Abstract

The static and dynamic mechanical properties and fire behaviors for long‐glass‐fiber reinforced polyamide 6 composite filled with organo‐modified montmorillonite/brominated epoxy resins/antimony trioxide (OMMT/FR/LGFPA6) have been investigated by comparison with the formulation without OMMT (FR/LGFPA6), being dealt with accelerated aging condition. Relative to the unaged composites, both aged composites presented the improved static mechanical properties after 10‐day aging, the increased degree of cross‐linking in the amorphous region, and the increased LOI value as well as maintained the optimal UL‐94 rating. However, after a long‐time aging exposure, the aged FR/LGFPA6 composite was more flammable and its mechanical properties were more severely impacted by aging. Remarkably, substitution of a certain content of halogen‐antimony flame retardants with OMMT not only slowed down the rate of degradation but also weakened the flammability for FR/LGFPA6 composite over the whole period of aging. POLYM. COMPOS., 40:2208–2218, 2019. © 2018 Society of Plastics Engineers
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Flame retardant materials and properties · Polymer Nanocomposites and Properties · Fiber-reinforced polymer composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

College of Materials Science and Engineering Guizhou Minzu University Guiyang China

Institut de Science des Materiaux de Mulhouse IS2M UMR CNRS 7361 Mulhouse France

Laboratoire de Chimie Organique et Bioorganique Mulhouse France

National Engineering Research Center for Compounding and Modification of Polymeric Materials, and College of Materials Science and Metallurgy Guizhou University Guiyang China

Funding

China Scholarship Council

References (43)

Show source-provided references
1. 10.1002/pen.76031180610.1002/pen.760311806 ↗
2. 10.1016/1359-835X(95)00038-410.1016/1359-835X(95)00038-4 ↗
3. 10.1002/app.1362710.1002/app.13627 ↗
4. 10.1016/j.polymer.2007.12.03710.1016/j.polymer.2007.12.037 ↗
5. 10.1016/j.polymdegradstab.2013.10.01410.1016/j.polymdegradstab.2013.10.014 ↗
6. 10.1016/j.polymdegradstab.2006.07.02610.1016/j.polymdegradstab.2006.07.026 ↗
7. 10.1016/j.polymdegradstab.2008.03.01010.1016/j.polymdegradstab.2008.03.010 ↗
8. 10.1016/j.polymdegradstab.2009.08.01010.1016/j.polymdegradstab.2009.08.010 ↗
9. Zuo X.L. · J. Appl. Polym. Sci. · 2014 · 131 · 1
10. Kartalis C.N. · J. Appl. Polym. Sci. · 2002 · 86 · 247
11. 10.1002/app.1226110.1002/app.12261 ↗
12. 10.1002/app.2579510.1002/app.25795 ↗
13. 10.1016/j.compositesa.2015.11.02810.1016/j.compositesa.2015.11.028 ↗
14. 10.1016/S0266-3538(02)00080-510.1016/S0266-3538(02)00080-5 ↗
15. 10.1002/app.2099610.1002/app.20996 ↗
16. 10.1023/A:100662473025710.1023/A:1006624730257 ↗
17. 10.1016/j.polymdegradstab.2016.01.02310.1016/j.polymdegradstab.2016.01.023 ↗
18. 10.1002/pc.1066110.1002/pc.10661 ↗
19. 10.1002/pi.484110.1002/pi.4841 ↗
20. 10.1002/pol.1983.17021031210.1002/pol.1983.170210312 ↗
21. Clough R. L.Aging effects on fire‐retardant additives in organic materials for nuclear plant applications. NUREG/CR‐2868 SAND82–0485 RV 1982.
22. 10.1177/073490410403960910.1177/0734904104039609 ↗
23. 10.1016/j.polymdegradstab.2010.08.02010.1016/j.polymdegradstab.2010.08.020 ↗
24. 10.1016/j.polymdegradstab.2014.05.01910.1016/j.polymdegradstab.2014.05.019 ↗
25. 10.1016/j.polymdegradstab.2015.10.01910.1016/j.polymdegradstab.2015.10.019 ↗
26. 10.1002/apmc.1990.05176012410.1002/apmc.1990.051760124 ↗
27. 10.1002/fam.94410.1002/fam.944 ↗
28. 10.1002/pat.76210.1002/pat.762 ↗
29. 10.1016/j.polymdegradstab.2010.02.03010.1016/j.polymdegradstab.2010.02.030 ↗
30. 10.1016/0014-3057(94)90160-010.1016/0014-3057(94)90160-0 ↗
31. 10.1080/1060132930802125310.1080/10601329308021253 ↗
32. 10.1002/pat.68410.1002/pat.684 ↗
33. 10.1016/j.polymdegradstab.2008.02.02110.1016/j.polymdegradstab.2008.02.021 ↗
34. 10.1002/marc.20060035610.1002/marc.200600356 ↗
35. 10.1021/ma702094e10.1021/ma702094e ↗
36. 10.1002/app.2864710.1002/app.28647 ↗
37. 10.1016/j.polymdegradstab.2006.11.00610.1016/j.polymdegradstab.2006.11.006 ↗
38. 10.1007/s10973-016-5601-910.1007/s10973-016-5601-9 ↗
39. 10.1016/S0141-3910(00)00024-010.1016/S0141-3910(00)00024-0 ↗
40. 10.1016/j.compositesa.2007.08.00910.1016/j.compositesa.2007.08.009 ↗
41. 10.1016/S0266-3538(96)00090-510.1016/S0266-3538(96)00090-5 ↗
42. Babrauskas V. · 2002 · 3
43. 10.1016/j.polymdegradstab.2005.02.02210.1016/j.polymdegradstab.2005.02.022 ↗