Abstract In this paper, we demonstrate a novel method for fabricating metal nanopatterns using cracking to address the limitations of traditional techniques. Parallel crack arrays were created in a polydimethylsiloxane (PDMS) mold using a combination of surface modification and control of strain fields. The elastic PDMS containing the crack arrays was subsequently used as a stamp to prepare nanoscale metal patterns on a substrate by transfer printing. To illustrate the functionality of this technique, we employed the metal patterns as the source and drain contacts of an organic field effect transistor. Using this approach, we fabricated transistors with channel lengths ranging from 70–600 nm. The performance of these devices when the channel length was reduced was studied. The drive current density increases as expected, indicating the creation of operational transistors with recognizable properties.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Nanofabrication and Lithography Techniques · Nanowire Synthesis and Applications · Force Microscopy Techniques and Applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (45)

Show source-provided references
1. Bio-inspired sensitive and reversible mechanochromisms via strain-dependent cracks and folds10.1038/ncomms11802 ↗
2. DNA biosensors and microarrays10.1021/cr0684467 ↗
3. Biochemistry nanosensor-based hybrid metallic nanostructures array10.1016/j.snb.2008.11.019 ↗
4. One-dimensional nanostructures for electronic and optoelectronic devices10.1007/s12200-010-0001-4 ↗
5. Plasmon–molecule interactions10.1016/j.nantod.2010.08.009 ↗
6. Implantation and growth of dendritic gold nanostructures on graphene derivatives: electrical property tailoring and raman enhancement10.1021/nn900504v ↗
7. Lithographically patterned nanowire electrodeposition: a method for patterning eletrically continuous metal nanowires on dielectrics10.1021/nn800394k ↗
8. Flow condition in resist spray coating and patterning performance for three-dimensional photolithography over deep structures10.1143/JJAP.43.2387 ↗
9. Large-scale process optimization for focused ion beam 3D nanofabrication10.1007/s00170-012-4429-0 ↗
10. Recent developments in nanofabrication using focused ion beams10.1002/smll.200500113 ↗
11. Resolution limits of electron-beam lithography toward the atomic scale10.1021/nl304715p ↗
12. Soft lithography for micro- and nanoscale patterning10.1038/nprot.2009.234 ↗
13. Nanoimprint lithography: methods and material requirements10.1002/adma.200600882 ↗
14. Non-lithographic wrinkle nanochannels for protein preconcentration10.1002/adma.200701715 ↗
15. Patterning by controlled cracking10.1038/nature11002 ↗
16. Unconventional micro-/nanofabrication technologies for hybrid-scale10.1039/C6LC01058J ↗
17. Strain-controlled growth of nanowires within thin-film cracks10.1038/nmat1128 ↗
18. Tuneable elastomeric nanochannels for nanofluidic manipulation10.1038/nmat1907 ↗
19. Mechanical control of surface adsorption by nanoscale cracking10.1002/adma.201306335 ↗
20. Nanoscale electrodes for flexible electronics by swelling controlled cracking10.1002/adma.201601007 ↗
21. Bio-inspired sensitive and reversible mechanochromisms via strain-dependent cracks and folds10.1038/ncomms11802 ↗
22. Cracking in drying colloidal films10.1103/PhysRevLett.98.218302 ↗
23. Self-replicating cracks: a collaborative fracture mode in thin films10.1103/PhysRevLett.113.085502 ↗
24. Crack pattern formation in thin film lithium-ion battery electrodes10.1149/1.3574027 ↗
25. Crack formation and prevention in colloidal drops10.1038/srep13166 ↗
26. The control of crack arrays in thin films10.1007/s10853-013-7700-3 ↗
27. Periodic cracking of films supported on compliant substrates10.1016/j.jmps.2011.04.009 ↗
28. Dimensional control of brittle nanoplatelets. A statistical analysis of a thin film cracking approach10.1021/nl061225w ↗
29. Control and manipulation of nano cracks mimicking optical wave10.1038/srep17292 ↗
30. Mixed mode cracking in layered materials10.1016/S0065-2156(08)70164-9 ↗
31. Cracking in drying colloidal films10.1103/PhysRevLett.98.218302 ↗
32. Fracture of colloidal single-crystal films fabricated by controlled vertical drying deposition10.1103/PhysRevE.82.031602 ↗
33. Plasticity and fracture in drying colloidal films10.1103/PhysRevLett.110.024301 ↗
34. Cracking in drying colloidal films of flocculated dispersions10.1021/la804331c ↗
35. Crack formation and prevention in colloidal drops10.1038/srep13166 ↗
36. The near-tip fields of fast cracks10.1126/science.1180476 ↗
37. Guided fracture of films on soft substrates to create micro/nano-feature arrays with controlled periodicity10.1038/srep03027 ↗
38. The mechanical properties of a surface-modified layer on poly(dimethylsiloxane)10.1557/JMR.2008.0029 ↗
39. Collapse of stamps for soft lithography due to interfacial adhesion10.1063/1.1900303 ↗
40. Fabrication of 70 nm channel length polymer organic thin-film transistors using nanoimprint lithography10.1063/1.1526457 ↗
41. Modeling of short-channel effects in organic thin-film transistors10.1109/TED.2008.2003022 ↗
42. Suppression of short channel effect in organic thin film transistors10.1063/1.2785118 ↗
43. Enhancement of carrier mobility along with anisotropic transport in non-regiocontrolled poly (3-hexylthiophene) films processed by floating film transfer method10.1016/j.orgel.2016.08.003 ↗
44. Influence of backbone structure on orientation of conjugated polymers in the dynamic casting of thin floating-films10.1016/j.tsf.2016.11.015 ↗
45. Enhancement of transport characteristics in poly(3-hexylthiophene) films deposited with floating film transfer method10.1143/APEX.2.111502 ↗