journal article·2022-03

Investigating the degradation behaviours of n+-doped Poly-Si passivation layers: An outlook on long-term stability and accelerated recovery

Daniel Chen, Chukwuka Madumelu, Moonyong Kim, Bruno Vicari Stefani, Anastasia Soeriyadi, Di Kang, Hang Cheong Sio, Xinyu Zhang, Peng Zhu, Brett Hallam, Matthew Wright

Publisher page

Abstract

In this article, we study the kinetics of firing-activated degradation and recovery of industrially processed n+-doped poly-Si on thin oxide passivation layers subjected to illuminated annealing at elevated temperatures. The impact of a comprehensive range of fast-firing conditions on the subsequent degradation and recovery were assessed. The results indicate that the recovery process is dependent on the peak firing temperature, where higher temperatures led to an improvement in effective lifetime of up to 20% compared to the pre-fired state, and a very low surface dark saturation current density of 2.9 fA/cm2. By cycling through light soaking and dark anneal conditions, we show that unlike the commonly studied boron-oxygen light-induced degradation (BO-LID) and light- and elevated temperature-induced degradation (LeTID), this newly observed instability in n+-doped poly-Si passivation layers is not reversible, that is, once a degradation/recovery cycle is completed, the lifetime remains very stable under subsequent light soaking. This indicates that the surface related instability may be able to be completely resolved following the completion of the first degradation/recovery cycle. With this in mind, we investigate the potential for high intensity laser illumination (up to 150 kW/m2) to rapidly increase the recovery rates, however, this does not seem sufficient to cycle through degradation and recovery on a timescale that is amenable with mass production. The mitigation of any potential instabilities at the poly-Si interface has significant implications for the reliability of n-type tunneling oxide passivated contact (TOPCon) solar cells. ; This work has been supported by the Australian Government through the Australian Renewable Energy Agency (ARENA) (RND010, RND017 and 1-A060) and the Key Project of Zhejiang Province (No. 2018C01034). Daniel Chen and Moonyong Kim would like to acknowledge the support of the Australian Centre for Advanced Photovoltaics (ACAP).
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Silicon and Solar Cell Technologies · Thin-Film Transistor Technologies · Silicon Nanostructures and Photoluminescence

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (34)

Show source-provided references
1. Upgrade PERC with TOPCon: efficiency potential by taking into account the electrical gains and optical losses, 36th
2. 24.58% total area efficiency of screen-printed, large area industrial silicon solar cells with the tunnel oxide passivated contacts (i-TOPCon) design10.1016/j.solmat.2019.110258 ↗
3. Hydrogen induced degradation: a possible mechanism for light- and elevated temperature- induced degradation in n-type silicon10.1016/j.solmat.2018.05.034 ↗
4. Hydrogen-induced degradation: explaining the mechanism behind light- and elevated temperature-induced degradation in n- and p-type silicon10.1016/j.solmat.2019.110353 ↗
5. Light and elevated temperature induced degradation in p-type and n-type cast-grown multicrystalline and mono-like silicon10.1016/j.solmat.2018.03.002 ↗
6. The value of efficiency in Photovoltaics10.1016/j.joule.2019.07.028 ↗
7. Effect of carrier-induced hydrogenation on the passivation of the poly-Si/SiOx/c-Si interface10.1063/1.5049289 ↗
8. Degradation and regeneration of n+-doped poly-Si surface passivation on p-type and n-type Cz-Si under illumination and dark annealing10.1109/JPHOTOV.2020.2964987 ↗
9. Influence of hydrogenated passivation layers on the regeneration of boron-oxygen related defects
10. Long-term stability study of the passivation quality of polysilicon-based passivation layers for silicon solar cells10.1016/j.solmat.2020.110691 ↗
11. Degradation of carrier lifetime in Cz silicon solar cells10.1016/S0927-0248(00)00098-2 ↗
12. Firing stability of SiNy/SiNx stacks for the surface passivation of crystalline silicon solar cells10.1016/j.solmat.2011.09.051 ↗
13. Kang
14. Firing stability of tube furnace-annealed n-type poly-Si on oxide junctions
15. Mass production of industrial tunnel oxide passivated contacts (i-TOPCon) silicon solar cells with average efficiency over 23% and modules over 345 W10.1002/pip.3180 ↗
16. Transparent electrodes consisting of a surface-treated buffer layer based on tungsten oxide for semitransparent perovskite solar cells and four-terminal tandem applications
17. Evidence of an identical firing-activated carrier-induced defect in monocrystalline and multicrystalline silicon10.1016/j.solmat.2017.08.003 ↗
18. Bulk and surface-related degradation in lifetime samples made of Czochralski silicon passivated by plasma-enhanced chemical vapor deposited layer stacks10.1002/pssa.201800741 ↗
19. Vacancy and vacancy-hydrogen complexes in silicon10.1103/PhysRevB.49.17040 ↗
20. Deep levels of copper-hydrogen complexes in silicon10.1103/PhysRevB.88.085205 ↗
21. Deep level of iron-hydrogen complex in silicon10.1063/1.365746 ↗
22. Investigation of carrier lifetime instabilities in Cz-grown silicon
23. A four-state kinetic model for the carrier-induced degradation in multicrystalline silicon: introducing the reservoir state10.1016/j.solmat.2018.04.024 ↗
24. Accelerated formation of the boron-oxygen complex in p-type Czochralski silicon10.1002/pssr.201510064 ↗
25. Acceleration and mitigation of carrier-induced degradation in p-type multi-crystalline silicon10.1002/pssr.201510437 ↗
26. Advanced hydrogenation of dislocation clusters and boron-oxygen defects in silicon solar cells
27. Rapid passivation of carrier-induced defects in p-type multi-crystalline silicon10.1016/j.solmat.2016.05.022 ↗
28. Influence of the formation- and passivation rate of boron-oxygen defects for mitigating carrier-induced degradation in silicon within a hydrogen-based model10.1063/1.4941387 ↗
29. Temporary recovery of the defect responsible for light- and elevated temperature-induced degradation: insights into the physical mechanisms behind LeTID10.1109/JPHOTOV.2020.3025240 ↗
30. On the meaning(fullness) of the intensity unit ‘suns’ in light induced degradation experiments10.1016/j.egypro.2017.09.339 ↗
31. Rapid mitigation of carrier-induced degradation in commercial silicon solar cells10.7567/JJAP.56.08MB13 ↗
32. Eliminating light- and elevated temperature-induced degradation in P-type PERC solar cells by a two-step thermal process10.1016/j.solmat.2020.110470 ↗
33. Optimization of belt furnace anneal to reduce light and elevated temperature induced degradation of effective carrier lifetime of P-type multicrystalline silicon wafers10.1002/solr.201800070 ↗
34. Production compatible remedy against LETID in high-performance multicrystalline silicon solar cells, 35th