journal article·2014-02

Room temperature ferromagnetism in Cd1−xCrxTe diluted magnetic semiconductor crystals

M. Rigana Begam, N. Madhusudhana Rao, S. Kaleemulla, N. Sai Krishna, M. Kuppan, G. Krishnaiah, J. Subrahmanyam

Publisher page

Abstract

Abstract Cd1−xCrxTe diluted magnetic semiconductor crystals were grown by vapor phase growth technique in the composition range of 0≤x≤0.05 and the effect of Cr doping on structural, morphological, optical and magnetic properties have been explored. X-ray diffraction analysis confirmed that all the grown crystals were zinc blende in structure without having any phase transition up to a Cr doping level of x=0.05. The lattice parameter decreased with increase in Cr doping level. Optical studies indicated that the optical band gap of the crystals decreased with the increase of Cr doping level. Magnetic properties were studied using vibrating sample magnetometer at room temperature and room temperature ferromagnetism was observed in all the Cr doped CdTe crystals.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: ZnO doping and properties · Advanced Semiconductor Detectors and Materials · Semiconductor Quantum Structures and Devices

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (22)

Show source-provided references
1. Ohno · Science · 1998 · 281 · 95110.1126/science.281.5379.951 ↗
2. Haury · Phys. Rev. Lett. · 1997 · 79 · 51110.1103/PhysRevLett.79.511 ↗
3. Ohno · J. Appl. Phys. · 1991 · 69 · 610310.1063/1.347780 ↗
4. Furdyna · J. Appl. Phys. · 1988 · 64 · 2910.1063/1.341700 ↗
5. Furdyna · J. Appl. Phys. · 1982 · 53 · 763710.1063/1.330137 ↗
6. Imamura · J. Appl. Phys. · 2006 · 99 · 70610.1063/1.2176181 ↗
7. Ando · J. Appl. Phys. · 2001 · 78 · 2700
8. Guo · Solid State Commun. · 2006 · 138 · 27510.1016/j.ssc.2006.03.019 ↗
9. Noor · J. Phys. Chem. Solids · 2011 · 72 · 83610.1016/j.jpcs.2011.04.008 ↗
10. Ko · Appl. Phys. Lett. · 2006 · 88 · 17210110.1063/1.2197940 ↗
11. Chandrasekharam · J. Cryst. Growth · 1983 · 63 · 30410.1016/0022-0248(83)90220-8 ↗
12. Subrahmanyam · J. Non-Cryst. Solids · 2011 · 357 · 140510.1016/j.jnoncrysol.2010.11.021 ↗
13. Singh · Thin Solid Films · 2010 · 519 · 107810.1016/j.tsf.2010.08.047 ↗
14. Mac · Phys. Rev. B · 1994 · 50 · 1414410.1103/PhysRevB.50.14144 ↗
15. Philip · Nat. Mater. · 2006 · 5 · 29810.1038/nmat1613 ↗
16. Krishnaiah · Phys. Lett. A · 2008 · 372 · 642910.1016/j.physleta.2008.08.039 ↗
17. Soundararajana · J. Alloys Compd. · 2011 · 509 · 8010.1016/j.jallcom.2010.08.103 ↗
18. Sato · J. Appl. Phys. · 1993 · 73 · 92610.1063/1.353305 ↗
19. Cardona · Phys. Rev. · 1963 · 131 · 9810.1103/PhysRev.131.98 ↗
20. Enloe · J. Appl. Phys. · 1987 · 61 · 200510.1063/1.337996 ↗
21. Chadi · Phys. Rev. B · 1972 · 5 · 305810.1103/PhysRevB.5.3058 ↗
22. Lines · 1977