Negative-bias-temperature-instability in metal–insulator–semiconductor structures

S.N. Volkos, A.R. Peaker, I.D. Hawkins, E. Efthimiou, G. Petkos

Materials Science and Engineering: B· Volume 109· Issue 1-3
Publisher page

Abstract

We have demonstrated that negative-bias-temperature-instability (NBTI) significantly decreases the minority carrier generation lifetime as well as modifying the dominant source supplying minority carriers to the inversion layer at the semiconductor-insulator interface. This was manifested by an NBTI-induced shift in the deep-level-transient-spectroscopy (DLTS) peak signal associated with the inversion layer formation at the semiconductor-insulator interface at temperatures above room temperature to a lower temperature. In addition, we have observed that the DLTS inversion layer-related peak signal gradually shifted back, close to its pre-NBTI temperature position after a substantial time at zero bias-voltage and room temperature conditions had elapsed since the NBTI experiment. We have tentatively ascribed this recovery to a post-NBTI reaction at the semiconductor-insulator interface between unpassivated positively charged silicon dangling bonds and negatively charged hydrogen ions.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Semiconductor materials and devices · Advanced Memory and Neural Computing · Integrated Circuits and Semiconductor Failure Analysis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (12)

Show source-provided references
1. Jeppson · J. Appl. Phys. · 1977 · 48 · 200410.1063/1.323909 ↗
2. Blat · J. Appl. Phys. · 1991 · 69 · 171210.1063/1.347217 ↗
3. Ogawa · Phys. Rev. B · 1995 · 51 · 421810.1103/PhysRevB.51.4218 ↗
4. Yamamoto · IEEE Trans. Electr. Dev. · 1999 · 46 · 92110.1109/16.760398 ↗
5. Liu · Jpn. J. Appl. Phys. · 2002 · 41 · 242310.1143/JJAP.41.2423 ↗
6. V. Huard, F. Monsieur, C.R. Parthasarathy, S. Bruyere, Proc. IRW Fin. Rep. (2002) 135.
7. S. Mahapatra, M.A. Alam, Proc. IEDM Tech. Dig. (2002) 505.
8. A. Toriumi, Proc. PPID (2002) 4.
9. Pearce · J. Appl. Phys. · 1987 · 62 · 57610.1063/1.339785 ↗
10. Zhu · Phys. Rev. B · 1990 · 41 · 1235410.1103/PhysRevB.41.12354 ↗
11. Johnson · Phys. Rev. B · 1992 · 46 · 1555410.1103/PhysRevB.46.15554 ↗
12. Herring · Phys. Rev. B · 2001 · 64 · 12520910.1103/PhysRevB.64.125209 ↗