Effects of passivation configuration and emitter surface doping concentration on polarization-type potential-induced degradation in n-type crystalline-silicon photovoltaic modules
Source abstract
Abstract
Abstract System voltages can cause significant degradation in photovoltaic modules. Polarization-type potential-induced degradation (PID) is accompanied by decreases in the short-circuit current density and the open-circuit voltage. The system voltage causes a polarization and surface charge accumulation, increasing the interface recombination. The surface passivation and the emitter doping concentration and gradient are considered to have large impacts. However, a systematic study on these effects has not yet been performed. In this paper, the effects of the front surface structure of n-type passivated emitter and rear totally diffused cell modules were investigated by accelerated PID tests. Standard cells with thin silicon dioxide/80-nm silicon nitride (SiNx) antireflection/passivation layers, refractive index (RI) of 2.0, exhibited typical polarization-type PID. Cells with increased RI = 2.4 for the bottom 20-nm SiNx showed no degradation at all. This may be caused by reduced charge accumulation in the SiNx layer near the interface due to the higher electrical conductivity of the Si-rich bottom layer. Secondly, cells with both a highly distorted interface, due to nitrogen insertion in the silicon surface, and an emitter with a high surface doping concentration have excellent resistance to PID. Cells with either the highly distorted interface or the higher emitter-surface doping concentration show no to minor improved resistance to PID. These findings improve the understanding of the effects of the front surface structure of cells on the polarization-type PID and may contribute to the implementation of these measures to reduce PID.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Silicon and Solar Cell Technologies · Photovoltaic System Optimization Techniques · Thin-Film Transistor Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (30)
Show source-provided references
1. Recombination activity of interstitial iron and other transition metal point defects in p- and n-type crystalline silicon10.1063/1.1812833 ↗
2. Advancements in n-type base crystalline silicon solar cells and their emergence in the photovoltaic industry10.1155/2013/470347 ↗
3. Investigation of carrier lifetime instabilities in Cz-grown silicon
4. Degradation of carrier lifetime in Cz silicon solar cells10.1016/S0927-0248(00)00098-2 ↗
5. Potential-induced degradation in photovoltaic modules: a critical review10.1039/C6EE02271E ↗
6. Potential induced degradation of solar cells and panels
7. Potential induced degradation of solar cells and panels
8. Characterization of multicrystalline silicon modules with system bias voltage applied in damp heat
9. The role of stacking faults for the formation of shunts during potential-induced degradation of crystalline Si solar cells10.1002/pssr.201307090 ↗
10. Explanation of potential-induced degradation of the shunting type by Na decoration of stacking faults in Si solar cells10.1016/j.solmat.2013.06.015 ↗
11. Potential-induced degradation in photovoltaic modules based on n-type single crystalline Si solar cells10.1016/j.solmat.2015.04.037 ↗
12. Progression of rapid potential-induced degradation of n-type single-crystalline silicon photovoltaic modules10.7567/APEX.9.112301 ↗
13. Rapid progression and subsequent saturation of polarization-type potential-induced degradation of n-type front-emitter crystalline-silicon photovoltaic modules10.7567/JJAP.57.122301 ↗
14. Multistage performance deterioration in n-type crystalline silicon photovoltaic modules undergoing potential-induced degradation10.1016/j.microrel.2018.03.018 ↗
15. Effect of a SiO2 layer on the potential-induced degradation of n-type front-emitter crystalline Si photovoltaic modules10.7567/1347-4065/ab4cf9 ↗
16. Potential induced degradation of n-type crystalline silicon solar cells with p+ front junction10.1002/ese3.146 ↗
17. Investigation of potential-induced degradation in n-PERT bifacial silicon photovoltaic modules with a glass/glass structure10.1109/JPHOTOV.2017.2762587 ↗
18. Investigation of the impact of illumination on the polarization-type potential-induced degradation of crystalline silicon photovoltaic modules10.1109/JPHOTOV.2018.2843791 ↗
19. PID- and UVID-free n-type solar cells and modules10.1016/j.egypro.2016.07.026 ↗
20. The surface polarization effect in high-efficiency silicon solar cells
21. Annual degradation rates of recent crystalline silicon photovoltaic modules10.1002/pip.2903 ↗
22. Potential-induced degradation for encapsulated n-type IBC solar cells with front floating emitter10.1016/j.egypro.2015.07.050 ↗
23. Elucidating potential-induced degradation in bifacial PERC silicon photovoltaic modules10.1002/pip.3028 ↗
24. Universal explanation for degradation by charge accumulation in crystalline Si photovoltaic modules with application of high voltage10.7567/1882-0786/ab3cf7 ↗
25. Minimizing the polarization-type potential-induced degradation in PV modules by modification of the dielectric antireflection and passivation stack10.1109/JPHOTOV.2019.2896944 ↗
26. Influence of sodium on the potential-induced degradation for n-type crystalline silicon photovoltaic modules10.7567/1882-0786/ab1b1a ↗
27. Nitric acid pretreatment for the passivation of boron emitters for n-type base silicon solar cells10.1063/1.2870202 ↗
28. Examination of the properties of the interface of a-SiNx:H/Si in crystalline silicon solar cells and its effect on cell efficiency10.1557/opl.2012.56 ↗
29. The interface of a-SiNx:H and Si: linking the nano-scale structure to passivation quality10.1016/j.solmat.2013.04.026 ↗
30. Potential-induced degradation of Cu(In,Ga)Se2 photovoltaic modules10.7567/JJAP.54.08KC13 ↗