journal article·2011-12

Dielectric and impedance spectroscopic studies of (Sr1−x Pb x )TiO2 glass ceramics with addition of Nb2O5

C. R. Gautam, Devendra Kumar, Om. Parkash

Bulletin of Materials Science· Volume 34· Issue 7
Publisher page

Abstract

Glasses were made by melt-quench method in the system [(Sr1−x Pb x )O·TiO2]-[2SiO2·B2O3]-5[K2O-BaO] (0·0 ≤ x ≤ 0·4) with addition of 1 mol% Nb2O5. Perovskite strontium lead titanate in solid solution phase has been crystallized in borosilicate glassy matrix with suitable choice of composition and heat treatment schedule. Addition of 1 mol% of Nb2O5 enhances the crystallization of lead strontium titanate phase in the glassy matrix. Scanning electron microscopy (SEM) is performed to study the surface morphology of the crystallites and crystalline interface to the glass. Dielectric properties of these glass ceramics were studied by measuring capacitance and dissipation factor as a function of temperature at a few selected frequencies. Nb2O5 doped strontium lead titanate glass ceramic shows a high value of dielectric constant. It is of the order of 10,000 while the dielectric constant of undoped glass ceramic sample is of the order of 500. Complex impedance and modulus spectroscopic techniques were used to find out the contributions of polarization of crystallites and glass crystal interfaces to the resulting dielectric behaviour.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Ferroelectric and Piezoelectric Materials · Microwave Dielectric Ceramics Synthesis · Glass properties and applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (23)

Show source-provided references
1. Herczog A 1964 J. Am. Ceram. Soc. 47 10710.1111/j.1151-2916.1964.tb14366.x ↗
2. Herczog A 1984 J. Am. Ceram. Soc. 67 48410.1111/j.1151-2916.1984.tb19640.x ↗
3. Hiremath V A, Date S K and Kulkarni S M 2001 Bull. Mater. Sci. 24 1001
4. Keith H D and Padden F J 1963 J. Appl. Phys. 34 240910.1063/1.1702757 ↗
5. Kokubo T and Tashiro M 1973/74 J. Non-Cryst. Solids 13 32810.1016/0022-3093(74)90101-X ↗
6. Lynch S M and Shelby J E 1984 J. Am. Ceram. Soc. 67 42410.1111/j.1151-2916.1984.tb19729.x ↗
7. MacDonald J R 1987 Impedance spectroscopy (New York: Wiley)
8. Mandal R K, Durga Prasad C, Parkash O and Kumar D 1987 Bull. Mater. Sci. 9 25510.1007/BF02743974 ↗
9. McCauley D, Newnham R E and Randall C A 1998 J. Am. Ceram. Soc. 81 97910.1111/j.1151-2916.1998.tb02435.x ↗
10. Morrison F D, Sinclair D C and West A R 1999 J. Appl. Phys. 86 635510.1063/1.371698 ↗
11. Parkash O, Kumar D and Pandey L 1986 Bull. Mater. Sci. 8 1310.1007/BF02744092 ↗
12. Sahu A K, Kumar D and Parkash O 2003 Br. Ceram. Trans. 102 13910.1179/096797803225004981 ↗
13. Shyu J and Yang Y 1995 J. Am. Ceram. Soc. 78 146310.1111/j.1151-2916.1995.tb08838.x ↗
14. Sinclair D C and West A R 1988 J. Mat. Sci. Lett. 7 82310.1007/BF00723773 ↗
15. Sinclair D C and West A R 1989 J. Appl. Phys. 68 385010.1063/1.344049 ↗
16. Swartz S L, Bhalla A S and Cross L E 1986 J. Appl. Phys. 60 206910.1063/1.337211 ↗
17. Swartz S L, Bhalla A S, Cross L E and Lawless W N 1988a J. Mater. Sci. 23 400410.1007/BF01106828 ↗
18. Swartz S L, Breval E and Bhalla A S 1988b Am. Ceram. Soc. Bull. 67 63
19. Swartz S L, Lanagan M T, Schulze W A and Cross L E 1983 Ferroelectrics 50 31310.1080/00150198308014468 ↗
20. Thakur O P 1998 Crystallization, microstructure and dielectric behaviour of strontium titanate borosilicate glass ceramics with some additives, Ph D thesis, Banaras Hindu University, Varanasi, India
21. Thakur O P, Kumar D, Parkash O and Pandey L 1995 Mater. Lett. 37 25310.1016/0167-577X(95)00043-7 ↗
22. Thakur O P, Kumar D, Parkash O and Pandey L 1997 Ind. J. Phys. 71 161
23. Thakur O P, Kumar D, Parkash O and Pandey L 2002 J. Mater. Sci. 37 259710.1023/A:1015476631462 ↗