Thermal Conductivity and Combustion Properties of Wheat Gluten Foams
Source abstract
Abstract
Freeze-dried wheat gluten foams were evaluated with respect to their thermal and fire-retardant properties, which are important for insulation applications. The thermal properties were assessed by differential scanning calorimetry, the laser flash method and a hot plate method. The unplasticised foam showed a similar specific heat capacity, a lower thermal diffusivity and a slightly higher thermal conductivity than conventional rigid polystyrene and polyurethane insulation foams. Interestingly, the thermal conductivity was similar to that of closed cell polyethylene and glass-wool insulation materials. Cone calorimetry showed that, compared to a polyurethane foam, both unplasticised and glycerol-plasticised foams had a significantly longer time to ignition, a lower effective heat of combustion and a higher char content. Overall, the unplasticised foam showed better fire-proof properties than the plasticized foam. The UL 94 test revealed that the unplasticised foam did not drip (form droplets of low viscous material) and, although the burning times varied, self-extinguished after flame removal. To conclude both the insulation and fire-retardant properties were very promising for the wheat gluten foam.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Flame retardant materials and properties · Fire dynamics and safety research · Polymer Foaming and Composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Department of Fibre and Polymer Technology, KTH Royal Institute of Technology, SE-10044, Stockholm, Sweden
Risø National Laboratory for Sustainable Energy, Technical University of Denmark, DK-4000 Roskilde, Denmark
Department of Agrosystems, The Swedish University of Agricultural Sciences, SE-23053, Alnarp, Sweden
References (38)
Show source-provided references
1. Gibson L. J. · 1988
2. Alvarez-Lainez M. · J. Polym. Sci. · 2008 · 46 · 21210.1002/polb.21358 ↗
3. Almanza O. · Polym. Int. · 2004 · 53 · 203810.1002/pi.1624 ↗
4. De Carvalho G. · Polym-Plast. Technol. · 2003 · 44 · 60510.1081/PPT-120023098 ↗
5. Gautam R. · Appl. Biochem. Biotechnol. · 2007 · 141 · 8510.1007/s12010-007-9212-6 ↗
6. Chao C. Y. H. · J. Fire Sci. · 2001 · 19 · 13710.1106/Q56W-KUDB-0VRT-6HLF ↗
7. Ahrens, M.,Home Fires That Began with Upholstered Furniture.National Fire Protection Association:Quincy, 2008; p68.
8. Blomfeldt T. O. J. · Macromol. Mater. Eng. · 2010 · 295 · 79610.1002/mame.201000049 ↗
9. Blomfeldt T. O. J. · Biomacromolecules · 2011 · 12 · 170710.1021/bm200067f ↗
10. Olabarrieta I. · Biomacromolecules · 2006 · 7 · 165710.1021/bm0600973 ↗
11. Ullsten H. N. · Biomacromolecules · 2006 · 7 · 77110.1021/bm050822u ↗
12. Gällstedt M. · Biomacromolecules · 2004 · 5 · 202010.1021/bm040044q ↗
13. Min S. · Thermochim. Acta · 2007 · 455 · 4610.1016/j.tca.2006.11.026 ↗
14. 2002
15. Lim H. · Express. Polym. Lett. · 2008 · 2 · 19410.3144/expresspolymlett.2008.24 ↗
16. www.isover.com
17. Yang C. G. · Energy Convers. Manage. · 2006 · 47 · 112410.1016/j.enconman.2005.07.006 ↗
18. Rudtsch S. · Int. J. Thermophys. · 2004 · 25 · 147510.1007/s10765-004-5752-y ↗
19. Al-Ajlan S A. · Appl. Therm. Eng. · 2006 · 26 · 218410.1016/j.applthermaleng.2006.04.006 ↗
20. Lim K.-H. · Thermochim. Acta · 2009 · 494 · 7110.1016/j.tca.2009.04.019 ↗
21. Prociak A. · Polym. Test. · 2000 · 19 · 70510.1016/S0142-9418(99)00042-2 ↗
22. dos Santos W. N. · Polym. Test. · 2005 · 24 · 62810.1016/j.polymertesting.2005.03.007 ↗
23. Gawryla M. D. · Green Chem. · 2008 · 10 · 107810.1039/b807473a ↗
24. Assael M. J. · Int. J. Thermophys · 2005 · 26 · 159510.1007/s10765-005-8106-5 ↗
25. Verbeek C. J. R. · Macromol. Mater. Eng. · 2010 · 295 · 1010.1002/mame.200900167 ↗
26. Swain S. N. · J. Appl. Polym. Sci. · 2004 · 93 · 259010.1002/app.20729 ↗
27. Janssens M. L. · Fire Technol. · 1991 · 27 · 23410.1007/BF01038449 ↗
28. Babrauskas V. · 2003
29. Karlsson B. A. · Fire Safety J. · 1993 · 20 · 9310.1016/0379-7112(93)90032-L ↗
30. Grant G. · Fire Safety J. · 1995 · 24 · 24710.1016/0379-7112(95)00022-L ↗
31. Kuang-Chung T. · Fire Safety J · 2002 · 37 · 69710.1016/S0379-7112(02)00024-3 ↗
32. Schartel B. · Fire Mater. · 2007 · 31 · 32710.1002/fam.949 ↗
33. Zhang J. · Fire Mater. · 1997 · 21 · 110.1002/(SICI)1099-1018(199701)21:1<1::AID-FAM583>3.0.CO;2-P ↗
34. Price D. · Polym. Int. · 2000 · 49 · 115310.1002/1097-0126(200010)49:10<1153::AID-PI551>3.0.CO;2-S ↗
35. Krämer R. H. · Polym. Degrad stabil. · 2010 · 95 · 111510.1016/j.polymdegradstab.2010.02.019 ↗
36. Ohlemiller T. J. · 2008
37. Checchin M. · Polym. Degrad. Sabil. · 1999 · 64 · 57310.1016/S0141-3910(98)00131-1 ↗
38. Mathias J.-D. · Int. J. Mol. Sci. · 2011 · 12 · 117510.3390/ijms12021175 ↗