Improving corrosion resistance of Kovar by subjection to a coupled electromagnetic treatment
Source abstract
Abstract
As a common electronic packaging device, Kovar primarily serves to secure, seal, and protect semiconductor chips. The Ni–Au coating applied to its surface effectively resists external corrosion. However, residual stress and defects generated during the electroplating process of the Ni–Au layer often diminish the corrosion resistance of the coating. This study employs a coupled electromagnetic treatment (CEMT) to regulate the Ni–Au coating after electroplating, with the aim of improving their corrosion resistance. The results indicate that the corrosion resistance of the Ni–Au coating was effectively improved after CEMT, and the product qualification rate is 95 %. The residual tensile stress was greatly reduced, the residual tensile stress in the X direction was reduced by 44.84 %, and in the Y direction was reduced by 61.75 %. The nanohardness increased from 0.74 GPa to 0.91 GPa, an increase of 22.97 %. Microstructure analysis showed that the dislocation density of the coating after CEMT was reduced by about 4.2 %, and the dislocation distribution was more uniform. The reduction of stress and the repair of defects provide an important basis for improving the corrosion resistance of the coating.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Electromagnetic Effects on Materials · Magnetic and Electromagnetic Effects · Surface Treatment and Coatings
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (37)
Show source-provided references
1. Wetting and spreading behavior of borosilicate glass on kovar10.1016/j.jallcom.2008.10.028 ↗
2. Wetting and sealing of interface between 7056 glass and kovar alloy10.1016/j.matchemphys.2007.04.012 ↗
3. The shear strength and fracture behavior of sn-ag-xsb solder joints with au/ni-p/cu ubm10.1007/s11664-008-0396-5 ↗
4. Liquid-state and solid-state interfacial reactions of fluxless-bonded au–20sn/enig solder joint10.1016/j.jallcom.2008.01.077 ↗
5. Improving the mechanical performance of sn57.6bi0.4ag solder joints on au/ni/cu pads during aging and electromigration through the addition of tungsten (w) nanoparticle reinforcement10.1016/j.msea.2016.05.092 ↗
6. Intermetallic reactions in reflowed and aged sn-9zn solder ball grid array packages with au/ni/cu and Ag/Cu pads10.1007/s11664-006-0198-6 ↗
7. Interfacial reaction and shear strength of pb-free snag2.5cu0.8sb0.5 and snag3.0cu0.5sb0.2 solder bumps on au/ni(p) metallization10.1016/j.jallcom.2005.06.087 ↗
8. Corrosion behavior of ni-w coatings with and without macroscopic defects under different corrosion conditions
9. Stress measurements in nanocrystalline ni electrodeposits10.1016/j.jallcom.2004.08.010 ↗
10. Unraveling the effects of co2 and h2s on the corrosion behavior of electroless ni-p coating in co2/h2s/cl– environments at high temperature and high pressure10.1016/j.corsci.2018.12.022 ↗
11. Effect of defect on corrosion behavior of electroless ni-p coating in co2-saturated nacl solution10.1016/j.corsci.2018.01.041 ↗
12. The effect of microstructure for ni-based surface finishing thin film on corrosion behavior10.1016/j.surfcoat.2023.129252 ↗
13. Graded composition and structure in nanocrystalline ni–co alloys for decreasing internal stress and improving tribological properties10.1088/0022-3727/38/8/033 ↗
14. Mechanisms inducing compressive stress during electrodeposition of ni10.1063/1.1819972 ↗
15. Improved corrosion resistance through microstructural modifications induced by codepositing sic-particles with electrolytic nickel10.1016/S0010-938X(02)00220-2 ↗
16. Interface behaviour in nickel composite coatings with nano-particles of oxidic ceramic10.1016/S0013-4686(03)00380-3 ↗
17. Hydrogen desorption and internal stress in nickel coatings obtained by periodic electrodeposition10.1149/1.2069098 ↗
18. Influence of lower current densities on the residual stress and structure of thick nickel electrodeposits10.1016/j.surfcoat.2011.01.012 ↗
19. The relationship between nano crystallite structure and internal stress in ni coatings electrodeposited by watts bath electrolyte mixed with supercritical co210.1149/2.061206jes ↗
20. Correlation between structure and corrosion behaviour of nickel dispersion coatings containing ceramic particles of different sizes10.1016/j.surfcoat.2006.08.073 ↗
21. Residual stresses and texture in ni/sic nanocomposite coatings10.1016/j.jallcom.2006.08.285 ↗
22. Elastic grain interaction in electrodeposited nanocomposite nickel matrix coatings10.1016/j.surfcoat.2011.10.056 ↗
23. Characteristics of electro-co-deposited ni–al2o3 nano-particle reinforced metal matrix composite (mmc) coatings
24. Microstructure of nanometer al2o3 particles reinforced aluminum matrix composites processed by high pulsed electromagnetic field10.1016/j.matlet.2013.02.089 ↗
25. The microstructure and property variations of metals induced by electric current treatment: a review10.1016/j.matchar.2018.08.058 ↗
26. An investigation on the mechanical property changing mechanism of high speed steel by pulsed magnetic treatment10.1016/j.msea.2014.04.100 ↗
27. Residual stress relaxation of 2a02 blade forging under electromagnetic coupling energy
28. Improvement of the fatigue life of an electron-beam welded ti2alnb joint subjected to an electromagnetic coupling treatment10.1016/j.msea.2024.146848 ↗
29. Effect of electromagnetic coupling treatment on the residual stress relief and mechanical properties of 7050 aluminum alloy10.1007/s10853-023-08775-y ↗
30. An investigation into different nickel and nickel–phosphorus stacked thin coatings for the corrosion protection of electrical contacts10.1016/j.surfcoat.2016.05.013 ↗
31. Improving thermal conductivity of a nickel-based alloy through advanced electromagnetic coupling treatment10.1016/j.jmrt.2022.11.066 ↗
32. An electromagnetic coupling treatment for improving the cutting performance of cemented carbide-coated tools, Asian
33. Magnetoplastic effect: basic properties and physical mechanisms10.1134/1.1612598 ↗
34. Mechanochemical reactions between structural defects in magnetic fields10.1023/B:JMSC.0000039196.60100.74 ↗
35. Dislocation structure evolution under electroplastic effect10.1016/j.msea.2019.138026 ↗
36. Technique for producing crack arrest by electromagnetic heating10.1179/026708301101509737 ↗
37. Microstructure characterization and thermal behavior around crack tip under electropulsing10.1007/s00339-015-9383-x ↗