Reduction in the short-circuit current density of silicon heterojunction photovoltaic modules subjected to potential-induced degradation tests
Source abstract
Abstract
Abstract This letter deals with the potential-induced degradation (PID) of silicon heterojunction (SHJ) photovoltaic (PV) modules. After rapid indoor PID tests applying a voltage of −1000 V at 85 °C, the modules exhibited a significant reduction in short-circuit current density ( J sc ). On the other hand, the dark current density–voltage characteristics of the modules were intact after the PID tests, indicating that the reduction in J sc is attributed not to carrier recombination but to optical loss. A degraded module slightly recovered its performance loss upon applying a positive bias but complete recovery was not observed, showing that the PID of SHJ PV modules is not reversible. A module with an ionomer encapsulant showed high PID resistance, revealing that the degradation of SHJ PV modules can be prevented by the use of ionomer encapsulants.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Silicon and Solar Cell Technologies · Photovoltaic System Optimization Techniques · Integrated Circuits and Semiconductor Failure Analysis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (40)
Show source-provided references
1. High-efficiency silicon heterojunction solar cells: a review10.1515/green-2011-0018 ↗
2. Development status of high-efficiency HIT solar cells10.1016/j.solmat.2010.04.030 ↗
3. T. Kinoshita, D. Fujishima, A. Yano, A. Ogane, S. Tohoda, K. Matsuyama, Y. Nakamura, N. Tokuoka, H. Kanno, H. Sakata, M. Taguchi, E. Maruyama, The approaches for high efficiency HIT solar cell with very thin (<100μm) silicon wafer over 23%, in: Proceedings of the 26th European Photovoltaic Solar Energy Conference and Exhibition, 5–9 September, Hamburg, Germany, 2011, pp. 871–874.
4. 24.7% record efficiency HIT solar cell on thin silicon wafer10.1109/JPHOTOV.2013.2282737 ↗
5. Impact of carrier recombination on fill factor for large area heterojunction crystalline silicon solar cell with 25.1% efficiency10.1063/1.4937224 ↗
6. Achievement of more than 25% conversion efficiency with crystalline silicon heterojunction solar cell10.1109/JPHOTOV.2014.2352151 ↗
7. Kaneka Corporation, World’s highest conversion efficiency of 26.33% achieved in a crystalline silicon solar cell —A world first in a practical cell size—, http://www.kaneka.co.jp/kaneka-e/images/topics/1473811995/1473811995_101.pdf, 2016 (accessed 12.10.16).
8. SEMI PV Group Europe, International Technology Roadmap for Photovoltaic (ITRPV). 〈http://www.itrpv.net/〉, 2016 (accessed 23.05.16).
9. S. Pingel, O. Frank, M. Winkler, S. Daryan, T. Geipel, H, Hoehne, J. Berghold, Potential induced degradation of solar cells and panels, in: Proceedings of the 35th IEEE Photovoltaic Specialists Conference, 20–25 June, Honolulu, HI, USA, 2010, pp. 2817–2822.10.1109/PVSC.2010.5616823 ↗
10. J. Berghold, O. Frank, H. Hoehne, S. Pingel, B. Richardson, M. Winkler, Potential induced degradation of solar cells and panels, in: Proceedings of the 25th European Photovoltaic Solar Energy Conference and Exhibition/5th World Conference on Photovoltaic Energy Conversion, 6–10 September, Valencia, Spain, 2010, pp. 3753–3759.
11. P. Hacke, M. Kempe, K. Terwilliger, S. Glick, N. Call, S. Johnston, S. Kurtz, I. Bennett, M. Kloos, Characterization of multicrystalline silicon modules with system bias voltage applied in damp heat, in: Proceedings of the 25th European Photovoltaic Solar Energy Conference and Exhibition/5th World Conference on Photovoltaic Energy Conversion, 6–10 September, Valencia, Spain, 2010, pp. 3760–3765.
12. PV module durability testing under high voltage biased damp heat conditions10.1016/j.egypro.2011.06.154 ↗
13. T. Ishiguro, H. Kanno, M. Taguchi, S. Okamoto, Study on PID resistance of HIT PV modules, presented at 2013 Photovoltaic Module Reliability Workshop, 26–27 February, Golden, CO, USA, 2013.
14. N. Riedel, L. Pratt, E. Moss, M. Yamasaki, 600 hour potential induced degradation (PID) testing on silicon, CIGS, and HIT modules, presented at 2015 Photovoltaic Reliability Workshop, 24–27 February, Golden, CO, USA, 2015.
15. Micro structural root cause analysis of potential induced degradation in c-Si solar cells10.1016/j.egypro.2012.07.020 ↗
16. On the mechanism of potential-induced degradation in crystalline silicon solar cells10.1002/pssr.201206276 ↗
17. The role of stacking faults for the formation of shunts during potential-induced degradation of crystalline Si solar cells10.1002/pssr.201307090 ↗
18. Explanation of potential-induced degradation of the shunting type by Na decoration of stacking faults in Si solar cells10.1016/j.solmat.2013.06.015 ↗
19. Crystalline Si photovoltaic modules based on TiO2-coated cover glass against potential-induced degradation10.1039/C4RA06791F ↗
20. Crystalline Si photovoltaic modules functionalized by a thin polyethylene film against potential and damp-heat-induced degradation10.1039/C4RA13360A ↗
21. Relationship between cross-linking conditions of ethylene vinyl acetate and potential induced degradation for crystalline silicon photovoltaic modules
22. Consideration on Na diffusion and recovery phenomena in potential-induced degradation for crystalline Si photovoltaic modules10.7567/JJAP.55.02BF10 ↗
23. Behavior of the potential-induced degradation of photovoltaic modules fabricated using flat mono-crystalline silicon cells with different surface orientations10.7567/JJAP.55.04ES14 ↗
24. Potential-induced degradation in photovoltaic modules based on n-type single crystalline Si solar cells10.1016/j.solmat.2015.04.037 ↗
25. Progression of rapid potential-induced degradation of n-type single-crystalline silicon photovoltaic modules10.7567/APEX.9.112301 ↗
26. Changes in current density-voltage and external quantum efficiency characteristics of n-type single-crystalline silicon photovoltaic modules with a rear-side emitter undergoing potential-induced degradation10.1016/j.solmat.2016.03.003 ↗
27. Potential-induced degradation of Cu(In,Ga)Se2 photovoltaic modules10.7567/JJAP.54.08KC13 ↗
28. Potential-induced degradation at interdigitated back contact solar cells10.1016/j.egypro.2014.08.015 ↗
29. Survey of potential-induced degradation in thin-film modules10.1117/1.JPE.5.053083 ↗
30. X-ray photoemission spectroscopy studies of Sn-doped indium-oxide films10.1063/1.324149 ↗
31. Interaction of hydrogenated amorphous silicon films with transparent conductive films10.1063/1.332436 ↗
32. Effect of hydrogen plasma treatment on transparent conducting oxides10.1063/1.97598 ↗
33. Degradation of tin-doped indium-oxide film in hydrogen and argon plasma10.1063/1.339699 ↗
34. Optical dispersion in electron-beam-evaporated indium tin oxide thin films10.1016/0040-6090(89)90834-1 ↗
35. Heat treatment in hydrogen gas and plasma for transparent conducting oxide films such as ZnO, SnO2 and indium tin oxide10.1016/0040-6090(89)90100-4 ↗
36. In situ investigation of the optoelectronic properties of transparent conducting oxide/amorphous silicon interfaces10.1063/1.101511 ↗
37. Sodium decoration of PID-s crystal defects after corona induced degradation of bare silicon solar cells10.1016/j.egypro.2015.07.055 ↗
38. Electrochemical corrosion of SnO2: F transparent conducting layers in thin-film photovoltaic modules10.1016/S0927-0248(02)00363-X ↗
39. A laboratory technique for the evaluation of electrochemical transparent conductive oxide delamination from glass substrates10.1016/S0040-6090(02)01020-9 ↗
40. Prevention of potential-induced degradation with thin ionomer film10.1109/JPHOTOV.2014.2365465 ↗