Abstract

Abstract Exposure to accelerated humidity lifetime conditions has been proved to have detrimental effects on organic photovoltaics (OPV) performance, because of the deterioration of the electrodes of the device rather than the active layer. Normal and inverted OPV devices are investigated in order to identify their main degradation mechanisms under accelerated humidity lifetime conditions. Reverse engineering can be a useful technique to probe main degradation mechanisms of the top electrode of both normal and inverted organic photovoltaic (OPVs). By using reverse engineering methods, we show that the major degradation mechanism of inverted OPVs under accelerated humidity lifetime conditions, is due to PEDOT:PSS hole selective top contact.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Organic Electronics and Photovoltaics · Thin-Film Transistor Technologies · Conducting polymers and applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (41)

Show source-provided references
1. Degradation of organic solar cells due to air exposure10.1016/j.solmat.2006.06.041 ↗
2. Effect of temperature on the morphological and photovoltaic stability of bulk heterojunction polymer:fullerene solar cells10.1016/j.solmat.2008.01.006 ↗
3. Environmental aging of poly(p-phenylenevinylene) based light-emitting diodes10.1016/S0379-6779(00)00254-X ↗
4. Photooxidation of electroluminescent polymers studied by corelevel photoabsorption spectroscopy10.1063/1.116298 ↗
5. Degradation mechanisms in organic photovoltaic devices10.1016/j.orgel.2011.11.027 ↗
6. M. Lira-Cantu, D.M. Tanenbaum, K. Norrman, E. Voroshazi, M. Hermenau, M.T. Lloyd, G. Teran-Escobar, Y. Galagan, B. Zimmermann; M. Hösel, H.F. Dam; M. Jørgensen, S. Gevorgyan,L. Lutsen, D. Vanderzande, H. Hoppe, R. Rösch, U. Würfel, R. Andriessen, A. Rivaton, G.Y. Uzunoğlu, D. Germack, B. Andreasen, M.V. Madsen, E. Bundgaard, F.C. Krebs, Combined characterization techniques to understand the stability of a variety of organic photovoltaic devices: the ISOS-3 inter-laboratory collaboration, in: Proceedings SPIE 8472, Reliability of Photovoltaic Cells, Modules, Components, and Systems 847203, October 2012, 10.1117/12.929579.10.1117/12.929579 ↗
7. Observation of degradation processes of Al electrodes in organic electroluminescence devices by electroluminescence microscopy, atomic force microscopy, scanning electron microscopy, and Auger electron spectroscopy10.1063/1.357224 ↗
8. The influence of materials work function on the open circuit voltage of plastic solar cells10.1016/S0040-6090(01)01586-3 ↗
9. Water vapor and oxygen degradation mechanisms in organic light emitting diodes10.1002/1616-3028(200104)11:2<116::AID-ADFM116>3.0.CO;2-B ↗
10. M.O. Reese, A.J. Morfa, M.S. White, N. Kopidakis, S.E. Shaheen, G. Rumbles, D.S. Ginley, Short-term metal/organic interface stability investigations of organic photovoltaic devices, in: Proceedings of the 33rd IEEE Photovoltaic Specialists Conference, San Diego, California, 2008.10.1109/PVSC.2008.4922720 ↗
11. Degradation mechanism of organic solar cells with aluminum cathode10.1016/j.solmat.2011.07.020 ↗
12. Influence of cathode oxidation via the hole extraction layer in polymer:fullerene solar cells10.1016/j.orgel.2011.01.025 ↗
13. Thermal degradation mechanisms of PEDOT:PSS10.1016/j.orgel.2008.10.008 ↗
14. Conductivity degradation study of PEDOT: PSS films under heat treatment in helium and atmospheric air10.4236/ojopm.2012.21002 ↗
15. Impact of contact evolution on the shelf life of organic solar cells10.1039/b910213b ↗
16. Characterization of polymer solar cells by TOF-SIMS depth profiling10.1016/S0169-4332(02)00756-0 ↗
17. Stability of the interface between indium-tin-oxide and poly(3,4-ethylenedioxythiophene)/poly(styrenesulfonate) in polymer light-emitting diodes10.1063/1.1315344 ↗
18. Stable organic photovoltaics using Ag thin film anodes10.1039/c2jm15670a ↗
19. Stability/degradation of polymer solar cells10.1016/j.solmat.2008.01.005 ↗
20. The ISOS-3 inter-laboratory collaboration focused on the stability of a variety of organic photovoltaic devices10.1039/C1RA00686J ↗
21. Consensus stability testing protocols for organic photovoltaic materials and devices10.1016/j.solmat.2011.01.036 ↗
22. Stability of Polymer Solar Cells10.1002/adma.201104187 ↗
23. TOF-SIMS investigation of degradation pathways occurring in a variety of organic photovoltaic devices – the ISOS-3 inter-laboratory collaboration10.1039/c2cp41787a ↗
24. On the stability of a variety of organic photovoltaic devices by IPCE and in situ IPCE analyses – the ISOS-3 inter-laboratory collaboration10.1039/c2cp40821j ↗
25. Investigation of the degradation mechanisms of a variety of organic photovoltaic devices by combination of imaging techniques—the ISOS-3 inter-laboratory collaboration10.1039/c2ee03508a ↗
26. Performance analysis of printed bulk heterojunction solar cells
27. Cesium-doped zinc oxide as electron selective contact in inverted organic photovoltaics10.1063/1.4811088 ↗
28. Synergistic effects of buffer layer processing additives for enhanced hole carrier selectivity in inverted organic photovoltaics10.1016/j.orgel.2013.07.024 ↗
29. A compact multi-chamber setup for degradation and lifetime studies of organic solar cells10.1016/j.solmat.2011.01.023 ↗
30. A roll-to-roll process to flexible polymer solar cells: model studies, manufacture and operational stability studies10.1039/b823001c ↗
31. Electron barrier formation at the organic-back contact interface is the first step in thermal degradation of polymer solar cells10.1002/adfm.201304166 ↗
32. Air-stable polymer electronic devices10.1002/adma.200602653 ↗
33. ITO-free flexible polymer solar cells: from small model devices to roll-to-roll processed large modules10.1016/j.orgel.2011.01.009 ↗
34. Life cycle assessment of ITO-free flexible polymer solar cells prepared by roll-to-roll coating and printing10.1016/j.solmat.2011.09.048 ↗
35. A conclusive view on charge generation, recombination, and extraction in as-prepared and annealed P3HT:PCBM Blends: combined experimental and simulation work
36. S.R. Dupont, E. Voroshazi, P. Heremans, R.H. Dauskardt, The effect of anneal, solar irradiation and humidity on the adhesion/cohesion properties of P3HT:PCBM based inverted polymer solar cells, in: Proceedings of the 38th IEEE Photovoltaic Specialists Conference, Austin, TX, USA, 2012, Art. No 6318272, pp. 3259–3262.10.1109/PVSC.2012.6318272 ↗
37. Influence of the hole-transport layer on the initial behavior and lifetime of inverted organic photovoltaics10.1016/j.solmat.2010.12.036 ↗
38. Simulation of light intensity dependent current characteristics of polymer solar cells10.1063/1.1646435 ↗
39. Molecular semiconductors in organic photovoltaic cells10.1021/cr9002984 ↗
40. Highly efficient inverted organic photovoltaics using solution based titanium oxide as electron selective contact10.1063/1.2402890 ↗
41. Degradation patterns in water and oxygen of an inverted polymer solar cell10.1021/ja106299g ↗