journal article·2018-08Open access

Superacid-derived surface passivation for measurement of ultra-long lifetimes in silicon photovoltaic materials

A.I. Pointon, N.E. Grant, E.C. Wheeler-Jones, P.P. Altermatt, J.D. Murphy

Abstract

Accurate measurements of bulk minority carrier lifetime are essential in order to determine the true limit of silicon's performance and to improve solar cell production processes. The thin film which forms when silicon wafers are dipped in solutions containing superacids such as bis(trifluoromethane)sulfonimide (TFSI) has recently been found to be effective at electronically passivating the silicon surface. In this paper we first study the role of the solvent in which TFSI is dissolved for the passivation process. We study ten solvents with a wide range of relative polarities, finding TFSI dissolved in hexane provides improved temporal stability, marginally better passivation and improved solution longevity compared to dichloroethane which has been used previously. Sample storage conditions, particularly humidity, can strongly influence the passivation stability. The optimised TFSI-hexane passivation scheme is then applied to a set of 3 Ω cm n-type wafers cut from the same float-zone ingot to have different thicknesses. This enables the reproducibility of the scheme to be systematically evaluated. At 1015 cm−3 injection the best case effective surface recombination velocity is 0.69 ± 0.04 cm/s, with bulk lifetimes measured up to the intrinsic lifetime limit at high injection and >43 ms at lower injection. Immersion of silicon in superacid-based ionic solutions therefore provides excellent surface passivation, and, as it is applied at room temperature, the effects on true bulk lifetime are minimal.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Silicon and Solar Cell Technologies · Semiconductor materials and interfaces · Thin-Film Transistor Technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (35)

Show source-provided references
1. Y. Wan, K.R. McIntosh, A.F. Thomson, A. Cuevas, "Low surface recombination velocity by low-absorption silicon nitride on c-Si". Proceedings of the 38th IEEE Photovoltaic Specialists Conference (PVSC) (Austin, TX, USA), doi: 10.1109/PVSC-Vol 2.2013.6656792, 2012.
2. Superacid-treated silicon surfaces: extending the limit of carrier lifetime for photovoltaic applications10.1109/JPHOTOV.2017.2751511 ↗
3. Unexpectedly high minority-carrier lifetimes exceeding 20 ms measured on 1.4-Ω cm n-type silicon wafers10.1002/pssr.201700235 ↗
4. Long-term stability of aluminum oxide based surface passivation schemes under illumination at elevated temperatures10.1109/JPHOTOV.2017.2713411 ↗
5. Extremely low surface recombination in 1 Ω cm n-type monocrystalline silicon10.1002/pssr.201600307 ↗
6. Improved quantitative description of Auger recombination in crystalline silicon10.1103/PhysRevB.86.165202 ↗
7. Dielectric surface passivation for silicon solar cells: a review10.1002/pssa.201700293 ↗
8. Gettering of interstitial iron in silicon by plasma-enhanced chemical vapour deposited silicon nitride films10.1063/1.4967914 ↗
9. Temporary surface passivation for characterisation of bulk defects in silicon: a review10.1002/pssr.201700243 ↗
10. Superacid passivation of crystalline silicon surfaces10.1021/acsami.6b07822 ↗
11. Minimising bulk lifetime degradation during the processing of interdigitated back contact silicon solar cells10.1002/pip.2928 ↗
12. 1,2-Dichloroethane. IARC Monographs on the Evaluation of Carcinogenic Risks to Humans (Lyon, France), 71, 1999, p. 501.
13. Stabilized cycling performance of silicon oxide anode in ionic liquid electrolyte for rechargeable lithium batteries10.1039/c2ra01183b ↗
14. Grown-in defects limiting the bulk lifetime of p-type float-zone silicon wafers10.1063/1.4907804 ↗
15. Thermal activation and deactivation of grown-in defects limiting the lifetime of float-zone silicon10.1002/pssr.201600080 ↗
16. Permanent annihilation of thermally activated defects which limit the lifetime of float-zone silicon10.1002/pssa.201600360 ↗
17. The effect of sample edge recombination on the averaged injection-dependent carrier lifetime in silicon10.1063/1.3691230 ↗
18. Injection dependence of the effective lifetime of n-type Si passivated by Al2O3: an edge effect?10.1016/j.solmat.2013.06.049 ↗
19. Reichardt · 2011
20. Inter-laboratory study of eddy-current measurement of excess-carrier recombination lifetime10.1109/JPHOTOV.2013.2284375 ↗
21. Temperature dependence of the radiative recombination coefficient of intrinsic crystalline silicon10.1063/1.1610231 ↗
22. Injection dependence of spontaneous radiative recombination in crystalline silicon: experimental verification and theoretical analysis10.1063/1.2218041 ↗
23. Interpretation of recombination at c-Si/SiNx interfaces by surface damage10.1063/1.3437643 ↗
24. Capture cross sections of defect states at the Si/SiO2 interface10.1063/1.373746 ↗
25. Effect of boron concentration on recombination at the p-Si–Al2O3 interface10.1063/1.4867643 ↗
26. Properties of the c-Si/Al2O3 interface of ultrathin atomic layer deposited Al2O3 layers capped by SiNx for c-Si surface passivation10.1063/1.4903483 ↗
27. Unusually low surface-recombination velocity on silicon and germanium surfaces10.1103/PhysRevLett.57.249 ↗
28. Selective catalytic self-condensation of acetone10.1016/0304-5102(89)80134-8 ↗
29. Pathway to vinyl chloride production via dehydrochlorination of 1,2-dichloroethane in ionic liquid media
30. Direct Synthesis of dimethylbiphenyls by toluene coupling in the presence of palladium triflate and triflic acid10.1006/jcat.1999.2616 ↗
31. Isomerization of substituted biphenyls by superacid. a remarkable confluence of experiment and theory10.1021/jo0106445 ↗
32. The molecular complexity of water in organic solvents. Part II10.1021/ba-1966-0052 ↗
33. Solubility of water in hydrocarbons as a function of water activity10.1016/0039-9140(68)80050-5 ↗
34. Light-induced activation and deactivation of bulk defects in boron-doped float-zone silicon10.1063/1.4983024 ↗
35. Degradation of surface passivation on crystalline silicon and its impact on light-induced degradation experiments10.1109/JPHOTOV.2017.2755072 ↗