journal article·2024-09Open access

Soiling, cleaning, and abrasion: The results of the 5-year photovoltaic glass coating field study

Joanna Bomber, Asher Einhorn, Chaiwat Engtrakul, Clare Lanaghan, Jeffrey Linger, Leonardo Micheli, David C. Miller, Joshua Morse, Helio Moutinho, Matthew Muller, Jimmy M. Newkirk, Lin Simpson, Bobby To, Sarah Toth, Telia Curtis, Fang Li, Govindasamy Tamizhmani, Sai Tatapudi, Vivian Alberts, Aaesha Al Nuaimi, Pedro Banda, Jim J. John, Gerhard Mathiak, Ahmad O.M. Safieh, Marco Stefancich, Bader Alabdulrazzaq, Ayman Al-Qattan, Sonali Bhaduri, Anil Kottantharayil, Ben Bourne, Zoe deFreitas, Fabrizio Farina, Greg Kimball, Adam Hoffman

Abstract

External contamination (“soiling”) of the incident surface is a major limiting factor for solar technologies. A 5-year field glass coupon study was conducted to better understand external contamination and its effects; compare cleaning methods and the use of preventative coatings; and explore the abrasion resulting from cleaning to advise on accelerated abrasion testing. Test sites included the cities of Dubai (UAE), Kuwait City (Kuwait), Mesa (AZ), Mumbai (India), and Sacramento (CA). Through the 5-year cumulative study, dry brush, water spray, and wet sponge and squeegee cleaning methods were compared to no cleaning. Optical microscopy was used to obtain images, including representative color images, grayscale images for object analysis, and oblique images for coating integrity assessment. A thresholding protocol was developed to analyze and distinguish specimens using the ImageJ software. Optical performance was quantified using a spectrophotometer, including comprehensive optical characterization (transmittance, reflectance, and absorptance in addition to forward- and back-scattering). Atomic force microscopy was used to verify the abrasion damage morphology, including the width and depth of surface scratches. Analysis of the results included correlation of optical performance and particle area coverage, rank order (by coating or location), and the acceleration factor for abrasion damage. The efficacy of external cleaning was more readily distinguished from the effectiveness of antisoiling coatings. The acceleration factor for dry brush cleaning of a porous silica coating was found to be on the order of unity.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: solar cell performance optimization · Thin-Film Transistor Technologies · Silicon and Solar Cell Technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (100+)

Show source-provided references
1. Photovoltaic module calibration value versus optical air mass: the Air Mass Function10.1002/pip.2303 ↗
2. A comprehensive review of the impact of dust on the use of solar energy: history, investigations, results, literature, and mitigation approaches10.1016/j.rser.2012.12.065 ↗
3. Fundamentals of soiling processes on photovoltaic modules10.1016/j.rser.2018.09.015 ↗
4. Durability of fresnel lenses: a review specific to the concentrating photovoltaic application10.1016/j.solmat.2011.01.031 ↗
5. Techno-economic assessment of soiling losses and mitigation strategies for solar power generation10.1016/j.joule.2019.08.019 ↗
6. Anti-reflective coatings: a critical, in-depth review10.1039/c1ee01297e ↗
7. Evaluation of soiling and potential mitigation approaches on photovoltaic glass
8. Hydrophobic–hydrophilic surfaces exhibiting dropwise condensation for anti-soiling applications
9. Combined soiling and abrasion testing of antisoiling coatings
10. The abrasion of photovoltaic glass: a comparison of the effects of natural and artificial aging10.1109/JPHOTOV.2019.2947029 ↗
11. 2022 · 1
12. Soiling and cleaning: initial observations from 5-year photovoltaic glass coating durability study10.1016/j.solmat.2018.05.039 ↗
13. Hoffman · 1980 · 1
14. Microbial colonization affects the efficiency of photovoltaic panels in a tropical environment10.1016/j.jenvman.2015.03.050 ↗
15. Impact of the 2019-2020 Australian black summer wildfires on photovoltaic energy production
16. Sheratte · 1979 · vols. 79–7052 · 1
17. Wavelength dependent scattering caused by dust accumulation on solar mirrors10.1016/0165-1633(80)90046-5 ↗
18. Durability of Poly(Methyl Methacrylate) Lenses Used in Concentrating Photovoltaics
19. Review of methods to account for the solar spectral influence on photovoltaic device performance10.1016/j.energy.2023.129461 ↗
20. Comparative modeling of optical soiling losses for CSP and PV energy systems10.1016/j.solener.2019.12.045 ↗
21. Quantifying soiling loss directly from PV yield
22. Fine particles and coarse particles: concentration relationships relevant to epidemiologic studies10.1080/10473289.1997.10464074 ↗
23. Properties of atmospheric aerosol
24. Bohren · 1983
25. Literature survey of dust particle dimensions on soiled solar panel modules
26. ACS, “ACS Advocacy Workshops,” n.d., https://www.acs.org/policy/memberadvocacy/acs-advocacy-workshops.html#:~:text=ACS20Climate20Science20Toolkit207C20Energy,emitted20at20the20sun's20surface.
27. Optical properties and mineralogical composition of different Saharan mineral dust samples: a laboratory study10.5194/acp-6-3315-2006 ↗
28. A laboratory investigation of light scattering from representative components of mineral dust aerosol at a wavelength of 550 nm10.1029/2007JD009387 ↗
29. Influence of soiling layer on quantum efficiency and spectral reflectance on crystalline silicon PV modules
30. The discoloration of the Taj Mahal due to particulate carbon and dust deposition10.1021/es504005q ↗
31. Spectral sensitivity of simulated photovoltaic module soiling for a variety of synthesized soil types
32. Study of soiling loss on photovoltaic modules with artificially deposited dust of different gravimetric densities and compositions collected from different locations in India
33. Dust potency in the context of solar photovoltaic (PV) soiling loss10.1016/j.solener.2021.04.015 ↗
34. Dust-induced shading on photovoltaic modules10.1002/pip.2230 ↗
35. Modelling photovoltaic soiling losses through optical characterization10.1038/s41598-019-56868-z ↗
36. Optical losses of photovoltaic cells due to aerosol deposition: role of particle refractive index and size10.1016/j.solener.2017.06.047 ↗
37. Correlating photovoltaic soiling losses to waveband and single-value transmittance measurements10.1016/j.energy.2019.05.097 ↗
38. 2021 · 1
39. Outdoor soiling microscope for measuring particle deposition and resuspension10.1016/j.solener.2016.08.015 ↗
40. NIH Image to ImageJ: 25 years of image analysis10.1038/nmeth.2089 ↗
41. ImageJ for microscopy
42. Evaluation of reflectance measurement techniques for artificially soiled solar reflectors: experimental campaign and model assessment10.1016/j.solmat.2021.111321 ↗
43. Comprehensive analysis of soiling and cementation processes on PV modules
44. Microstructural analysis of the PV module cementation process at the solar platform of the Atacama Desert10.1016/j.solmat.2021.111109 ↗
45. Pattern effects of soil on photovoltaic surfaces
46. Dew as a detrimental influencing factor for soiling of PV modules
47. Anti-soiling surfaces for PV applications prepared by solgel processing: comparison of laboratory testing and outdoor exposure
48. Environ. “Characterization of dust particles in South India and investigation on soiling image analysis for photovoltaic application,”10.1007/s11356-022-22630-8 ↗
49. Novel soiling detection system for solar panels
50. Mars soiling sensor
51. Efficient image-based soiling quantification using histograms of a checkered pattern10.1016/j.solener.2022.07.034 ↗
52. 2014 · 1
53. Techniques to measure grain-size distributions of loamy sediments: a comparative study of ten instruments for wet analysis10.1111/j.1365-3091.2007.00893.x ↗
54. Size frequency distribution of sediments
55. 2017 · 1
56. IEST-STD-CC1246E: product cleanliness levels – applications, requirements, and determination
57. Surface particle obscuration and BRDF predictions10.1117/12.962866 ↗
58. The performance and durability of single layer sol-gel anti-reflection coatings applied to solar module cover glass10.1016/j.surfcoat.2018.11.030 ↗
59. The performance and durability of Anti-reflection coatings for solar module cover glass – a review10.1016/j.solener.2023.06.009 ↗
60. Photoinduced surface reactions on TiO2 and SrTiO3 films: photocatalytic oxidation and photoinduced hydrophilicity10.1021/cm990556p ↗
61. Hydrophobic-hydrophilic surfaces exhibiting dropwise condensation for anti-soiling applications
62. Fluoropolymer coatings for solar cover glass: anti-soiling mechanisms in the presence of dew
63. Photovoltaics module reliability for the terawatt age10.1088/2516-1083/ac6111 ↗
64. Artificial linear brush abrasion of coatings for photovoltaic module first surfaces
65. Optimized cleaning cost and schedule based on observed soiling conditions for photovoltaic plants in central Saudi Arabia
66. Economics of seasonal photovoltaic soiling and cleaning optimization scenarios
67. 2016 · 1
68. Vdi · 2020 · 1
69. Characterizing mineral dusts and other aerosols from the Middle East—Part 1: ambient sampling10.1080/08958370802464273 ↗
70. Ashes to ashes, dust to dust: averting a potential showstopper for solar photovoltaics
71. Characterization of dust accumulated on photovoltaic panels in Doha, Qatar10.1016/j.solener.2016.11.053 ↗
72. The IEC 62788-7-3 abrasion methods standard and supporting experiments at NREL on PV surfaces and coatings
73. Measurement of saltation process over gobi and sand dunes in the Taklimakan desert, China, with newly developed sand particle counter10.1029/2004JD004688 ↗
74. Review of artificial abrasion test methods for PV module technology
75. 2022 · 1
76. Din · 2022 · 1
77. Non-destructive characterization of anti-reflection coatings on PV modules
78. 2016 · 1
79. Examination of an optical transmittance test for photovoltaic encapsulation materials
80. Adaptive local thresholding for detection of nuclei in diversity stained cytology images
81. Biological soiling
82. I. Cordero, “Fungus: how to prevent growth and remove it from optical components,” Comm. Eye Health, 26 (83), 2013, 57. PMID: 24421580; PMCID: PMC3864060.
83. Molecular and physiological effects of environmental UV radiation on fungal conidia10.1007/s00294-015-0483-0 ↗
84. CAMS global greenhouse gas reanalysis (EGG4), https://ads.atmosphere.copernicus.eu/cdsapp#!/dataset/cams-global-ghg-reanalysis-egg4?tab=overview.
85. CAMS global reanalysis (EAC4), https://ads.atmosphere.copernicus.eu/cdsapp#!/dataset/cams-global-reanalysis-eac4?tab=overview.
86. Surface soiling: theoretical mechanisms and evaluation of low-soiling coatings
87. Multi-year field assessment of seasonal variability of photovoltaic soiling and environmental factors in a desert environment10.1016/j.solener.2020.10.076 ↗
88. Comparative analysis of energy produced by photovoltaic modules with anti-soiling coated surface in arid climates10.1016/j.apenergy.2013.01.048 ↗
89. Brophy · 2015
90. Soiling, cleaning, and abrasion: the results of the 5-year photovoltaic glass coating field study
91. A highly diverse, desert-like microbial biocenosis on solar panels in a Mediterranean city10.1038/srep29235 ↗
92. Microbial colonization affects the efficiency of photovoltaic panels in a tropical environment10.1016/j.jenvman.2015.03.050 ↗
93. A custom high-throughput optical mapping instrument for accelerated stress testing of PV module materials
94. Degradation of anti-soiling coatings: mechanical impact of rainfall
95. S. Bhaduri, R. Bajhal, M. Farkade, S. Mallick, N. Shiradkar and A. Kottantharayil, “Understanding multiple stressors which degrade antisoiling coatings: combined effect of rain, abrasion, and UV radiation,” IEEE J PV, 13 (4), 603–609, doi: 10.1109/JPHOTOV.2023.3273812.10.1109/JPHOTOV.2023.3273812 ↗
96. Bobby To, “The IEC 62788-7-3 abrasion methods standard and supporting experiments at NREL on PV surfaces and coatings,”
97. Glass durability and breakage
98. Wolfertstetter · 2016
99. Particle sizing by means of the forward scattering lobe10.1364/AO.5.000839 ↗
100. Quantification of spectral losses of Natural soiling and detailed microstructural analysis of Dust collected from Different locations in Dubai, UAE