journal article·2013-09Open access

Epitaxial undoped indium oxide thin films: Structural and physical properties

W. Seiler, M. Nistor, C. Hebert, J. Perrière

Abstract

Indium oxide thin films were grown by the pulsed electron beam deposition method on c-cut sapphire substrates at 10−2 mbar oxygen pressure and temperature up to 500 1C. Such conditions lead to the formation of dense, smooth and stoichiometric In2O3 films, with the cubic bixbyite structure. Epitaxial thin films were obtained at substrate temperatures as low as 200 1C. Pole figure measurements indicate the existence of (111) oriented In2O3 crystallites with different in-plane symmetry, i.e. three-fold and six-fold symmetry. The origin of this effect may be related to the specificities of the growth method which can induce a large disorder in the oxygen network of In2O3, leading then to a six-fold symmetry in the (111) plane of the bixbyite structure. This temperature resistivity behaviour shows metallic conductivity at room temperature and a metal- semiconductor transition at low temperature for In2O3 films grown at 200 1C, while the classical semiconductor behaviour was observed for the films grown at 400 and 500 1C. A maximum mobility of 24.7 cm2/V s was measured at 200 1C, and then it falls off with improving the crystalline quality of films. The optical transparency is high (480%) in a spectral range from 500 nm to 900 nm.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: ZnO doping and properties · Gas Sensing Nanomaterials and Sensors · Ga2O3 and related materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (43)

Show source-provided references
1. 2010
2. 2011
3. Surface origin of high conductivities in undoped In2O3 films10.1103/PhysRevLett.108.016802 ↗
4. Highly electrically conductive indium-tin-oxide thin films epitaxially grown on yttria-stabilized zirconia (100) by pulsed-laser deposition10.1063/1.126461 ↗
5. Domain matching epitaxial growth of In2O3 thin films on α-Al2O3 (0001)10.1021/cg201474h ↗
6. Domain structure and optical property of epitaxial indium oxide film deposited on MgO (100) substrate10.1016/j.susc.2011.02.017 ↗
7. Growth mechanisms and electrical properties of epitaxial In2O3 films on sapphire
8. Structural and photoluminescence properties of single-crystalline In2O3 films grown by metal organic vapor deposition10.1016/j.jcrysgro.2008.06.075 ↗
9. Growth of In2O3 single-crystalline film on sapphire (0001) substrate by molecular beam epitaxy10.1016/j.jcrysgro.2005.12.086 ↗
10. Surface structure and electronic properties of In2O3 (111) single-crystal thin films grown on Y-stabilized ZrO2 (111)10.1021/cm901127r ↗
11. Growth of epitaxial zirconium-doped indium oxide (222) at low temperature by rf sputtering10.1039/c004452k ↗
12. On the physical properties of In2O3 films grown on (0001) sapphire substrates by atomic layer deposition
13. Pulsed laser deposition of oriented In2O3 on (001) InAs, MgO and yttria-stabilized zirconia10.1063/1.109408 ↗
14. Real-time evolution of electrical properties and structure of indium oxide and indium tin oxide during crystalization10.1016/j.scriptamat.2008.09.020 ↗
15. Sputtered In2O3 and ITO thin films containing zirconium10.1063/1.3116542 ↗
16. Twinned domains in epitaxial ZnO/SnO2 –cosubstituted In2O3 thin films10.1016/j.jcrysgro.2007.08.006 ↗
17. Nanocomposite indium tin oxide thin films: formation induced by a large oxygen deficiency and properties10.1088/0953-8984/22/4/045006 ↗
18. Pure and Nb-doped TiO1.5 films grown by pulsed-laser deposition for transparent p–n homojunction10.1016/j.apsusc.2010.10.149 ↗
19. Oxygen content of YBaCuO thin films10.1016/0921-4534(95)00666-4 ↗
20. Thin films of oxygen deficient perovskite phases10.1103/PhysRevB.75.165317 ↗
21. Nanocomposite oxide thin films grown by pulsed energy beam deposition10.1016/j.apsusc.2010.11.139 ↗
22. Phase separation in nanocomposite indium tin oxide thin films grown at room temperature10.1039/c2jm16753k ↗
23. Dopability, intrinsic conductivity and nonstoichiometry of transparent conducting oxides10.1103/PhysRevLett.98.045501 ↗
24. Surface energies control the self-organization of oriented In2O3 nanostructures on cubic zirconia10.1021/nl102403t ↗
25. Defects and interfaces in epitaxial ZnO/α-Al2O3 and AlN/ZnO/α-Al2O3 heterostructures10.1063/1.368440 ↗
26. RHEED analysis of interface growth modes of TiN on Si (001) produced by crossed beam laser ablation10.1016/S0169-4332(97)00618-1 ↗
27. Substrate surface step effects on microstructure of epitaxial films10.1063/1.107978 ↗
28. Crystal defects and related stress in Y2O3 thin films: origin, modeling and consequence on the stability of the C-type structure10.1103/PhysRevB.84.014104 ↗
29. Nature of the band gap of In2O3 revealed by first principles calculations and X-ray spectroscopy10.1103/PhysRevLett.100.167402 ↗
30. Growth of In2O3 (100) on Y-stabilized ZrO2 (100) by O-plasma assisted molecular beam epitaxy10.1063/1.2889500 ↗
31. Indium-oxide polymorphs from first principles: quasiparticles electronic states10.1103/PhysRevB.77.155107 ↗
32. High electron mobility of indium oxide grown on yttria-stabilized zirconia10.1063/1.2203722 ↗
33. Carrier transport in polycrystalline ITO and ZnO:Al II: The influence of grain barriers and boundaries
34. The electronic properties of amorphous and crystalllized In2O3 films10.1063/1.2358829 ↗
35. Mott · 1993
36. Ferromagnetism and spin-polarized charge carriers in In2O3 thin films10.1103/PhysRevB.79.165208 ↗
37. Electrical transport properties in indium tin oxide films prepared by electron-beam evaporation10.1063/1.2988901 ↗
38. Metal–semiconductor transition in epitaxial ZnO films10.1063/1.3259412 ↗
39. Metallic conductivity and metal-semiconductor transition in Ga-doped ZnO10.1063/1.2165281 ↗
40. Disordered electronic systems10.1103/RevModPhys.57.287 ↗
41. Weak localization effects in some metallic perovskites10.1140/epjb/e2004-00207-9 ↗
42. Oxygen-induced metal–insulator-transition on single crystalline metal oxide wires10.1063/1.3675204 ↗
43. Origin of definite Hall voltage and positive slope in mobility-donor density relation in disordered oxide semiconductors10.1063/1.3364131 ↗