Abstract
Abstract Lead zirconate titanate thin films by a sol–gel method are deposited on platinum coated silicon wafer for pyroelectric application. Annealing temperature is varied between 560 and 700 °C in order to optimize the detectivity figure of merit F d = p /[ c ( e r e 0 tan δ ) 1/2 ] (where p is pyroelectric coefficient, c is volume specific heat, e r is the relative dielectric constant, e 0 is dielectric constant of free space and tan δ is the dielectric loss tangent). Only perovskite crystalline structure are observed in all the films annealed in this temperature range. It is found that higher annealing temperature is beneficial for better pyroelectric property. The measured pyroelectric coefficient is increased from 220 μC m −2 K −1 at 560 °C annealing temperature to 300 μC m −2 K −1 at 700 °C annealing temperature. But dielectric constant is also found to increase with annealing temperature from 310 at 560 °C to 560 at 700 °C, which impairs the value of detectivity figure of merit. Another important parameter is dielectric loss tangent, which is found to decrease with annealing temperature from 0.025 at 560 °C to 0.011 at 700 °C. The calculated detectivity figure of merit increases with increasing annealing temperature from 560 to 640 °C and decreases with further increasing annealing temperature. The optimized annealing temperature is determined to be 640 °C, and the detectivity figure of merit is 16.6×10 −6 Pa −1/2 .
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Ferroelectric and Piezoelectric Materials · Dielectric properties of ceramics · Microwave Dielectric Ceramics Synthesis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (10)
Show source-provided references
1. Whatmore · Rep. Prog. Phys. · 1986 · 49 · 133510.1088/0034-4885/49/12/002 ↗
2. Lang · Ferroelectrics Rev. · 2000 · 2 · 217
3. Shorrocks · Microelectronic Eng. · 1995 · 29 · 5910.1016/0167-9317(95)00115-8 ↗
4. Impey · J. Appl. Phys. · 1998 · 83 · 220210.1063/1.366957 ↗
5. Song · Appl. Phys. Lett. · 1998 · 72 · 268610.1063/1.121099 ↗
6. Huang · J. Appl. Phys. · 1999 · 85 · 735510.1063/1.369362 ↗
7. W.G. Liu, L.L. Sun, W. Zhu, O.K. Tan, Integrated Ferroelectrics, (in press).
8. Liu · Thin Solid Films · 2000 · 371 · 25410.1016/S0040-6090(00)01012-9 ↗
9. Al-Shareef · Ferroelectrics · 1994 · 152 · 8510.1080/00150199408017601 ↗
10. L.L. Sun, O.K. Tan, W.G. Liu, W. Zhu, Infrared Physics and Technology, (in press).