Mode‐I intralaminar fracture toughness of silica particles‐filled glass woven fabric‐reinforced vinyl ester composites

M. S. Sham Prasad, C. S. Venkatesha, T. Jayaraju, D. Janardhan

Polymer Composites· Volume 33· Issue 5

Abstract

Abstract Glass woven fabric reinforced vinyl ester (GV) composites filled with different weight proportions of silica particles were fabricated by hand lay up technique followed by oven curing. The plane strain Mode‐I Intralaminar fracture toughness, K IC of the silica filled GV composites has been studied and the experimental results were compared with those of unfilled GV composites. The findings of the experiments showed that the fracture toughness has improved by the addition of silica particles up to 6 weight % with marginal increase of tensile properties. The silica filled and unfilled GV composites showed brittle fracture, with maximum toughness for 6 weight % silica particles. The morphology of fracture surfaces was examined by using SEM. Pulled and fractured fibers are observed on the fracture surface of GV composites evidencing fiber bridging but not in the silica filled GV composites. POLYM. COMPOS., 2012. © 2012 Society of Plastics Engineers
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Mechanical Behavior of Composites · Structural Analysis of Composite Materials · Advanced Fiber Optic Sensors

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (24)

Show source-provided references
1. W.D. Bascom D.L. Hunston 1980 Applied Science Publisher London
2. 10.1016/S0300-9440(02)00085-110.1016/S0300-9440(02)00085-1 ↗
3. 10.1007/BF0054382710.1007/BF00543827 ↗
4. 10.1016/0266-3538(88)90009-710.1016/0266-3538(88)90009-7 ↗
5. 10.1016/0263-8223(88)90006-210.1016/0263-8223(88)90006-2 ↗
6. 10.1007/BF0057537910.1007/BF00575379 ↗
7. 10.1016/S1359-835X(98)00156-010.1016/S1359-835X(98)00156-0 ↗
8. 10.1016/S0266-3538(99)00166-910.1016/S0266-3538(99)00166-9 ↗
9. E.Greene Use of fiber reinforced plastics in marine industry Ship Structure Committee Washington SSC 360 (1990).
10. 10.1016/0266-3538(92)90003-L10.1016/0266-3538(92)90003-L ↗
11. 10.1016/0266-3538(90)90041-310.1016/0266-3538(90)90041-3 ↗
12. Leonard L.W.H. · Proc. I Mech E J. Mater. Des. Appl. · 2009 · 223 · 83
13. 10.1177/00219983920260110110.1177/002199839202601101 ↗
14. 10.1177/00219983990330010510.1177/002199839903300105 ↗
15. 10.1016/j.compositesa.2005.01.00610.1016/j.compositesa.2005.01.006 ↗
16. J.G. Funk J.W. Deaton 1989 The interlaminar fracture toughness of woven graphite/epoxy composites NASA Tech Paper 2950 NASA Langley Research Center Hampton VA
17. 10.1007/BF0094216110.1007/BF00942161 ↗
18. 10.1016/S0266-3538(01)00011-210.1016/S0266-3538(01)00011-2 ↗
19. 10.1016/j.compscitech.2005.12.02310.1016/j.compscitech.2005.12.023 ↗
20. 10.1016/j.compscitech.2009.03.00710.1016/j.compscitech.2009.03.007 ↗
21. 10.1016/0013-7944(86)90118-910.1016/0013-7944(86)90118-9 ↗
22. 10.1016/0167-577X(95)00224-310.1016/0167-577X(95)00224-3 ↗
23. 10.1016/j.compositesa.2006.03.00110.1016/j.compositesa.2006.03.001 ↗
24. ASTM D5045–99 · 1999