Abstract
Hydrothermal synthesis has proven to be a cost-effective, energy-efficient approach for the manufacture of lithium iron phosphate (LiFePO₄) and its related materials. However, hydrothermally prepared LiFePO₄ typically suffers from antisite defects, where some of the iron resides on lithium sites and restricts lithium-ion mobility. A post-heat-treatment temperature of around 700 °C is generally used to eliminate cation disorder, but little is known about these antisite defects or their concentration as a function of the post-heat-treatment temperature. In this study, time-resolved, synchrotron X-ray diffraction reveals that antisite defects are completely eliminated above 500 °C, suggesting that the electrochemical performance may be significantly enhanced by a milder postsynthesis heat treatment. The preliminary electrochemical results show a significant enhancement in the electrochemical capacity with the defect-free material, with the specific capacity increasing by approximately 60% at a C/20 rate.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Advancements in Battery Materials · Extraction and Separation Processes · Advanced Battery Materials and Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Energy Science and Technology Department, Brookhaven National Laboratory, Upton, New York 11973, United States
References (19)
Show source-provided references
1. Padhi A. K. · J. Electrochem. Soc. · 1997 · 144 · 118810.1149/1.1837571 ↗
2. Chen J. J. · Solid State Ionics · 2008 · 178 · 167610.1016/j.ssi.2007.10.015 ↗
3. Whittingham M. S. · Chem. Rev. · 2004 · 104 · 427110.1021/cr020731c ↗
4. Lu Z. H. · J. Electrochem. Soc. · 2002 · 149 · A77810.1149/1.1471541 ↗
5. Morgan D. · Electrochem. Solid-State Lett. · 2004 · 7 · A3010.1149/1.1633511 ↗
6. Yang S. F. · Electrochem. Commun. · 2001 · 3 · 50510.1016/S1388-2481(01)00200-4 ↗
7. Yang S. F. · J. Power Sources · 2003 · 119 · 23910.1016/S0378-7753(03)00240-4 ↗
8. Chen J. J. · Electrochem. Commun. · 2006 · 8 · 85510.1016/j.elecom.2006.03.021 ↗
9. Islam M. S. · Chem. Mater. · 2005 · 17 · 508510.1021/cm050999v ↗
10. Liu J. L. · J. Power Sources · 2009 · 194 · 53610.1016/j.jpowsour.2009.05.007 ↗
11. Fang H. S. · Electrochem. Commun. · 2008 · 10 · 107110.1016/j.elecom.2008.05.010 ↗
12. Shiraishi K. · J. Power Sources · 2005 · 146 · 55510.1016/j.jpowsour.2005.03.060 ↗
13. Dokko K. · J. Electrochem. Soc. · 2005 · 152 · A219910.1149/1.2051987 ↗
14. Jozwiak P. · J. Non-Cryst. Solids · 2008 · 354 · 191510.1016/j.jnoncrysol.2007.10.032 ↗
15. Chen J. · J. Power Sources · 2007 · 174 · 44210.1016/j.jpowsour.2007.06.189 ↗
16. Streltsov V. A. · Acta Crystallogr., Sect. B · 1993 · 49 · 14710.1107/S0108768192004701 ↗
17. Axmann P. · Chem. Mater. · 2009 · 21 · 163610.1021/cm803408y ↗
18. Nishimura S. · Nat. Mater. · 2008 · 7 · 70710.1038/nmat2251 ↗
19. Yang S. F. · Electrochem. Commun. · 2002 · 4 · 23910.1016/S1388-2481(01)00298-3 ↗