Temperature-Dependent Oxidation Behavior of Silicon Carbide Surface: Reactive Molecular Dynamics Simulations
Source abstract
Abstract
The high-temperature oxidation mechanism of silicon carbide (SiC) is crucial for designing thermal protection systems in aircraft. This study explored the oxidative chemical reaction processes and mechanism on SiC surface and interfaces within the temperature range of 300–2300 K by using reactive molecular dynamics simulation. The oxygen impact on the silica (SiO x ) growth of the SiC surface was analyzed, which shows a progressive increase of silica thickness. The simulation results indicated that the oxidation process of SiC was a typical passive oxidation mechanism. With the environmental temperature rising and oxygen impact, the increase of oxidation thickness on the SiC surface undergoes three oxidizing reaction processes: little chemical adsorption of oxygen molecules on the initial surface, rapid oxidation of silicon and carbon, and dramatic oxidation of the interface between the oxidation layer and SiC. Additionally, this work studied the mechanism of oxidation thickness growth and chemical diffusion of oxygen. The oxidation rate is weakened according to the oxygen atom diffusion barrier effect of silica repulsion. Moreover, the kinetic parameters were statistically calculated by fitting the growth of Si–O bonds and their reaction rate constants. Subsequently, the activation energy and pre-exponential factors were derived by using the Arrhenius equation to model the chemical reaction kinetics of the thermal oxidation process. The chemical reaction behaviors of the two stages could be concluded as follows: (i) in stage I, the initial oxidation is reaction rate limiting; (ii) in stage II, SiC oxidation is limited by both the oxidation reaction rate and the oxygen diffusion coefficient of the oxidation layer. The activation energy of stage II increased compared with stage I due to the oxygen atoms diffusion barrier between the oxidation layers. This study on the oxidation and ablation mechanism of the SiC surface at the atomic scale would provide insight into understanding thermal oxidation behavior and the design of ceramic materials.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Semiconductor materials and devices · Diamond and Carbon-based Materials Research · Ion-surface interactions and analysis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
State Key Laboratory of Environment-friendly Energy Materials, Southwest University of Science and Technology, Mianyang 621010, China
State Key Laboratory of Aerodynamics, Mianyang 621000, China
Funding
National Natural Science Foundation of China · Southwest University of Science and Technology · State Key Laboratory of Aerodynamics
References (53)
Show source-provided references
1. 10.1016/j.corsci.2021.10933110.1016/j.corsci.2021.109331 ↗
2. 10.1016/j.corsci.2022.11080210.1016/j.corsci.2022.110802 ↗
3. 10.1016/j.ceramint.2018.01.12510.1016/j.ceramint.2018.01.125 ↗
4. Guo Y.-J. · Acta Aerodyn. Sin. · 2012 · 30 · 34
5. 10.1007/s11085-010-9216-410.1007/s11085-010-9216-4 ↗
6. 10.1111/jace.1210810.1111/jace.12108 ↗
7. 10.1111/jace.1210410.1111/jace.12104 ↗
8. 10.1063/1.172342910.1063/1.1723429 ↗
9. 10.1111/j.1151-2916.1996.tb08724.x10.1111/j.1151-2916.1996.tb08724.x ↗
10. 10.1016/j.corsci.2014.07.05210.1016/j.corsci.2014.07.052 ↗
11. 10.1116/1.58095110.1116/1.580951 ↗
12. 10.1007/s40195-022-01375-w10.1007/s40195-022-01375-w ↗
13. 10.1038/s41598-017-13569-910.1038/s41598-017-13569-9 ↗
14. 10.1016/j.surfcoat.2020.12533510.1016/j.surfcoat.2020.125335 ↗
15. 10.1088/1674-1056/24/9/09620310.1088/1674-1056/24/9/096203 ↗
16. 10.1021/acs.jpca.7b0898310.1021/acs.jpca.7b08983 ↗
17. 10.1021/jp306391p10.1021/jp306391p ↗
18. 10.1021/jp307680t10.1021/jp307680t ↗
19. 10.1016/j.commatsci.2021.11034110.1016/j.commatsci.2021.110341 ↗
20. 10.1016/j.fuel.2020.11948410.1016/j.fuel.2020.119484 ↗
21. 10.1016/j.polymdegradstab.2022.11003810.1016/j.polymdegradstab.2022.110038 ↗
22. 10.1016/j.cej.2024.15072810.1016/j.cej.2024.150728 ↗
23. 10.1021/acs.jpca.6b0677010.1021/acs.jpca.6b06770 ↗
24. 10.1021/acs.jpca.1c0693910.1021/acs.jpca.1c06939 ↗
25. 10.1016/j.fuel.2020.11798910.1016/j.fuel.2020.117989 ↗
26. 10.1016/j.apsusc.2023.15828010.1016/j.apsusc.2023.158280 ↗
27. 10.1021/acsami.1c2395010.1021/acsami.1c23950 ↗
28. 10.1016/j.triboint.2023.10919110.1016/j.triboint.2023.109191 ↗
29. 10.1016/j.apsusc.2020.14832110.1016/j.apsusc.2020.148321 ↗
30. Shi, L.; Sessim, M.; Tonks, M.; Phillpot, S. Modeling Carbon Fiber Oxidation under High Temperature by ReaxFF Based Molecular Dynamics Simulation. AIAA Scitech 2020 Forum; AIAA: Orlando, FL, 2020.10.2514/6.2020-0484 ↗
31. 10.1016/j.apsusc.2020.14524710.1016/j.apsusc.2020.145247 ↗
32. 10.1016/j.commatsci.2021.11075110.1016/j.commatsci.2021.110751 ↗
33. 10.1016/j.commatsci.2020.10988110.1016/j.commatsci.2020.109881 ↗
34. 10.1063/5.004484010.1063/5.0044840 ↗
35. 10.1021/jp027630310.1021/jp0276303 ↗
36. 10.1021/acs.langmuir.7b0310210.1021/acs.langmuir.7b03102 ↗
37. 10.1021/acs.langmuir.3c0076410.1021/acs.langmuir.3c00764 ↗
38. 10.1021/acsanm.3c0207710.1021/acsanm.3c02077 ↗
39. 10.1016/j.ceramint.2023.11.07010.1016/j.ceramint.2023.11.070 ↗
40. 10.1016/j.jaap.2022.10562010.1016/j.jaap.2022.105620 ↗
41. 10.1038/npjcompumats.2015.1110.1038/npjcompumats.2015.11 ↗
42. 10.1006/jcph.1995.103910.1006/jcph.1995.1039 ↗
43. 10.1063/1.44811810.1063/1.448118 ↗
44. 10.1088/0965-0393/18/1/01501210.1088/0965-0393/18/1/015012 ↗
45. 10.3390/app1109427810.3390/app11094278 ↗
46. 10.1139/p03-07710.1139/p03-077 ↗
47. 10.1163/15685510377265849810.1163/156855103772658498 ↗
48. 10.1111/jace.1283310.1111/jace.12833 ↗
49. 10.1016/j.jnucmat.2020.15230810.1016/j.jnucmat.2020.152308 ↗
50. 10.1063/5.009200510.1063/5.0092005 ↗
51. 10.1063/1.509805110.1063/1.5098051 ↗
52. Einstein A. · Annalen. Der. Phys. · 1905 · 17 · 54910.1002/andp.19053220806 ↗
53. 10.1016/j.jeurceramsoc.2021.04.04010.1016/j.jeurceramsoc.2021.04.040 ↗