Enhanced infrared sensing properties of vanadium pentoxide nanofibers for bolometer application
Source abstract
Abstract
Abstract The main aim of this work is to report an alternative technique of creating vanadium pentoxide (V2O5) based uncooled infrared (IR) detector, by a state-of-the-art V2O5 nanofibers, manufactured by facile and economical electrospinning process. The nanofibers were thermally and electrically characterized to determine their bolometric performance. The nanofibers show maximum voltage responsivity ( R v ) 6987.3 V/W at 100 mA DC bias, in a normal room temperature and pressure condition. Nanofibers show very good thermal response ( τ s ) and recovery time ( τ r ) when subjected to a periodic On-Off cycle of IR lamp (150 W) illumination. Temperature dependent resistance measurement shows that nanofibers are exhibiting semiconductor to metallic phase transition at 67 °C with maximum temperature coefficient of resistance (TCR%) − 1.6%/K at the transition. V2O5 nanofibers characterized using X-ray diffraction (XRD), X-ray photoelectron spectroscopy (XPS) and Raman Spectroscopy confirms their crystallinity and elemental composition. The optical band gap of the nanofibers is analyzed by UV–Visible spectroscopy. Scanning electron microscopy (SEM) and atomic force microscopy (AFM) images confirms their microstructural dimensions and surface homogeneity. The entire analysis reaffirms the suitability of V2O5 nanofibers as one of the futuristic sensing material for IR imaging applications.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Transition Metal Oxide Nanomaterials · Gas Sensing Nanomaterials and Sensors · ZnO doping and properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (42)
Show source-provided references
1. Oxides which show a metal-to-insulator transition at the neel temperature10.1103/PhysRevLett.3.34 ↗
2. Effects of Ti–W codoping on the optical and electrical switching of vanadium dioxide thin films grown by a reactive pulsed laser deposition10.1063/1.1788883 ↗
3. Pulsed laser deposition of VO2 thin films10.1063/1.112476 ↗
4. Metal-insulator transition in epitaxial V1−xWxO2 (0≤x≤0.33) thin films10.1063/1.3291053 ↗
5. Thin-film resistance bolometer IR detectors10.1016/0020-0891(84)90048-4 ↗
6. Infrared focal plane array incorporating silicon IC process compatible bolometer10.1109/16.543017 ↗
7. H. Jerominek, F. Picard, N. Swart, M. Renaud, M. Levesque, M. Lehoux, J. Sebastien, M. Pelletier, G. Bilodeau, D. Audet, T. Pope, P. Lambert, Micromachined uncooled VO2-based IR bolometer arrays, in: In Infrared Detectors and Focal Plane Arrays IV, International Society for Optics and Photonics, 2746, 1996, pp. 60–72.10.1117/12.243056 ↗
8. E. Mottin, A. Bain, J.L. Martin, J.L. Ouvrier-Buffet, S. Bisotto, J.J. Yon, J.L. Tissot, Uncooled amorphous silicon technology enhancement for 25-μm pixel pitch achievement, in: Infrared Technology and Applications XXVIII, International Society for Optics and Photonics, 4820, 2003, pp. 200–208.10.1117/12.464848 ↗
9. A review of the growth of V2O5 films from 1885 to 201010.1016/j.tsf.2010.11.001 ↗
10. Synthesis and gas sensing behavior of nanostructured V2O5 thin films prepared by spray pyrolysis10.1016/j.mssp.2014.01.008 ↗
11. Influence of deposition temperature on the growth of vacuum evaporated V2O5 thin films10.1016/S0167-577X(03)00185-X ↗
12. Structural and optical properties of pulsed laser deposited V2O5 thin films10.1016/j.tsf.2007.08.113 ↗
13. Dependence of optical properties of vanadium oxide films on crystallization and temperature10.1016/j.tsf.2011.11.028 ↗
14. Nanostructured V2O5 thin films deposited at low sputtering power10.1016/j.mssp.2015.04.054 ↗
15. Spectroscopic characterization of electron-beam evaporated V2O5 thin films10.1016/S0040-6090(97)00141-7 ↗
16. Hydrothermal synthesis of vanadium pentoxide nanostructures and their morphology control10.1016/j.ceramint.2012.09.029 ↗
17. Temperature coefficient of resistance and thermal conductivity of vanadium oxide ‘Big Mac'sandwich structure10.1016/j.infrared.2015.03.006 ↗
18. Fabrication of vanadium oxide thin film with high-temperature coefficient of resistance using V2O5/V/V2O5 multi-layers for uncooled microbolometers10.1016/S0040-6090(02)01263-4 ↗
19. Nano-vanadium oxide thin films in phase for microbolometer applications10.1088/0022-3727/41/19/195108 ↗
20. Eco-friendly all-carbon paper electronics fabricated by a solvent-free drawing method10.1088/0957-4484/27/9/095206 ↗
21. Briggs · 1990 · 1 · 1
22. Determination of the V2p XPS binding energies for different vanadium oxidation states (V5+ to V0+)10.1016/j.elspec.2004.03.004 ↗
23. J.F. Moulder, W.F. Stricle, P.E. Sobol, K.D. Bomben, Handbook of X-ray photoelectron spectroscopy, Perkin-Elmer Corporation, Physical Electronics Division, 1995.
24. Resolving surface chemical states in XPS analysis of first row transition metals, oxides and hydroxides: Sc, Ti, V, Cu and Zn10.1016/j.apsusc.2010.07.086 ↗
25. Synthesis of vanadium pentoxide (V2O5) ultralong nanobelts via an oriented attachment growth mechanism10.1039/c1ce05477e ↗
26. Electrochemical conditioning of vanadium (V) pentoxide xerogel films10.1016/S1388-2481(99)00067-3 ↗
27. Centimeter-long V2O5 nanowires: from synthesis to field-emission, electrochemical, electrical transport, and photoconductive properties10.1002/adma.200903586 ↗
28. Nanoporous vanadium oxide network prepared by spray pyrolysis10.1016/j.matlet.2016.01.040 ↗
29. Temperature dependence of the interband transition in a V2O5 film10.1063/1.4808021 ↗
30. Geometric and electronic structure of vanadium pentoxide: a density functional bulk and surface study10.1103/PhysRevB.59.10583 ↗
31. On the electrical conductivity of V2O5 single crystals10.1002/pssa.2210200140 ↗
32. Electrical properties of V2O5 thin films obtained by atomic layer deposition (ALD)10.1039/b410324f ↗
33. Lattice vibrations of V2O5. Calculation of normal vibrations in a urey-bradley force field10.1002/pssb.2221310207 ↗
34. Synthesis of multiwalled carbon nanotube-based infrared radiation detector10.1016/j.sna.2012.08.028 ↗
35. Wearable temperature sensor based on graphene nanowalls10.1039/C5RA00871A ↗
36. Design and characterization of adaptive microbolometers10.1088/0960-1317/16/5/028 ↗
37. A plastic-based bolometer array sensor using carbon nanotubes for low-cost infrared imaging devices10.1016/j.sna.2013.03.008 ↗
38. High sensitivity bolometers from self-oriented single walled carbon nanotube composites10.1021/am2007036 ↗
39. A Low cost 128 × 128 uncooled infrared detector array in CMOS process10.1109/JMEMS.2007.910235 ↗
40. Characterization of uncooled bolometer with vanadium tungsten oxide infrared active layer
41. Multiwalled carbon nanotube films as small-sized temperature sensors10.1063/1.3093680 ↗
42. Micromachined thermal flow sensors – a review10.3390/mi3030550 ↗