ↗
38. Adhesional shear strength and surface analysis of a PV module deployed in harsh coastal climate10.1016/S0927-0248(00)00304-4 ↗
39. Potential-free sodium-induced degradation of silicon heterojunction solar cells10.1002/pip.3698 ↗
40. Ag/Cu plating to improve Ag grid electrodes of the recycled c-Si solar cells10.20964/2020.12.77 ↗
41. Study of annealing temperature for Ni/Cu/Ag plated front contact single crystalline solar cells10.1109/JPHOTOV.2016.2576683 ↗
42. Optimizing adhesion of laser structured plated Ni-Cu contacts with insights from micro characterization10.1016/j.egypro.2016.07.101 ↗
43. Plated TOPCon solar cells & modules with reliable fracture stress and soldered module interconnection10.1051/epjpv/2021010 ↗
44. Realization of micropatterned, narrow line-width Ni–Cu–Sn front contact grid pattern using maskless direct-write lithography for industrial silicon solar cells10.1021/acsaem.1c01699 ↗
45. Review on metallization approaches for high-efficiency silicon heterojunction solar cells10.1007/s12209-022-00336-9 ↗
46. An advanced software suite for the processing and analysis of silicon luminescence images10.1016/j.cpc.2017.02.012 ↗
47. NIH Image to ImageJ: 25 years of image analysis10.1038/nmeth.2089 ↗
48. Challenges facing copper-plated metallisation for silicon photovoltaics: insights from integrated circuit technology development10.1002/pip.3062 ↗
49. Electrical properties and recombination activity of copper, nickel and cobalt in silicon10.1007/s003390050649 ↗
50. Diffusion, solubility and gettering of copper in silicon10.1016/S0921-5107(99)00514-0 ↗
51. Long term stability of copper front side contacts for crystalline silicon solar cells10.1016/j.solmat.2014.12.024 ↗
52. Passivation effect of silicon nitride against copper diffusion10.1063/1.365380 ↗
53. Effects of Ag thickness and deposition temperature on prevention of Cu diffusion in Cu/Ag/Si system10.1143/JJAP.44.3187 ↗
54. Y.-C. Chang, Y. Zhang, L. Wang, S. Wang, H. Wang, C.-Y. Huang, R. Chen, C. Chan, B. Hallam, Silver-lean metallization and hybrid contacts via plating on screen-printed metal for silicon solar cells manufacturing, Prog. Photovolt.: Res. App. n/a (n.d.). https://doi.org/10.1002/pip.3799.10.1002/pip.3799 ↗
55. Griddler_and_PRO_manual.pdf, (n.d.). https://griddlersolar.com/wp-content/uploads/Griddler_and_PRO_manual.pdf (accessed June 5, 2024).