journal article·2022-05-11

Metaphosphate-Bridged Interface Boosts High-Performance Lithium Storage

Yanli Chen, Jiaqi Ma, Qiong Peng, Xiu Gong, Jie Lin, Xiaosi Qi, Hang Guo

ACS Applied Materials & Interfaces· Volume 14· Issue 18
Publisher page

Abstract

Carbon materials with well-dispersed SnO x particles exhibit excellent lithium-storage performance. However, the volume change of SnO x and the weak interaction between SnO x and carbon induce an unsteady SnO x –C interface during the lithiation/delithiation process. This phenomenon results in enhanced charge transfer resistance and reduced electrical contact of active materials, which leads to low reversibility of tin oxidation, restricted capacity, sluggish kinetics, structural deterioration, and rapid capacity decay. Herein, tin oxide/carbon composites with a metaphosphate-bridged interface are synthesized to construct a robust interfacial contact between tin oxides and carbon. The metaphosphate group functions as a bridge between SnO x and carbon and results in excellent electrochemical stability during the charge/discharge process, which is favorable for electrode structural integrity. The formation of the metaphosphate-bridged interface provides a steady transport channel for e – /Li + and thus improves the reversibility of the conversion reaction. The enhanced charge transfer and interaction can also boost the charge transfer between SnO x and carbon, which leads to higher SnO x utilization. Thus, the prepared P-SnO x /C anode exhibits enhanced lithium-storage performance in terms of specific capacity, cycling stability, and rate performance.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Advancements in Battery Materials · Advanced Battery Materials and Technologies · Advanced Battery Technologies Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

College of Physics, Guizhou University, Guiyang, Guizhou 550025, P. R. China

College of Materials, Xiamen University, Xiamen, Fujian 361005, P. R. China

Pen-Tung Sah Institute of Micro-Nano Science and Technology, Xiamen University, Xiamen, Fujian 361005, P. R. China

Funding

Natural Science Foundation of Guizhou Province · Fok Ying Tung Education Foundation · National Natural Science Foundation of China · Natural Science Special (Special Post) Research Foundation of Guizhou University · Major Research Project of innovative Group of Guizhou province

References (49)

Show source-provided references
1. 10.1021/cm901452z10.1021/cm901452z ↗
2. 10.1038/s41467-020-15355-010.1038/s41467-020-15355-0 ↗
3. 10.1038/s41560-020-00764-810.1038/s41560-020-00764-8 ↗
4. 10.1016/j.ensm.2020.11.02810.1016/j.ensm.2020.11.028 ↗
5. 10.1021/acsnano.8b0058610.1021/acsnano.8b00586 ↗
6. 10.1016/j.ensm.2021.05.00810.1016/j.ensm.2021.05.008 ↗
7. 10.1002/adfm.20201052610.1002/adfm.202010526 ↗
8. 10.1016/j.nanoen.2020.10481510.1016/j.nanoen.2020.104815 ↗
9. 10.1126/science.276.5317.139510.1126/science.276.5317.1395 ↗
10. 10.1016/j.ensm.2020.12.03310.1016/j.ensm.2020.12.033 ↗
11. 10.1021/cm502560310.1021/cm5025603 ↗
12. 10.1021/nl200272n10.1021/nl200272n ↗
13. 10.1038/451652a10.1038/451652a ↗
14. 10.1126/science.119859110.1126/science.1198591 ↗
15. 10.1016/j.nanoen.2017.06.02110.1016/j.nanoen.2017.06.021 ↗
16. 10.1002/smll.20150218310.1002/smll.201502183 ↗
17. 10.1021/nl403631h10.1021/nl403631h ↗
18. 10.1039/C9NR03445E10.1039/C9NR03445E ↗
19. 10.1021/acsami.6b1080710.1021/acsami.6b10807 ↗
20. 10.1016/j.electacta.2021.13783410.1016/j.electacta.2021.137834 ↗
21. 10.1021/acsaem.9b0120510.1021/acsaem.9b01205 ↗
22. 10.1021/acsnano.8b0977310.1021/acsnano.8b09773 ↗
23. 10.1002/adma.20207031910.1002/adma.202070319 ↗
24. 10.1016/j.electacta.2021.13819510.1016/j.electacta.2021.138195 ↗
25. 10.1016/j.jallcom.2017.11.12710.1016/j.jallcom.2017.11.127 ↗
26. 10.1016/j.carbon.2018.02.07910.1016/j.carbon.2018.02.079 ↗
27. 10.3390/ma1106090410.3390/ma11060904 ↗
28. 10.1016/j.tsf.2015.09.02610.1016/j.tsf.2015.09.026 ↗
29. 10.1016/j.carbon.2020.06.05010.1016/j.carbon.2020.06.050 ↗
30. 10.1038/s41598-020-78078-810.1038/s41598-020-78078-8 ↗
31. 10.1007/s11051-021-05187-410.1007/s11051-021-05187-4 ↗
32. 10.1007/s40843-017-9218-610.1007/s40843-017-9218-6 ↗
33. 10.1016/j.apsusc.2019.06.12910.1016/j.apsusc.2019.06.129 ↗
34. 10.1016/j.matdes.2004.08.02010.1016/j.matdes.2004.08.020 ↗
35. 10.1016/j.nanoen.2016.12.05810.1016/j.nanoen.2016.12.058 ↗
36. 10.1021/acsami.9b1181710.1021/acsami.9b11817 ↗
37. 10.1177/07349041900080020210.1177/073490419000800202 ↗
38. 10.1186/2228-5326-2-1710.1186/2228-5326-2-17 ↗
39. 10.1007/BF0049162410.1007/BF00491624 ↗
40. 10.1021/cm503268810.1021/cm5032688 ↗
41. 10.1016/j.matlet.2015.06.05610.1016/j.matlet.2015.06.056 ↗
42. 10.1016/j.electacta.2017.11.01810.1016/j.electacta.2017.11.018 ↗
43. 10.1016/j.electacta.2014.07.09010.1016/j.electacta.2014.07.090 ↗
44. 10.1002/aenm.20210004610.1002/aenm.202100046 ↗
45. 10.1021/acsomega.9b0166510.1021/acsomega.9b01665 ↗
46. 10.1016/j.nanoen.2015.10.02610.1016/j.nanoen.2015.10.026 ↗
47. 10.1016/j.jpowsour.2018.09.01410.1016/j.jpowsour.2018.09.014 ↗
48. 10.1039/D1TA05108C10.1039/D1TA05108C ↗
49. Lan, X.; Cui, J.; Zhang, X.; Hu, R.; Tan, L.; He, J.; Zhang, H.; Xiong, X.; Yang, X.; Wu, S.; Zhu, M. Achieving over 90% initial Coulombic Efficiency and Highly Stable Li Storage in SnO2 by Constructing Interfacial Oxygen Redistribution in Multilayers; Research Square, 2021.10.21203/rs.3.rs-243641/v1 ↗