Degradation of plated silicon solar module due to copper diffusion: The role of capping layer formation and contact adhesion
Source abstract
Abstract
Abstract Copper plating can provide significant cost savings over screen printed Ag for industrially produced Si photovoltaic modules, however concerns exist with regard to the durability of Cu-plated modules. This study investigated the effect of different capping layers and their method of application on the durability of Cu-plated PERC one-cell modules, with a focus on durability after damp heat (DH) testing. It is shown that the adhesion of Cu-plated fingers capped with immersion-plated Ag and Sn was poorer than that of fingers capped with light-induced plated (LIP) Ag due to the under-etching of Cu finger by corrosive additives that are present in the immersion plating formulations. It is proposed that the weak finger adhesion resulted in fingers dislodging during DH testing of the modules, thereby opening a pathway for Cu to in-diffuse into Si resulting initially in an increased non-ideal recombination and then increased series resistance due to encapsulant flowing under the dislodged finger. Increased recombination due to the Cu in-diffusion was evident in cells with poor finger adhesion through an increase of the non-ideal recombination current density, J02, of 166%, 253%, 266% for LIP Ag, immersion Ag and immersion Sn, respectively, during the first 1000 h of DH. In comparison, with stronger finger adhesion, J02 increases were
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Silicon and Solar Cell Technologies · Thin-Film Transistor Technologies · Integrated Circuits and Semiconductor Failure Analysis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (67)
Show source-provided references
1. ITRPV · 2019
2. Industrial Si solar cells with Cu-based plated contacts10.1109/JPHOTOV.2015.2478067 ↗
3. Addressing perceived barriers to the adoption of plated metallisation for silicon photovoltaic manufacturing
4. Evolution of metal plating for silicon solar cell metallisation10.1002/pip.2221 ↗
5. Large area copper plated silicon solar cell exceeding 19.5% efficiency10.1016/j.egypro.2012.05.008 ↗
6. Challenges facing copper-plated metallisation for silicon photovoltaics: insights from integrated circuit technology development10.1002/pip.3062 ↗
7. Untangling the mysteries of plated metal finger adhesion: understanding the contributions from plating rate, chemistry, grid geometry, and sintering10.1109/JPHOTOV.2016.2589364 ↗
8. Monitoring of adhesion for plated metallisation: why busbar pull tests are not sufficient10.1016/j.egypro.2016.07.110 ↗
9. Impact of contact integrity during thermal stress testing on degradation analysis of copper-plated silicon solar cells10.1016/j.solmat.2017.09.005 ↗
10. Copper penetration in laser-doped selective-emitter silicon solar cells with plated nickel barrier layers10.1016/j.solmat.2014.07.026 ↗
11. Barrier properties of electroplating nickel layer for copper metallization in silicon solar cells10.20964/2018.12.23 ↗
12. Electrical characterization of thermally-formed nickel silicide for nickel-copper plated solar cell contacts
13. Diffusion, solubility and gettering of copper in silicon10.1016/S0921-5107(99)00514-0 ↗
14. Electrical properties and recombination activity of copper, nickel and cobalt in silicon10.1007/s003390050649 ↗
15. Interstitial copper-related center in n-type silicon10.1063/1.120026 ↗
16. Characterization of metallic impurities in Si using a recombination-lifetime correlation method10.1063/1.365632 ↗
17. Electric degradation and defect formation of silicon due to Cu, Fe, and Ni contamination10.1557/PROC-262-641 ↗
18. Recombination activity of copper in silicon10.1063/1.1415350 ↗
19. Addressing adhesion and reliability concerns of copper-plated c-Si solar cells and modules
20. Electrical and mechanical properties of plated Ni/Cu contacts for Si solar cells10.1016/j.egypro.2015.07.104 ↗
21. A simple copper metallisation process for high cell efficiencies and reliable modules
22. Low cost metallisation based on Ni/Cu plating enabling high efficiency industrial solar cells
23. Degradation studies including light-induced degradation of c-Si solar cells with nickel-copper plated contacts
24. Pilot production of highly efficient metal catalyzed textured diamond wire sawn mc-Si solar cells combined with nickel-copper plated front contact processing10.1016/j.egypro.2017.09.407 ↗
25. Reliable contact formation for industrial solar cells by laser ablation and Ni/Cu plating
26. Damp heat induced degradation of silicon heterojunction solar cells with Cu-plated contacts10.1109/JPHOTOV.2019.2941693 ↗
27. Towards 20% efficient silicon solar cells manufactured at 60 MWp per annum
28. M. Alonso-Abella, F. Chenlo, A. Alonso, D. González, T. Corporation, Toledo PV plant 1 MWp – 20 Years of operation, in: 29th European Photovoltaic Solar Energy Conference and Exhibition, WIP, pp. 1-14.
29. Dielectric patterning using aerosol jet printing10.2352/J.ImagingSci.Technol.2012.56.4.040502 ↗
30. Forming openings to semiconductor layers of silicon solar cells by inkjet printing10.1016/j.solmat.2008.05.018 ↗
31. Patterning for plated heterojunction cells10.1016/j.egypro.2015.03.290 ↗
32. Patterning and metallization of silicon solar cells by inkjet-printed functional ink on a photoresist layer
33. Influence of the ARC patterning method and annealing on the contact adhesion of Ni/Cu-plated solar cells10.3938/jkps.68.1109 ↗
34. Damage-free laser patterning of silicon nitride on textured crystalline silicon using an amorphous silicon etch mask for Ni/Cu plated silicon solar cells10.1016/j.tsf.2016.06.011 ↗
35. Easy plating—a simple approach to suppress parasitically metallized areas in front side Ni/Cu plated crystalline Si solar cells10.1109/JPHOTOV.2017.2720461 ↗
36. Optimizing adhesion of laser structured plated Ni-Cu contacts with insights from micro characterization10.1016/j.egypro.2016.07.101 ↗
37. Interface oxides in femtosecond laser structured plated Ni-Cu-Ag contacts for silicon solar cells10.1016/j.solmat.2017.03.016 ↗
38. Experimental study on the elimination of over-plating problems in industrial manufacturing of large-area acidic-textured laser-doped multi-crystalline solar cells10.1016/j.solmat.2012.08.019 ↗
39. Pulse plating of semiconductors for solar cells10.1016/j.solener.2014.03.003 ↗
40. Laser chemical metal deposition for silicon solar cell metallization10.1016/j.egypro.2012.05.007 ↗
41. Characterization of electroless nickel as a seed layer for silicon solar cell metallization10.1007/s12034-014-0828-1 ↗
42. A study on characterization of light-induced electroless plated Ni seed layer and silicide formation for solar cell application10.3938/jkps.72.615 ↗
43. 266-nm ps laser ablation for copper-plated p-type selective emitter PERC silicon solar cells10.1109/JPHOTOV.2018.2834629 ↗
44. Microstructure analysis of the interface situation and adhesion of thermally formed nickel silicide for plated nickel–copper contacts on silicon solar cells10.1016/j.solmat.2013.06.005 ↗
45. Electroless nickel deposition and silicide formation for advanced front side metallization of industrial silicon solar cells10.1016/j.egypro.2012.05.006 ↗
46. Plated metal adhesion to picosecond laser-ablated silicon solar cells: influence of surface chemistry and wettability
47. Plated contacts for solar cells with superior adhesion strength to screen printed solar cells10.1007/s11708-016-0428-4 ↗
48. Ni/Cu/Ag plated contacts: a study of resistivity and contact adhesion for crystalline-Si solar cells10.1007/s13391-016-4003-2 ↗
49. Adhesion strength of plated Ni/Cu metallization in Si solar cells10.1007/s10854-018-00631-z ↗
50. Improved metal adhesion with galvanic nickel plating to silicon solar cells10.1016/j.solmat.2016.12.012 ↗
51. Copper and silicon : implications for the long-term stability of plated contacts for silicon solar cells
52. Impact of laser-induced oxidation on silicon wafer solar cells' performance10.1109/JPHOTOV.2016.2535243 ↗
53. Design and characterization of an adhesion strength tester for evaluating metal contacts on silicon solar cells
54. Towards a more reliable manufacturing future – automatic classification of failure modes during adhesion testing of silicon solar cells10.1016/j.solener.2018.12.004 ↗
55. Failure modes identified during adhesion testing of metal fingers on silicon solar cells
56. The effect of accelerated aging tests on the optical properties of silicone and EVA encapsulants
57. The effect of damp-heat and UV aging tests on the optical properties of silicone and EVA encapsulants10.1002/pip.1025 ↗
58. Modeling of voids evolution in the encapsulation process of photovoltaic modules
59. Light-induced degradation in copper-contaminated gallium-doped silicon10.1002/pssr.201307011 ↗
60. The precipitation behaviour of copper in silicon single crystals10.1002/pssb.19650120125 ↗
61. Microprobe investigations of copper precipitates in silicon single crystals10.1002/pssb.19670210221 ↗
62. Copper precipitation at the silicon-silicon-dioxide interface: role of oxygen10.1143/JJAP.33.1217 ↗
63. Oxygen and copper precipitation at the silicon/silicon dioxide interface10.4028/www.scientific.net/SSP.32-33.191 ↗
64. Kirkendall voids in the intermetallic layers of solder joints in MEMS10.1016/j.commatsci.2008.09.028 ↗
65. Study of annealing temperature for Ni/Cu/Ag plated front contact single crystalline solar cells10.1109/JPHOTOV.2016.2576683 ↗
66. Leaching of copper from malachite with methane-sulfonic acid
67. Leaching studies for copper and solder alloy recovery from shredded particles of waste printed circuit boards10.1007/s11663-018-1243-6 ↗