New skin corrosion effect of magnetorheological electro-Fenton polishing investigated by friction and wear experiments
Source abstract
Abstract
Currently, most magnetorheological polishing methods use point or linear scanning. When these methods are applied to large-size semiconductor polishing, they are often limited by efficiency, making it difficult to simultaneously consider the surface quality and processing efficiency. In addition, because the mechanism of magnetorheological polishing is not yet clear, it is difficult to achieve the effect of synergistic enhancement of polishing efficiency and surface quality by simply increasing the magnetic field strength or introducing chemical reactions. In this paper, we propose a new method of combining the flexible force of magnetorheological action with the controllable electro-Fenton chemical action, and experimentally confirm the mechanism of the new skin corrosion effect that occurs under the flexible force applied to the magnetorheological micro-abrasive head, which provides a favorable theoretical research basis for improving the quality and efficiency of magnetorheological polishing. We also simulated the process using a magnetorheological electro-Fenton friction wear device and analyzed the influence of various parameters on the formation of the new skin corrosion effect. The results show that in the case of conventional friction and wear methods failing to form significant material removal corrosion trajectories, the composite friction method of magnetorheological electro-Fenton was able to form a corrosion layer of significant thickness over the entire range of action after the use of magnetorheological electro-Fenton composite friction method. Different third-generation semiconductor materials and crystal directions are presented with very significant corrosion effects. In particular, the best results were obtained when H 2 O 2 was continuously added at a rate of 0.30 g/min, a current parameter of 20 mA, a concentration of 3 wt% diamond particles, and a load of 0.418 N was applied, resulting in a cracked corrosion layer.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Corrosion Behavior and Inhibition · Advanced Surface Polishing Techniques · Diamond and Carbon-based Materials Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (28)
Show source-provided references
1. Progress in electrochemical etching of third-generation semiconductors10.1149/2162-8777/acce03 ↗
2. Effects of thermal boundary resistance on thermal management of gallium-nitride-based semiconductor devices: A review10.3390/mi14112076 ↗
3. Chemical mechanical polishing for sapphire wafers using a developed slurry10.1016/j.jmapro.2021.01.004 ↗
4. A novel slurry for chemical mechanical polishing of single crystal diamond10.1016/j.apsusc.2021.150431 ↗
5. Atomic surface of silicon wafers induced by grafted silica nanoparticles and sodium carbonate10.1016/j.apsusc.2024.160234 ↗
6. Atomic surface achieved through a novel cross-scale model from macroscale to nanoscale10.1039/D3NR05278H ↗
7. Advanced polishing methods for atomic-scale surfaces: A review
8. Highly efficient and atomic scale polishing of GaN via plasma-based atom-selective etching10.1016/j.apsusc.2023.156786 ↗
9. Chemical mechanical polishing of silicon carbide (SiC) based on coupling effect of ultrasonic vibration and catalysis10.1016/j.jece.2023.111080 ↗
10. Catalytic mechanism of tribochemical mechanical polishing on (0001) C-face of single crystal 6H-SiC substrate10.1007/s00170-023-11494-y ↗
11. UV-TiO2 photocatalysis-assisted chemical mechanical polishing 4H-SiC wafer10.1080/10426914.2017.1364855 ↗
12. Highly efficient and damage-free polishing of GaN (0 0 0 1) by electrochemical etching-enhanced CMP process10.1016/j.apsusc.2020.145957 ↗
13. Tribological approaches to material removal rate during chemical mechanical polishing10.1007/s12540-013-2031-0 ↗
14. Tribo-electrochemical study of stainless steel surfaces during chemical–mechanical polishing10.1002/ls.1336 ↗
15. Mechanical wear behavior between CeO2 (100), CeO2 (110), CeO2 (111), and silicon studied through atomic force microscopy10.1016/j.triboint.2020.106616 ↗
16. Tribological behavior of 6H–SiC wafers in different chemical mechanical polishing slurries
17. Kinetic modeling of the electro-Fenton process: quantification of reactive oxygen species generation10.1016/j.electacta.2015.06.103 ↗
18. Cooperative roles of chemical reactions and mechanical friction in chemical mechanical polishing of gallium nitride assisted by OH radicals: tight-binding quantum chemical molecular dynamics simulations10.1039/D0CP05826B ↗
19. Mathematical model of material removal for magnetorheological polishing10.3901/JME.2004.04.067 ↗
20. Feng · 2000
21. Study of initiation and development of local oxidation phenomena during anodizing of SiC10.1016/j.elecom.2018.02.013 ↗
22. Liquid electrolyte-free electrochemical oxidation of GaN surface using a solid polymer electrolyte toward electrochemical mechanical polishing10.1016/j.elecom.2018.11.006 ↗
23. Study of corrosion rate control mechanism based on magnetorheological electro-fenton composite polishing of single-crystal GaN wafers10.1007/s10008-023-05468-z ↗
24. Friction and wear mechanisms for single crystal GaN based on an electro-fenton enhanced chemical reaction
25. Electro-fenton process and related electrochemical technologies based on Fenton’s reaction chemistry10.1021/cr900136g ↗
26. Hydrothermal synthesis of alpha alumina (α-Al2O3) powders: study of the processing variables and growth mechanisms10.1111/j.1551-2916.2009.03399.x ↗
27. Atomistic mechanisms of chemical mechanical polishing of diamond (1 0 0) in aqueous H2O2/pure H2O: molecular dynamics simulations using reactive force field (reaxff)10.1016/j.commatsci.2018.10.041 ↗
28. MD simulation of chemically enhanced polishing of 6H-SiC in aqueous H2O210.1016/j.jmapro.2023.10.056 ↗