journal article·2001-01

Dielectric and ferroelectric properties of phosphoric acid doped triglycine sulfate single crystals

Aparna Saxena, Vinay Gupta, K. Sreenivas

Publisher page

Abstract

Abstract Single crystals of triglycine sulfate (TGS) grown with 25–50 mol% phosphoric acid dopant in solution were investigated for their dielectric, ferroelectric and mechanical hardness properties. A 25 mol% of H 3 PO 4 in solution yielded crystals with a large area in the ac plane without any seed crystal. The room temperature (300 K) dielectric constant (e′) and tan δ in the frequency range 0.1–100 kHz were found to increase with increasing phosphoric acid concentration. A maximum shift of 2.5 K in the phase transition temperature ( T c ) is observed for crystals grown with 50 mol% of H 3 PO 4 . Systematic lowering of Curie–Weiss constant ( C f ) in ferroelectric phase and an increase in the paraelectric phase ( C p ) indicates domain wall clamping effects in the doped samples. The changes in the spontaneous polarization (2.6–3.2 μC cm −2 ) with phosphoric acid doping are insignificant, but the high coercive fields ( E c =5 kV cm −1 ), and distorted loops indicate the presence of stresses and inhomogeneities. The activation energy (Δ E ) from temperature dependent d.c. conductivity measurements is lower in both the ferroelectric and the paraelectric phase for doped crystals indicating a strong influence of dopants on the conduction process. The microhardness of the doped crystals is lower in comparison to undoped TGS.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Crystallization and Solubility Studies · Nonlinear Optical Materials Research · Solid-state spectroscopy and crystallography

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (24)

Show source-provided references
1. Lal · Ferroelectrics · 1993 · 142 · 5110.1080/00150199308237884 ↗
2. Lock · Appl. Phys. Letts. · 1970 · 19 · 39010.1063/1.1653742 ↗
3. Gaffar · Indian J. Pure Appl. Phys. · 1988 · 26 · 28
4. Gaffar · J. Phys. D: Appl. Phys. · 1989 · 22 · 32710.1088/0022-3727/22/2/016 ↗
5. Bhalla · Ferroelectrics · 1984 · 54 · 15110.1080/00150198408215838 ↗
6. Ravi · J. Crys. Growth · 1993 · 133 · 21210.1016/0022-0248(93)90157-R ↗
7. Nakatani · Jpn. J. Appl. Phys. · 1996 · 35 · L50810.1143/JJAP.35.L508 ↗
8. Kim · Ferroelectrics · 1993 · 146 · 9910.1080/00150199308008530 ↗
9. Nakatani · Jpn. J. Appl. Phys. · 1997 · 36 · L42510.1143/JJAP.36.L425 ↗
10. Nakatani · Jpn. J. Appl. Phys. · 1996 · 35 · 575210.1143/JJAP.35.5752 ↗
11. Newmann · Ferroelectrics · 1993 · 142 · 85
12. Porter · Ferroelectrics · 1981 · 33 · 19310.1080/00150198108008086 ↗
13. Fang · Ferroelectrics · 1983 · 51 · 910.1080/00150198308009046 ↗
14. Selvarajan · J. Mater. Sci. Letts. · 1992 · 11 · 131210.1007/BF00742188 ↗
15. Glass · 1977
16. Jona · 1962
17. Hoshino · Phys. Rev. · 1957 · 107 · 125510.1103/PhysRev.107.1255 ↗
18. Dacko · Phys. Letts. · 1996 · A223 · 21710.1016/S0375-9601(96)00698-6 ↗
19. Zheludev · 1971 · 2
20. Fang · Ferroelectrics · 1993 · 142 · 9310.1080/00150199308237886 ↗
21. Toyoda · Rev. Electron. Comm. Lab. · 1961 · 9 · 485
22. Mathur · J. Phys. D: Appl. Phys. · 1980 · 13 · 7910.1088/0022-3727/13/1/018 ↗
23. Martin · Ferroelectrics · 1984 · 55 · 26110.1080/00150198408015383 ↗
24. Ravi · Mater. Chem. Phys. · 1993 · 37 · 18010.1016/0254-0584(94)90090-6 ↗