Fragmentation of photovoltaic backsheets after accelerated weathering exposure
Source abstract
Abstract
Abstract The backsheet of a photovoltaic (PV) module functions primarily to provide safe operation through electrical insulation and protect the interior from environmental exposure. For most applications, backsheets consist of opaque, but highly reflective, films that protect inner layers from degradation from ultraviolet (UV) light. Backsheets can fail if they delaminate or form cracks under strain. In a PV module, the maximum strains that can be applied are only on the order of a few percent. The greatest strains are likely to be highly localized around topographical features. Therefore, to assess the likelihood of a crack being initiated in a backsheet, we apply small amplitude strains to backsheet films under microscopic examination using a laser scanning confocal microscope. This allows us to monitor both the depth and density of cracks as well as the onset strain. Here we perform these measurements after exposure to UV light.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Photovoltaic System Optimization Techniques · Integrated Circuits and Semiconductor Failure Analysis · Non-Destructive Testing Techniques
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (31)
Show source-provided references
1. Lyu · 2018 · 1
2. Owen-Bellini · 2018
3. Rummens · 2018 · 2018
4. A comparison of key PV backsheet and module performance from fielded module exposures and accelerated tests10.1109/JPHOTOV.2014.2305472 ↗
5. Gambogi · 2015
6. Hu · 2016
7. Trout · 2018
8. Eder · 2019
9. Depth profiling of chemical and mechanical degradation of UV-exposed PV backsheets
10. E. F. Cuddihy, C. D. Coulbert, A. Gupta, and R. Liang, "Electricity from photovoltaic solar cells, flat-plate solar array project final report, Volume VII: Module Encapsulation," DOE/JPL-1012-125, 1986.
11. Kempe · 2019
12. Choudhury · 2018
13. Effect of coefficient of thermal expansion (CTE) mismatch of solder joint materials in photovoltaic (PV) modules operating in elevated temperature climate on the joint's damage10.1016/j.promfg.2017.07.236 ↗
14. The effect of cooling press on the encapsulation properties of crystalline photovoltaic modules: residual stress and adhesion10.1002/pip.2409 ↗
15. Eitner · 2009 · 1280
16. Survey of mechanical durability of PV backsheets
17. 2017
18. ASTM D7869 - 13, Standard practice for xenon arc exposure test with enhanced light and water exposure for transportation coatings.".
19. A novel test method for quantifying cracking propensity of photovoltaic backsheets after ultraviolet exposure10.1002/pip.3038 ↗
20. Iec · 2017
21. 2016
22. Cracking and microstructural changes of PVDF-based backsheets during aging
23. Gu · 2019 · 20899
24. Effect of TiO2 on morphology and mechanical properties of PVDF/PMMA blend films prepared by melt casting process10.1002/app.40454 ↗
25. Properties and applications of the β phase poly(vinylidene fluoride)10.3390/polym10030228 ↗
26. Ftir and dsc studies OF mechanically deformed β-PVDF films10.1081/MB-100106174 ↗
27. Effect of crystallization temperature on the crystalline phase content and morphology of poly(vinylidene fluoride)10.1002/polb.1994.090320509 ↗
28. Studies on the transformation process of PVDF from α to β phase by stretching10.1039/C3RA45134H ↗
29. A non-destructive method for crack quantification in photovoltaic backsheets under accelerated and real-world exposures10.1016/j.polymdegradstab.2018.05.008 ↗
30. Drivers for the cracking of multilayer polyamide-based backsheets in field photovoltaic modules: in-depth degradation mapping analysis
31. Evaluation of the uncertainty in accelerated stress testing