CAFM on conjugated polymer nanofibers: Capable of assessing one fiber mobility

Jean-Christophe Bolsée, Wibren D. Oosterbaan, Laurence Lutsen, Dirk Vanderzande, Jean Manca

Organic Electronics· Volume 12· Issue 12
Publisher page

Abstract

Abstract Poly(3-alkylthiophene) (P3AT) nanofibers (NFs) are interesting as building blocks for future organic electronic devices but also as a model system to examine transport mechanisms in semiconducting polymers. However, due to the technical problem of making good contacts at the nanometer scale, electrical characterizations on one isolated P3AT NF are rare. Here, using Conductive Atomic Force Microscopy (CAFM), charge transport investigations along the length ( π – π stacking direction) and the height (alkyl chain direction) of one single NF are reported. Firstly, by developing a transistor structure with one electrode being the CAFM tip, we measured the longitudinal mobility: μ L = 0.07 ± 0.03 cm 2 V −1 s −1 . Secondly, charge transport along the NF height was done in a sandwich structure and led to a transversal mobility of μ T ∼ 10 −5 –10 −6 cm 2 V −1 s −1 where μ T was found to decrease with increasing alkyl side chain length. With CAFM charge transport anisotropy in P3AT NF is thus evidenced at the nanometer scale, since we find at least four orders of magnitude difference between μ L and μ T .
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Organic Electronics and Photovoltaics · Conducting polymers and applications · Carbon Nanotubes in Composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (26)

Show source-provided references
1. O’Brien · Adv. Mater. · 2006 · 18 · 237910.1002/adma.200601012 ↗
2. Samitsu · Macromolecules · 2010 · 43 · 789110.1021/ma101655s ↗
3. Berson · Adv. Funct. Mater. · 2007 · 17 · 137710.1002/adfm.200600922 ↗
4. Bertho · Org. Electron. · 2009 · 10 · 124810.1016/j.orgel.2009.06.018 ↗
5. Ihn · Polym. Sci. Part B: Polym. Phys. · 1993 · 31 · 73510.1002/polb.1993.090310614 ↗
6. Merlo · J. Polym. Sci. Part B: Polym. Phys. · 2003 · 41 · 267410.1002/polb.10656 ↗
7. Samitsu · Macromolecules · 2008 · 41 · 800010.1021/ma801128v ↗
8. Oosterbaan · J. Mater. Chem. · 2009 · 19 · 542410.1039/b900670b ↗
9. Merlo · J. Phys. Chem. B · 2004 · 108 · 1916910.1021/jp047023a ↗
10. Shimomura · Phys. Rev. B · 2011 · 83 · 11531410.1103/PhysRevB.83.115314 ↗
11. Oosterbaan · Adv. Funct. Mater. · 2010 · 20 · 79210.1002/adfm.200901471 ↗
12. Miyauchi · J. Appl. Polym. Sci. · 2002 · 85 · 142910.1002/app.10676 ↗
13. According to the Hertz model, the contact radius, r, is given r3=3FR/4E with 1/E=(1-v12)/E1+(1-v22)/E2 where F is the load, R is the tip radius and E is the Young’s modulus. With E1=195GPa,v1=0.38 for PtIr5 and E2=1GPa, v2=0.35 for polymer, r is found to be around 2nm.
14. Bolsée · Synth. Met. · 2011 · 161 · 78910.1016/j.synthmet.2011.01.031 ↗
15. Karl · 2001
16. Northrup · Phys. Rev. B · 2007 · 76 · 24520210.1103/PhysRevB.76.245202 ↗
17. Sirringhaus · Nature · 1999 · 401 · 68510.1038/44359 ↗
18. Chang · Chem. Mater. · 2004 · 16 · 477210.1021/cm049617w ↗
19. Xie · Phys. Rev. B · 2011 · 83 · 18411710.1103/PhysRevB.83.184117 ↗
20. Blom · Appl. Phys. Lett. · 1996 · 68 · 2310.1063/1.116583 ↗
21. Lampert · 1970
22. Mott · 1948
23. Reid · Nano Lett. · 2008 · 8 · 160210.1021/nl080155l ↗
24. Lin · Appl. Phys. Lett. · 2002 · 81 · 257210.1063/1.1509464 ↗
25. Frammelsberger · Appl. Surf. Sci. · 2007 · 253 · 361510.1016/j.apsusc.2006.07.070 ↗
26. For longitudinal configuration: E∼106 V.m-1. For transversal configuration: E∼108 V.m-1.