journal article·2022-09

Crack damage control for diamond wire sawing of silicon: The selection of processing parameters

Mengran Ge, Zibin Chen, Peizhi Wang, Peiqi Ge

Publisher page

Abstract

Fixed diamond wire sawing has been the most common technology to cut mono- and multi-crystalline silicon into wafers in the fields of photovoltaics and integrated circuits. The crack damage inevitably occurred in wire sawing is preventing the further reduction of wafer manufacturing cost due to wafer breakage and subsequent crack damage removal. This paper presents a numerical model to predict the processing parameters for a given expected crack damage depth of as-cut wafers, aiming to realize the control of crack damage. The model adopts a classic median-and-lateral crack system to describe the crack damage induced by the scratching of diamond abrasives randomly distributed on wire. The key processing parameter - the ratio of feed speed to wire speed - is determined by making the calculated crack damage depth equal to the expected value. The deflection/bow angle of wire is checked to avoid excessive end-cutting time and severe shape deviation of wafers. The established model is verified by wire sawing experiments using the processing parameters predicted by this model. The maximum relative error between experimental values and expected values of the crack damage depth is 5.26%. This model can be applied to the industrial crack damage control of as-cut wafers by the selection of processing parameters.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced Surface Polishing Techniques · Diamond and Carbon-based Materials Research · Advanced machining processes and optimization

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (39)

Show source-provided references
1. Wire sawing technology: A state-of-the-art review10.1016/j.precisioneng.2015.08.008 ↗
2. Simulation analysis on cutting forces based on surface topography of fixed abrasive wire saw10.1016/j.mssp.2021.105900 ↗
3. Research on the capillary penetration mechanism of cutting fluid supplied by electrostatic spraying in diamond wire sawing10.1016/j.jmapro.2021.08.004 ↗
4. Research on the machinability of A-plane sapphire under diamond wire sawing in different sawing directions10.1016/j.ceramint.2019.02.086 ↗
5. Diamond wire sawing of solar silicon wafers: a sustainable manufacturing alternative to loose abrasive slurry sawing10.1016/j.promfg.2018.02.156 ↗
6. Surface damage and metal-catalyzed chemical etching investigation of multicrystalline silicon by diamond wire sawing10.1016/j.solener.2020.07.019 ↗
7. Mechanisms of material removal and subsurface damage in fixed-abrasive diamond wire slicing of single-crystalline silicon10.1016/j.precisioneng.2017.04.011 ↗
8. The study of crack damage and fracture strength for single crystal silicon wafers sawn by fixed diamond wire10.1016/j.mssp.2021.106017 ↗
9. Study of ductile-to-brittle transition in single grit diamond scribing of silicon: application to wire sawing of silicon wafers10.1115/1.4006177 ↗
10. Experimental and numerical analysis of scratching induced damage during diamond wire sawing of silicon10.1016/j.wear.2020.203328 ↗
11. Investigation on secondary self-sharpness performance of hollow-sphere abrasive grains in belt grinding of titanium alloy10.1016/j.jmapro.2020.09.030 ↗
12. Elastic/plastic indentation damage in ceramics: the median/radial crack system10.1111/j.1151-2916.1980.tb10768.x ↗
13. Elastic/plastic indentation damage in ceramics: the lateral crack system10.1111/j.1151-2916.1982.tb10782.x ↗
14. Elastic stress fields caused by indenting brittle materials10.1080/01418618208236917 ↗
15. Sliding microindentation fracture of brittle materials: role of elastic stress fields10.1016/S0167-6636(98)00012-X ↗
16. Elastic stress field model and micro-crack evolution for isotropic brittle materials during single grit scratching10.1016/j.ceramint.2017.05.054 ↗
17. Towards understanding the brittle-ductile transition in the extreme manufacturing
18. Investigation on critical crack-free cutting depth for single crystal silicon slicing with fixed abrasive wire saw based on the scratching machining experiments10.1016/j.mssp.2017.10.027 ↗
19. Anisotropy dependence of material removal and deformation mechanisms during nanoscratch of gallium nitride single crystals on (0001) plane10.1016/j.apsusc.2021.152028 ↗
20. Strain-rate dependence of surface/subsurface deformation mechanisms during nanoscratching tests of GGG single crystal10.1016/j.ceramint.2019.04.238 ↗
21. Modeling and simulation of phase transformation and crack formation during scribing of mono-crystalline silicon10.1016/j.ijmecsci.2020.105527 ↗
22. Effect of grit shape and crystal structure on damage in diamond wire scribing of silicon10.1111/jace.14732 ↗
23. Material removal of optical glass BK7 during single and double scratch tests10.1016/j.wear.2010.10.064 ↗
24. Analysis of grit interference mechanisms for the double scratching of monocrystalline silicon carbide by coupling the FEM and SPH10.1016/j.ijmachtools.2017.04.012 ↗
25. Crack propagation and the material removal mechanism of glass–ceramics by the scratch test10.1016/j.jmbbm.2016.07.021 ↗
26. Interaction of lateral cracks in double scratching of single-crystal silicon carbide10.1016/j.tafmec.2019.102378 ↗
27. Evaluation of fixed abrasive diamond wire sawing induced subsurface damage of solar silicon wafers10.1016/j.jmatprotec.2019.116267 ↗
28. Analytical prediction of subsurface microcrack damage depth in diamond wire sawing silicon crystal10.1016/j.mssp.2020.105015 ↗
29. Study on the subsurface damage depth of monocrystalline silicon in ultrasonic vibration assisted diamond wire sawing10.1016/j.engfracmech.2021.108077 ↗
30. Effect of cutting parameters on surface integrity of monocrystalline silicon sawn with an endless diamond wire saw10.1016/j.solener.2020.07.018 ↗
31. Experiment and theoretical prediction for surface roughness of PV polycrystalline silicon wafer in electroplated diamond wire sawing10.1016/j.jmapro.2019.11.022 ↗
32. Three-dimensional shape modeling of diamond abrasive grains measured by a scanning laser microscope10.4028/www.scientific.net/KEM.238-239.131 ↗
33. Measurement of hardness and elastic modulus by instrumented indentation: advances in understanding and refinements to methodology10.1557/jmr.2004.19.1.3 ↗
34. A scratching force model of diamond abrasive particles in wire sawing of single crystal SiC10.1016/j.mssp.2017.05.032 ↗
35. Fabrication of thin resin-bonded diamond wire and its application to ductile-mode wire sawing of mono-crystalline silicon10.1016/j.mssp.2021.105665 ↗
36. Prediction of sawing force for single-crystal silicon carbide with fixed abrasive diamond wire saw10.1016/j.mssp.2017.01.014 ↗
37. Chen · 2021
38. Liu · 2018
39. Investigation on residual scratch depth and material removal rate of scratching machining single crystal silicon with Berkovich indenter10.1016/j.mssp.2019.04.037 ↗