Concentrated sunlight for accelerated stability testing of organic photovoltaic materials: towards decoupling light intensity and temperature
Source abstract
Abstract
We have demonstrated OPV accelerated degradation studies using concentrated sunlight, where the atmosphere, temperature and illumination intensity were independently controlled. Testing various schemes for controlling the sample temperature under concentrated sunlight showed that heating of P3HT:PCBM was caused by photons at the absorbed wavelength range and dissipation of excess photon energy, and not necessarily by IR photon absorption. Sunlight chopping was found to be an effective method for independent temperature control under illumination by concentrated sunlight. The first accelerated degradation tests using sunlight concentration applied to P3HT:PCBM blends were reported. P3HT:PCBM blends exposed to concentrated sunlight in the presence of traces of oxygen/ humidity showed degradation induced by photo-oxidation of the P3HT backbone within the P3HT:PCBM blend, which is significantly thermally accelerated, in agreement with previous observations. However, this could be demonstrated in a time scale of minutes and hours, i.e., significantly accelerated. Exposure of well encapsulated P3HT:PCBM films to concentrated sunlight demonstrated stability up to 3,600 sun*hours, corresponding to about 1.6 years of operating time. This result was obtained at 300 suns exposure after merely 12 hours, demonstrating the advantage of using concentrated sunlight for accelerated stability tests. These tests can therefore combine extremely high acceleration factors with profound understanding of the effect of various, independently controlled factors on the degradation mechanisms.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Organic Electronics and Photovoltaics · Conducting polymers and applications · Thin-Film Transistor Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (57)
Show source-provided references
1. Longterm stability of efficient inverted P3HT:PCBM solar cells10.1016/j.solmat.2008.12.022 ↗
2. Flexible organic P3HT: PCBM bulk-heterojunction modules with more than 1 year outdoor lifetime10.1016/j.solmat.2008.01.004 ↗
3. Interlaboratory outdoor stability studies of flexible roll-to-roll coated organic photovoltaic modules: stability over 10,000h10.1016/j.solmat.2013.04.024 ↗
4. D. Angmo, P.M. Sommeling, R. Gupta, M. Hösel, S.A. Gevorgyan, J.M. Kroon, G.U. Kulkarni, F.C. Krebs, Outdoor operational stability of indium-free flexible polymer solar modules over 1 year studied in India, Holland, and Denmark. Adv. Eng. Mater. (2014) Early view, doi:10.1002/adem.201400002.10.1002/adem.201400002 ↗
5. Polymer solar cells with enhanced lifetime by improved electrode stability and sealing10.1016/j.solmat.2013.05.013 ↗
6. Intrinsic burn-in efficiency loss of small-molecule organic photovoltaic cells due to exciton-induced trap formation10.1016/j.solmat.2013.08.006 ↗
7. Photodegradation of small-molecule organic photovoltaics10.1016/j.solmat.2014.03.005 ↗
8. Water and oxygen induced degradation of small molecule organic solar cells10.1016/j.solmat.2011.01.001 ↗
9. Heliatek-Gmbh. 〈http://www.heliatek.com〉.
10. Determination of the degradation constant of bulk heterojunction solar cells by accelerated lifetime measurements10.1007/s00339-003-2499-4 ↗
11. Consensus stability testing protocols for organic photovoltaic materials and devices10.1016/j.solmat.2011.01.036 ↗
12. Accelerated weathering testing principles to estimate the service life of organic PV modules10.1016/j.solmat.2010.08.033 ↗
13. Accelerated lifetime measurements of P3HT: PCBM solar cells10.1016/j.synthmet.2005.06.016 ↗
14. Water ingress into and climate dependent lifetime of organic photovoltaic cells investigated by calcium corrosion tests10.1016/j.solmat.2013.10.023 ↗
15. Stability of polymer solar cells10.1002/adma.201104187 ↗
16. Concentrated light for accelerated photo degradation of polymer materials10.1002/aenm.201200663 ↗
17. Effects of concentrated sunlight on organic photovoltaics10.1063/1.3298742 ↗
18. Degradation of semiconducting polymers by concentrated sunlight10.1016/j.solmat.2010.09.022 ↗
19. Electrical and photo-induced degradation of ZnO layers in organic photovoltaics10.1002/aenm.201100227 ↗
20. Oxygen-induced quenching of photoexcited states in polythiophene films10.1016/j.orgel.2003.12.005 ↗
21. Formation of metastable charges as a first step in photoinduced degradation in pi-conjugated polymer: fullerene blends for photovoltaic applications10.1016/j.orgel.2011.06.020 ↗
22. Reversible and irreversible degradation of organic solar cell performance by oxygen10.1016/j.solener.2010.09.007 ↗
23. Degradation and stabilization of poly(3-hexylthiophene) thin films for photovoltaic applications10.1007/s00289-010-0323-9 ↗
24. Light-induced degradation of the P3HT-based solar cells active layer10.1016/j.solmat.2010.09.021 ↗
25. Stability and photodegradation mechanisms of conjugated polymer/fullerene plastic solar cells10.1016/S0927-0248(99)00094-X ↗
26. Stability/degradation of polymer solar cells10.1016/j.solmat.2008.01.005 ↗
27. Photoinduced degradation of polymer and polymer-fullerene active layers: experiment and theory10.1002/adfm.201001079 ↗
28. Degradation of organic solar cells due to air exposure10.1016/j.solmat.2006.06.041 ↗
29. Stability of the interface between indium-tin-oxide and poly(3,4-ethylenedioxythiophene)/poly(styrenesulfonate) in polymer light-emitting diodes10.1063/1.1315344 ↗
30. Photoelectron spectroscopy of thin films of PEDOT-PSS conjugated polymer blend: a mini-review and some new results10.1016/S0368-2048(01)00323-1 ↗
31. Influence of controlled acidity of hole-collecting buffer layers on the performance and lifetime of polymer:fullerene solar cells10.1021/jp2028615 ↗
32. Pathways for the degradation of organic photovoltaic P3HT: PCBM based devices10.1016/j.solmat.2008.01.020 ↗
33. Analysis of the failure mechanism for a stable organic photovoltaic during 10000h of testing10.1002/pip.794 ↗
34. Conjugated polymer surfaces and interfaces: a mini-review and some new results10.1016/S0379-6779(96)03692-2 ↗
35. The electronic structure of neutral and alkali metal-doped poly[3-(4-octylphenyl)thiophene] studied by photoelectron spectroscopy10.1016/0379-6779(96)80203-7 ↗
36. Long-term operational lifetime and degradation analysis of P3HT: PCBM photovoltaic cells10.1016/j.solmat.2010.09.007 ↗
37. Influence of thermal ageing on the stability of polymer bulk heterojunction solar cells10.1016/j.solmat.2006.10.008 ↗
38. Time-resolved morphological study of bulk heterojunction films for efficient organic solar devices10.1021/jp801674v ↗
39. Methods in determination of morphological degradation of polymer:fullerene solar cells10.1016/j.synthmet.2011.09.014 ↗
40. Tracing photoinduced electron transfer process in conjugated polymer/fullerene bulk heterojunctions in real time10.1016/S0009-2614(01)00431-6 ↗
41. Effects of long-term UV–visible light irradiation in the absence of oxygen on P3HT and P3HT:PCBM blend10.1016/j.solmat.2010.03.012 ↗
42. Toward ultrahigh-flux photovoltaic concentration10.1063/1.1723690 ↗
43. Photovoltaic characterization of concentrator solar cells by localized irradiation10.1063/1.2266161 ↗
44. A high-irradiance solar furnace for photovoltaic characterization and nanomaterial synthesis10.1016/j.solmat.2010.11.030 ↗
45. Temperature dynamics of multijunction concentrator solar cells up to ultra-high irradiance10.1002/pip.1179 ↗
46. Thin-film barrier on foil for organic LED lamps
47. ITO-free flexible organic solar cells with printed current collecting grids10.1016/j.solmat.2010.08.011 ↗
48. NREL, ASTM G173-03 Reference Solar Spectral Irradiance, 〈http://rredc.nrel.gov/solar/spectra/am1.5/ASTMG173/ASTMG173.html〉.
49. E.A. Katz, A. Manor, A. Mescheloff, T. Tromholt, F.C. Krebs, Accelerated stability testing of organic photovoltaics using concentrated sunlight, Thirty Eighth IEEE Photovoltaic Specialists Conference, IEEE, Austin, TX, USA, 2012, pp. 3249-3252.10.1109/PVSC.2012.6318270 ↗
50. Effect of interchaini nteractions on the absorption and emission of poly(3-hexylthiophene)10.1103/PhysRevB.67.064203 ↗
51. Structural and photo-physical properties of spin-coated poly(3-hexylthiophene) thin films10.1016/j.matchemphys.2009.03.028 ↗
52. Raman spectroscopic studies of regioregular poly(3-alkylthiophenes)10.1021/jp960104p ↗
53. Insights into the stability and thermal degradation of P3HT:C60 blended films for solar cell applications10.1007/s10853-011-5408-9 ↗
54. The mechanism of photo- and thermooxidation of poly(3-hexylthiophene) (P3HT) reconsidered10.1016/j.polymdegradstab.2009.03.005 ↗
55. Large-area organic photovoltaic module — fabrication and performance10.1016/j.solmat.2008.11.018 ↗
56. Faiman · Data processing for the negev radiation survey: Part II - typical meteorological year (TMY), Version 5, Israel Ministry of Energy and Water publication RD-20-12 · 2012
57. Morphology and photochemical stability of P3HT:PCBM active layers of organic solar cells10.1051/epjap/2011110132 ↗