Potential-induced degradation of n-type front-emitter crystalline silicon photovoltaic modules — Comparison between indoor and outdoor test results
Source abstract
Abstract
We perform indoor and outdoor potential-induced degradation (PID) tests for n-type front-emitter (n-FE) crystalline Si (c-Si) photovoltaic (PV) modules and compare their results. The indoor/outdoor acceleration factor for the polarization-type PID (PID-p) of n-FE PV modules is found to be ∼1000 at an indoor test temperature of 85 °C. We observe the progression of the PID-p of n-FE PV modules in rainy days, while their performance is recovered in sunny days. This may be because of the formation of a water film on a module surface acting as a conductive film, resulting in a larger electric field near the n-FE cells in rainy days. The recovery of the PV performance of n-FE modules in sunny days can partly explain the large acceleration factor for the indoor PID test against the outdoor test.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Silicon and Solar Cell Technologies · Photovoltaic System Optimization Techniques · Thin-Film Transistor Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (38)
Show source-provided references
1. Potential-induced degradation in photovoltaic modules: a critical review10.1039/C6EE02271E ↗
2. The surface polarization effect in high-efficiency silicon solar cells
3. Characterization of multicrystalline silicon modules with system bias voltage applied in damp heat
4. Potential induced degradation of solar cells and panels
5. Microscopic aspects of potential-induced degradation phenomena and their recovery processes for p-type crystalline Si photovoltaic modules10.1016/j.cap.2016.10.001 ↗
6. Explanation of potential-induced degradation of the shunting type by Na decoration of stacking faults in Si solar cells10.1016/j.solmat.2013.06.015 ↗
7. Local corrosion of silicon as root cause for potential-induced degradation at the rear side of bifacial PERC solar cells10.1002/pssr.201900163 ↗
8. Assessing the causes of encapsulant delamination in PV modules
9. Universal explanation for degradation by charge accumulation in crystalline Si photovoltaic modules with application of high voltage10.7567/1882-0786/ab3cf7 ↗
10. N-type solar cells: advantages, issues, and current scenarios10.1088/2053-1591/aa6402 ↗
11. Potential induced degradation of n-type crystalline silicon solar cells with p+ front junction10.1002/ese3.146 ↗
12. Potential-induced degradation for encapsulated n-type IBC solar cells with front floating emitter10.1016/j.egypro.2015.07.050 ↗
13. Comparison of potential-induced degradation (PID) of n-type and p-type silicon solar cells10.1016/j.energy.2018.07.118 ↗
14. Investigation of the impact of illumination on the polarization-type potential-induced degradation of crystalline silicon photovoltaic modules10.1109/JPHOTOV.2018.2843791 ↗
15. Potential-induced degradation in photovoltaic modules based on n-type single crystalline Si solar cells10.1016/j.solmat.2015.04.037 ↗
16. Progression of rapid potential-induced degradation of n-type single-crystalline silicon photovoltaic modules10.7567/APEX.9.112301 ↗
17. Rapid progression and subsequent saturation of polarization-type potential-induced degradation of n-type front-emitter crystalline-silicon photovoltaic modules10.7567/JJAP.57.122301 ↗
18. Multistage performance deterioration in n-type crystalline silicon photovoltaic modules undergoing potential-induced degradation10.1016/j.microrel.2018.03.018 ↗
19. Influence of sodium on the potential-induced degradation for n-type crystalline silicon photovoltaic modules10.7567/1882-0786/ab1b1a ↗
20. Influence of backsheet materials on potential-induced degradation in n-type crystalline-silicon photovoltaic cell modules10.7567/1347-4065/ab4fd2 ↗
21. Effect of a SiO2 film on the potential-induced degradation of n-type front-emitter crystalline silicon photovoltaic modules10.35848/1347-4065/abb39e ↗
22. Effect of a silicon nitride film on the potential-induced degradation of n-type front-emitter crystalline silicon photovoltaic modules10.35848/1347-4065/abb39e ↗
23. Effects of passivation configuration and emitter surface doping concentration on polarization-type potential-induced degradation in n-type crystalline-silicon photovoltaic modules10.1016/j.solmat.2021.111074 ↗
24. Potential-induced degradation in high-efficiency n-type crystalline-silicon photovoltaic modules: a literature review10.1002/solr.202100708 ↗
25. Influence of light irradiation on the charge-accumulation-type potential-induced degradation of n-type front-emitter crystalline Si photovoltaic modules10.35848/1347-4065/ac279f ↗
26. Changes in the current density-voltage and external quantum efficiency characteristics of n-type single-crystalline silicon photovoltaic modules with a rear-side emitter undergoing potential-induced degradation10.1016/j.solmat.2016.03.003 ↗
27. Reduction in the short-circuit current density of silicon heterojunction photovoltaic modules subjected to potential-induced degradation tests10.1016/j.solmat.2016.12.027 ↗
28. Comprehensive study of potential-induced degradation in silicon heterojunction photovoltaic cell modules10.1002/pip.3006 ↗
29. Influence of emitter position of silicon heterojunction photovoltaic solar cell modules on their potential-induced degradation behaviors10.1016/j.solmat.2020.110716 ↗
30. Influence of hygrothermal stress on potential-induced degradation for homojunction and heterojunction crystalline Si photovoltaic modules10.35848/1347-4065/ab9a8a ↗
31. Influence of light illumination on the potential-induced degradation of n-type interdigitated back-contact crystalline Si photovoltaic modules10.35848/1347-4065/abd9cf ↗
32. Effect of temperature and pre-annealing on the potential-induced degradation of silicon heterojunction photovoltaic modules10.35848/1347-4065/ac3f6e ↗
33. Comparison between indoor and outdoor test results on potential-induced degradation behavior for n-type front-emitter crystalline Si photovoltaic modules
34. Potential-induced degradation of n-type crystalline Si photovoltaic modules in practical outdoor systems10.7567/JJAP.57.117102 ↗
35. Crystalline Si photovoltaic modules based on TiO2-coated cover glass against potential-induced degradation10.1039/C4RA06791F ↗
36. Elucidating potential‐induced degradation in bifacial PERC silicon photovoltaic modules10.1002/pip.3028 ↗
37. Impact of illumination and encapsulant resistivity on polarization-type potential-induced degradation on n-PERT cells10.1002/pip.3505 ↗
38. Effects of SiNx refractive index and SiO2 thickness on polarization-type potential-induced degradation in front-emitter n-type crystalline-silicon photovoltaic cell modules10.1002/ese3.1135 ↗