Mechanical strength problem of thin silicon wafers (120 and 140 μ m ) cut with thinner diamond wires (Si kerf 120 → 100 μ m ) for photovoltaic use
Source abstract
Abstract
We compared the mechanical strength of as-sawn thin silicon wafers (120 and 140 μm) cut by thinner diamond wires (Si kerf 120 → 100 μm). The fracture strength was evaluated by applying uniaxial mechanical loads on the fresh- and worn-wire sides of the wafers. The loads were applied parallel and perpendicular to the direction of the wire saw marks. Under parallel loading, wafers from both the fresh- and worn-wire sides had approximately the same low fracture strength, whereas under perpendicular loading, wafers from the fresh-wire side had a larger strength distribution compared to that of wafers from the worn-wire side. Observation by laser microscope revealed deeper pits in the lower strength wafers compared to the higher strength wafers. Observation by ion milling and subsequent scanning electron microscope revealed several cracks below the deeper pits whereas few cracks appeared below the shallower pits. Since the cracks were thought to be the deciding factor in the wafer fracture, we conducted a fractographic study on the fractured surfaces from the perspective of crack propagation. We found that the mechanical strength of the wafers cut by thinner wires showed a larger strength distribution. Although this variation was probably caused by the motion of the thin wire during the sawing process, further study is required for confirmation.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Silicon and Solar Cell Technologies · Nanowire Synthesis and Applications · Integrated Circuits and Semiconductor Failure Analysis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (50)
Show source-provided references
1. 2018
2. A cost roadmap for silicon heterojunction solar cells10.1016/j.solmat.2015.12.026 ↗
3. Review of status developments of high-efficiency crystalline silicon solar cells10.1088/1361-6463/aaac6d ↗
4. Detailed balance limit of efficiency of p-n junction solar cells10.1063/1.1736034 ↗
5. Silicon heterojunction solar cell with interdigitated back contacts for a photoconversion efficiency over 26%10.1038/nenergy.2017.32 ↗
6. Raising the one-sun conversion efficiency of III–V/Si solar cells to 32.8% for two junctions and 35.9% for three junctions10.1038/nenergy.2017.144 ↗
7. Fully textured monolithic perovskite/silicon tandem solar cells with 25.2% power conversion efficiency10.1038/s41563-018-0115-4 ↗
8. Impact of silicon quantum dot super lattice and quantum well structure as intermediate layer on p-i-n silicon solar cells10.1002/pip.2726 ↗
9. Epitaxial growth of high quality n-type silicon foils in a quasi-inline APCVD reactor10.1016/j.egypro.2015.07.088 ↗
10. The impact of subsurface damage on the fracture strength of diamond-wire-sawn monocrystalline silicon wafers
11. The impact of saw mark direction on the fracture strength of thin (120 μm) monocrystalline silicon wafers for photovoltaic cells
12. The impact of damage etching on fracture strength of diamond wire sawn monocrystalline silicon wafers for photovoltaics use10.7567/JJAP.57.126501 ↗
13. Mechanisms of material removal and subsurface damage in fixed-abrasive diamond wire slicing of single-crystalline silicon10.1016/j.precisioneng.2017.04.011 ↗
14. New potential for reduction of kerf loss and wire consumption in multi-wire sawing10.1016/j.solmat.2014.12.020 ↗
15. Reaching a kerf loss below 100 μm by optimizing the relation between wire thickness and abrasive size for multi-wire sawing
16. Surface layer damage of silicon wafers sliced by wire saw process10.4028/www.scientific.net/AMR.797.685 ↗
17. On the cracks self-healing mechanism at ductile mode cutting of silicon10.1016/j.triboint.2014.07.003 ↗
18. Wire sawing technology: a state-of-the-art review10.1016/j.precisioneng.2015.08.008 ↗
19. Diamond turning of silicon substrates in ductile-regime10.1016/S0924-0136(97)00210-0 ↗
20. Physics of loose abrasive micro grinding10.1364/AO.30.002761 ↗
21. A novel approach of high speed scratching on silicon wafers at nanoscale depths of cut10.1038/srep16395 ↗
22. Effects of mirror polishing brick surface on process yield of multi-wire slicing for thin single-crystalline silicon solar cells10.1016/j.solener.2015.10.022 ↗
23. Raman micro spectroscopy analysis of pressure-induced metallization in scratching of silicon10.1088/0268-1242/16/5/311 ↗
24. Suppressing scratch induced brittle fracture in silicon by geometric design modification of the abrasive grits10.1016/j.jmrt.2018.05.016 ↗
25. Ductile mode behavior of silicon during scribing by spherical abrasive particles10.1016/j.procir.2016.02.341 ↗
26. Study of ductile-to-brittle transition in single grit diamond scribing of silicon: application to wire sawing of silicon wafers10.1115/1.4006177 ↗
27. Effect of grit shape and crystal structure on damage in diamond wire scribing of silicon10.1111/jace.14732 ↗
28. The impact of silicon brick polishing on thin (120 μm) silicon wafer sawing yields and fracture strengths in diamond-wire sawing10.1016/j.mssp.2019.104751 ↗
29. Comparative analysis of mechanical strength of diamond-sawn silicon wafers depending on saw mark orientation, crystalline nature and thickness
30. On the residual stress and fracture strength of crystalline silicon wafers
31. Endless diamond wire saw for monocrystalline silicon cutting
32. Mechanical strength of silicon solar wafers characterized by ring-on-ring test in combination with digital image correlation
33. Damage evaluation of wet chemical Si-wafer thinning/backside via exposure process10.1109/TCPMT.2014.2304462 ↗
34. Klute · 2014 · 753
35. DIN SPEC 91351 Strength Testing for Photovoltaic Wafers.
36. Measurement of residual stress field anisotropy at indentations in silicon10.1016/j.scriptamat.2010.05.017 ↗
37. Anisotropy effects on the reliability of single-crystal silicon10.1016/j.scriptamat.2010.07.024 ↗
38. Aspects of rapid crack propagation in silicon10.1111/j.1460-2695.2006.01054.x ↗
39. Dislocations deflect and perturb dynamically propagating cracks10.1103/PhysRevLett.93.265501 ↗
40. Energy considerations in crack deflection phenomenon in single crystal silicon10.1007/s10704-006-0048-9 ↗
41. From crack defection to lattice vibrations - macro to atomistic examination of dynamic cleavage fracture10.1016/j.jmps.2004.02.004 ↗
42. Hackle or textured mirror? Analysis of surface perturbation in single crystal silicon
43. Fractography of dynamic crack propagation in silicon crystal10.4028/www.scientific.net/KEM.409.55 ↗
44. The impact of surface finish conditions of silicon bricks on the mechanical strength of diamond-wire-sawn thin wafers (120 μm)10.1063/1.5123902 ↗
45. Velocity correlated crack front and surface marks in single crystalline silicon10.1038/s41467-018-03642-w ↗
46. Crack plane deflection and shear wave effects in the dynamic fracture of silicon single crystal10.1016/j.jmps.2018.09.031 ↗
47. T. Ono, R.A. Allaire, Fracture Analysis, a Basic Tool to Solve Breakage Issues. Corning Display Technology.
48. G.D. Quinn, A NIST Recommended Practice Guide; Special Publication 960–16; National Institute of Standards and Technology; Washington, DC: [May 2007]. Fractography of Ceramics and Glasses.
49. Wallner lines, crack velocity and mechanisms of crack nucleation and growth in a brittle bulk metallic glass10.1016/j.actamat.2014.07.024 ↗
50. Experimental analysis of river patterns in silicon brittle fractures10.1051/jp1:1995159 ↗