Abstract Thermooxidative degradation at and beyond processing temperatures has been carried out on polyoxymethylene (POM) enhanced with four different types of POSS, being Glycidyl, GlycidylIsobutyl, Aminopropylisobutyl, and Poly(ethylene glycol). The quantification of such degradation was carried out through FTIR spectrography, color spectrophotometry, and thermogravimetric analysis methods. The results showed that the presence of POSS in the blend improves dramatically the thermal stability of the POM matrix. The best performance was found with Aminopropylisobutyl, whereby the onset of degradation temperature increased by more than 50°C. Said improvement is referred to the conditions where the nanocomposite developed only 2% of carbonyl yield and 8% of yellowing of the 100% deterioration suffered by the standard POM copolymer. POLYM. COMPOS., 2011. © 2011 Society of Plastics Engineers
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Silicone and Siloxane Chemistry · biodegradable polymer synthesis and properties · Polymer Nanocomposites and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (23)

Show source-provided references
1. 10.1021/ma051357w10.1021/ma051357w ↗
2. 10.1021/ma070673310.1021/ma0706733 ↗
3. Manikantan B.N. · Polym. Prepr. · 2005 · 46 · 367
4. 10.1016/S0032-3861(03)00018-110.1016/S0032-3861(03)00018-1 ↗
5. 10.1002/mame.20100006410.1002/mame.201000064 ↗
6. 10.1002/app.2664810.1002/app.26648 ↗
7. 10.1002/app.2912610.1002/app.29126 ↗
8. 10.1002/app.3120910.1002/app.31209 ↗
9. Yang N.L. · Abstr. Papers Am. Chem. Soc. · 1984 · 188 · 149
10. Ranby B. · 1996 · 236
11. 10.1002/app.2652410.1002/app.26524 ↗
12. 10.1002/app.2291310.1002/app.22913 ↗
13. 10.1016/j.polymdegradstab.2005.01.02910.1016/j.polymdegradstab.2005.01.029 ↗
14. 10.1016/j.eurpolymj.2008.12.00910.1016/j.eurpolymj.2008.12.009 ↗
15. 10.1080/0360255090282433310.1080/03602550902824333 ↗
16. 10.1007/s10853-008-3227-410.1007/s10853-008-3227-4 ↗
17. 10.1080/0360255090272547210.1080/03602550902725472 ↗
18. 10.1166/jnn.2010.184510.1166/jnn.2010.1845 ↗
19. 10.1016/S0032-3861(99)00131-710.1016/S0032-3861(99)00131-7 ↗
20. 10.1016/S0141-3910(00)00111-710.1016/S0141-3910(00)00111-7 ↗
21. 10.1016/j.polymdegradstab.2004.03.00810.1016/j.polymdegradstab.2004.03.008 ↗
22. 10.1007/s00397-002-0282-710.1007/s00397-002-0282-7 ↗
23. M.Gröning Unpublished undergraduate dissertation UniversityKTH Fibre and Polymer Technology Stockolm 19 (2004).