Effect of SnO2 concentration on the dielectric properties of BaTiO3–(Sr1−1.5xBix)TiO3 ceramics
Source abstract
Abstract
Abstract SnO 2 -doped 0.45BaTiO 3 –0.55(Sr 1−1.5 x Bi x )TiO 3 (BT–SBT) ceramics were prepared by the conventional solid state reaction method. The effect of SnO 2 concentration on the microstructures and dielectric properties has been investigated. XRD results indicate all the specimens have a perovskite structure without any secondary phases. With increasing SnO 2 concentration, the maximum dielectric constant decreases with slight shift in Curie temperature and the peak in temperature spectra becomes much broader. When the SnO 2 concentration is 1 mol%, the specimen exhibits a more homogeneous microstructure and an improvement of the dielectric breakdown strength compared with the undoped one. Impedance analysis was carried out to investigate the trend in activation energy with the increase of SnO 2 concentration. The correlation between the dielectric breakdown strength and the difference of the activation energies of grain and grain boundary was qualitatively discussed. The accumulation of space charge was found to enhance the dielectric breakdown strength.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Ferroelectric and Piezoelectric Materials · Microwave Dielectric Ceramics Synthesis · Dielectric properties of ceramics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (19)
Show source-provided references
1. Pan · IEEE Electr. Insul. Mag. · 2010 · 26 · 4410.1109/MEI.2010.5482787 ↗
2. Zhi · Mater. Lett. · 2003 · 57 · 292710.1016/S0167-577X(02)01398-8 ↗
3. Jeon · J. Eur. Ceram. Soc. · 2001 · 21 · 165310.1016/S0955-2219(01)00085-1 ↗
4. Zhou · J. Eur. Ceram. Soc. · 2001 · 21 · 53110.1016/S0955-2219(00)00239-9 ↗
5. Cernea · J. Am. Ceram. Soc. · 2007 · 90 · 172810.1111/j.1551-2916.2007.01648.x ↗
6. Fu · J. Electroceram · 2008 · 21 · 56110.1007/s10832-008-9511-5 ↗
7. Baskaran · J. Mater. Sci. – Mater. Electron. · 2001 · 12 · 52710.1023/A:1012453526652 ↗
8. Morrison · J. Am. Ceram. Soc. · 2001 · 84 · 53110.1111/j.1151-2916.2001.tb00694.x ↗
9. Senturk · Solid State Ionics · 2005 · 49 · 935
10. Yoon · J. Am. Ceram. Soc. · 2009 · 92 · 175810.1111/j.1551-2916.2009.03121.x ↗
11. Caballero · J. Am. Ceram. Soc. · 1998 · 81 · 93910.1111/j.1151-2916.1998.tb02430.x ↗
12. Weibull · J. Appl. Mech. · 1951 · 18 · 29310.1115/1.4010337 ↗
13. Kishimoto · J. Mater. Sci. · 1989 · 24 · 69810.1007/BF01107462 ↗
14. Owate · J. Appl. Phys. · 1992 · 72 · 241810.1063/1.351586 ↗
15. Touzin · J. Eur. Ceram. Soc. · 2007 · 27 · 119310.1016/j.jeurceramsoc.2006.05.047 ↗
16. Chen · Appl. Phys. Lett. · 2007 · 90 · 20290310.1063/1.2736298 ↗
17. Sinclar · J. Appl. Phys. · 1989 · 66 · 385010.1063/1.344049 ↗
18. Mahajan · J. Phys. D: Appl. Phys. · 2009 · 42 · 06541310.1088/0022-3727/42/6/065413 ↗
19. Zhou · Jpn. J. Appl. Phys. · 2001 · 40 · 233610.1143/JJAP.40.2336 ↗