Promotion of Oxygen Reduction Reaction Durability of Carbon-Supported PtAu Catalysts by Surface Segregation and TiO2Addition
Source abstract
Abstract
Highly effective carbon supported-Pt75Au25 catalysts for oxygen reduction reaction (ORR) are prepared though titanium dioxide modification and post heat treatment. After accelerated durability test (ADT) of 1700 cycles, the ORR activity of PtAu/C catalysts modified by TiO2 and air heat treatment is 3 times higher than that of the commercial Pt/C. The enhancement of ORR activity is attributed to surface and structural alteration by air-induced Pt surface segregation and lower unfilled d states. On the contrary, for TiO2 modified and H2 treated PtAu/C catalysts, the deterioration of the ORR activity may be due to the loss of electrochemical surface area after ADT and the increase of d-band vacancy.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Electrocatalysts for Energy Conversion · Fuel Cells and Related Materials · Catalytic Processes in Materials Science
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Institute of Materials Science and Engineering, National Central University, Taoyuan 320, Taiwan
Material and Chemical Research Laboratories, Industrial Technology Research Institute, Hsinchu 310, Taiwan
References (32)
Show source-provided references
1. Sarma L. S. · Langmuir · 2007 · 23 · 580210.1021/la0637418 ↗
2. Ralph T. · Platinum Met. Rev. · 2002 · 46 · 11710.1595/003214002X463117135 ↗
3. Ferreira P. J. · J. Electrochem. Soc. · 2005 · 152 · A225610.1149/1.2050347 ↗
4. Antolini E. · J. Mater. Sci. · 2003 · 38 · 299510.1023/A:1024771618027 ↗
5. Blurton K. · Electrochimi. Acta · 1978 · 23 · 18310.1016/0013-4686(78)85044-0 ↗
6. Zhai Y. · J. Power Sources · 2007 · 164 · 12610.1016/j.jpowsour.2006.09.069 ↗
7. Zhang J. · Science · 2007 · 315 · 22010.1126/science.1134569 ↗
8. Fang Y. H. · J. Phys. Chem. C · 2011 · 115 · 1750810.1021/jp205376b ↗
9. Mukerjee S. · J. Electrochem. Soc. · 1995 · 142 · 140910.1149/1.2048590 ↗
10. Liu C. W. · J. Colloid Interface Sci. · 2009 · 336 · 65410.1016/j.jcis.2009.04.081 ↗
11. Liu X. · J. Power Sources · 2010 · 195 · 409810.1016/j.jpowsour.2010.01.077 ↗
12. Huang K. · J. Mater. Chem. · 2012 · 22 · 1682410.1039/c2jm32234j ↗
13. Liu G. · Electrochem. Commun. · 2007 · 9 · 13510.1016/j.elecom.2006.08.056 ↗
14. Kim D. S. · Appli. Catal. A: General · 2007 · 323 · 11010.1016/j.apcata.2007.02.010 ↗
15. Sathiyanarayanan S. · Electrochimi. Acta · 2007 · 52 · 206810.1016/j.electacta.2006.08.022 ↗
16. Shim J. · J. Power Sources · 2001 · 102 · 17210.1016/S0378-7753(01)00817-5 ↗
17. Sarkar A. · J. Phys. Chem. C · 2008 · 112 · 1203710.1021/jp801824g ↗
18. Liu C. W. · Chem. Commun. · 2010 · 46 · 248310.1039/b920212a ↗
19. Wei Y. C. · ChemPhysChem · 2009 · 10 · 123010.1002/cphc.200800685 ↗
20. Li X. · Electrochimi. Acta · 2006 · 52 · 135810.1016/j.electacta.2006.07.037 ↗
21. Wei Y. C. · J. Alloys Compd. · 2011 · 509 · 53510.1016/j.jallcom.2010.09.096 ↗
22. Pozio A. · J. Power Sources · 2002 · 105 · 1310.1016/S0378-7753(01)00921-1 ↗
23. Ticianelli E. · J. Appl. Electrochem. · 1991 · 21 · 59710.1007/BF01024847 ↗
24. Antolini E. · J. Power Sources · 1999 · 77 · 13610.1016/S0378-7753(98)00186-4 ↗
25. Chen J. · J. Am. Chem. Soc. · 2004 · 126 · 1085410.1021/ja0468224 ↗
26. Huang K. · J. Mater. Chem. · 2012 · 22 · 1682410.1039/c2jm32234j ↗
27. Choi J. H. · J. Electrochem. Soc. · 2006 · 153 · A181210.1149/1.2224055 ↗
28. Liu H. · J. Phys. Chem. C · 2008 · 112 · 1917310.1021/jp802804u ↗
29. Liu C. W. · J. Phys. Chem. C · 2011 · 115 · 870210.1021/jp1120614 ↗
30. Lai F. J. · J. Phys. Chem. C · 2009 · 113 · 1267410.1021/jp903105e ↗
31. Lai F. J. · Chem.—Eur. J. · 2010 · 16 · 460210.1002/chem.200902263 ↗
32. Yeh T.-H. · Electrochem. Commun. · 2013 · 31 · 12510.1016/j.elecom.2013.03.025 ↗