Microwave anisotropy and dichroism of ferroelectric crystals CH3NH3HgCl3
Source abstract
Abstract
Microwave dielectric anisotropy of oriented crystals of CH3NH3HgCl3 is measured by a resonant cavity method at 9.5 GHz. A general expression for the perturbation cavity is given, taking into account anisotropies of the electrical properties and of the depolarisation factor of the sample. Measurements of the frequency shift and transmitted power are made versus crystal orientation relative to the microwave field. Using the general formulas established in this work, the complex permittivity tensor is calculated (at 9.5 GHz and 300 K): εc = 22.0 – j 2.60, εa = 22.0 – j 0.40 (a ⊥ c).
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Solid-state spectroscopy and crystallography · Organic and Molecular Conductors Research · Advanced NMR Techniques and Applications
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.