journal article·2019-10Open access

Comparative analysis of mechanical strength of diamond-sawn silicon wafers depending on saw mark orientation, crystalline nature and thickness

Louise Carton, Roland Riva, Daniel Nelias, Marion Fourmeau, Fabrice Coustier, Amal Chabli

Abstract

Abstract Reducing the as-cut thickness of silicon wafers is one of the key issues to significantly lower the manufacturing costs of the photovoltaic industry. The pursuit of this objective is encouraged by the outstanding development of diamond wire sawing technology, which in addition to being twice more productive, also has great potential for further kerf reduction. However, in order to avoid higher breakage rates, it is crucial to understand how the sawing process affects the mechanical resistance of wafers as their thickness decreases. In this study, wafers of 180, 160 and 140 μm thickness were cut out of monocrystalline and multicrystalline silicon bricks. Their mechanical strength was evaluated by performing 4-line bending tests coupled with finite element simulations. The specimens were loaded in the parallel and perpendicular direction with respect to the saw marks. Because of the particular shape and orientation of the sawing-induced defects, all tested wafers are significantly weaker in parallel loading. While monocrystalline and multicrystalline wafers exhibit similar mechanical strength when bent perpendicular to the sawing marks, multicrystalline wafers are 30% less resistant in parallel loading. Finally, it is shown that the fracture stress of a wafer of a given silicon quality is independent of its thickness.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced Surface Polishing Techniques · Tunneling and Rock Mechanics · Diamond and Carbon-based Materials Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (56)

Show source-provided references
1. Solution-processed tBu 4 -ZnPc:C 61 bulk heterojunction organic photovoltaic cells10.7567/JJAP.55.032301 ↗
2. Perovskite solar cells: in pursuit of efficiency and stability10.1016/j.matdes.2017.09.037 ↗
3. 2019
4. Diamond wire sawing of solar silicon wafers: a sustainable manufacturing alternative to loose abrasive slurry sawing
5. Diamond wire sawing - state of the art and perspectives (2012).pdf
6. Effect of crystal defects on mechanical properties relevant to cutting of multicrystalline solar silicon10.1016/j.mssp.2013.05.016 ↗
7. Textural development of SiC and diamond wire sawed sc-silicon wafer10.1016/j.egypro.2012.07.072 ↗
8. Structured wire: from single wire experiments to multi-crystalline silicon wafer mass production10.1016/j.solmat.2014.06.008 ↗
9. Analysis of structured wire wafering processes to predict optimized process settings by varying particle size and wire diameter10.1063/1.5049340 ↗
10. Improved mechanical strength and reflectance of diamond wire sawn multi-crystalline silicon wafers by inductively coupled plasma (ICP) etching10.1016/j.solmat.2018.05.057 ↗
11. Texturization using metal catalyst wet chemical etching for multicrystalline diamond wire sawn wafer10.1016/j.solmat.2014.11.008 ↗
12. Wear of diamond in scribing of multi-crystalline silicon10.1063/1.5037106 ↗
13. 2018
14. Diamond wire-sawn silicon wafers-from the lab to the cell production
15. Mechanisms of material removal and subsurface damage in fixed-abrasive diamond wire slicing of single-crystalline silicon10.1016/j.precisioneng.2017.04.011 ↗
16. Comparative analysis of fracture strength of slurry and diamond wire sawn multicrystalline silicon solar wafers10.1002/adem.201200262 ↗
17. Characterization of the surfaces generated by diamond cutting of crystalline silicon
18. Effect of wear of diamond wire on surface morphology, roughness and subsurface damage of silicon wafers10.1016/j.wear.2016.07.009 ↗
19. Ductile mode behavior of silicon during scribing by spherical abrasive particles10.1016/j.procir.2016.02.341 ↗
20. Studies of the ductile mode of cutting brittle materials (A review)10.3103/S1063457613050018 ↗
21. Effect of crystallographic orientation on ductile scribing of crystalline silicon: role of phase transformation and slip10.1016/j.msea.2012.04.034 ↗
22. Effect of grit shape and crystal structure on damage in diamond wire scribing of silicon10.1111/jace.14732 ↗
23. Suppressing scratch-induced brittle fracture in silicon by geometric design modification of the abrasive grits
24. Analyses of diamond wire sawn wafers: effect of various cutting parameters
25. Determination of the impact of the wire velocity on the surface damage of diamond wire sawn silicon wafers10.1016/j.egypro.2015.07.124 ↗
26. Subsurface crack damage in silicon wafers induced by resin bonded diamond wire sawing10.1016/j.mssp.2016.10.021 ↗
27. The chemo-mechanical effect of cutting fluid on material removal in diamond scribing of silicon10.1063/1.4991536 ↗
28. Mechanical behavior of diamond-sawn multi-crystalline silicon wafers and its improvement10.1007/s12633-013-9170-2 ↗
29. On the residual stress and fracture strength of crystalline silicon wafers
30. The impact of damage etching on fracture strength of diamond wire sawn monocrystalline silicon wafers for photovoltaics use10.7567/JJAP.57.126501 ↗
31. Effect of growth rate and wafering on residual stress of diamond wire sawn silicon wafers10.1016/j.promfg.2016.08.108 ↗
32. Spatial distribution of full-field residual stress and its correlation with fracture strength of thin silicon wafers
33. Effect of microstructure and processing parameters on mechanical strength of multicrystalline silicon solar cells
34. Relationship between macro- scale and micro- scale mechanical properties of photovoltaic silicon wafers
35. Improved fracture strength of multicrystalline silicon by germanium doping10.1016/j.jcrysgro.2010.11.081 ↗
36. Modeling and testing the mechanical strength of solar cells10.1016/j.solmat.2013.06.048 ↗
37. Fatigue crack growth in Silicon solar cells and hysteretic behaviour of busbars10.1016/j.solmat.2018.02.016 ↗
38. Electronic effects in the elastic constants of n-type silicon10.1103/PhysRev.161.756 ↗
39. Biaxial fracture test of silicon wafers10.1002/adem.200400406 ↗
40. Stiffness and fracture analysis of photovoltaic grade silicon plates10.1016/j.ijsolstr.2016.07.013 ↗
41. Fracture analysis and distribution of surface cracks in multicrystalline silicon wafers10.1115/1.4025972 ↗
42. Comparison of test methods for strength characterization of thin solar wafer
43. Mechanical strength of silicon solar wafers characterized by ring-on-ring test in combination with digital image correlation
44. Damage evaluation of wet-chemical Si-wafer thinning/backside via exposure process10.1109/TCPMT.2014.2304462 ↗
45. ASTM International · 2018 · vol. 1161
46. Effect of sawing induced micro-crack orientations on fracture properties of silicon wafers10.1016/j.engfracmech.2016.01.014 ↗
47. 2017
48. A statistical distribution function of wide applicability
49. Diamond wire wafering: wafer morphology in comparison to slurry sawn wafers
50. The impact of saw mark direction on the fracture strength of thin (120 μm) monocrystalline silicon wafers for photovoltaic cells
51. Analysis of the sub-surface damage of mc- and cz-Si wafers sawn with diamond-plated wire10.1016/j.egypro.2013.07.363 ↗
52. Directional anisotropy in the cleavage fracture of silicon10.1103/PhysRevLett.84.5347 ↗
53. Velocity dependent crack deflection in single crystal silicon10.1016/S1359-6462(03)00354-3 ↗
54. Crack initiation behavior in single crystalline silicon10.1016/j.scriptamat.2016.11.015 ↗
55. Crack plane deflection and shear wave effects in the dynamic fracture of silicon single crystal10.1016/j.jmps.2018.09.031 ↗
56. On the fracture of multi-crystalline silicon wafer10.1088/0022-3727/49/47/475601 ↗