High piezoelectric properties above 150 °C in (Bi0.5Na0.5)TiO3-Based lead-free piezoelectric ceramics
Source abstract
Abstract
Abstract (Bi0.5Na0.5)TiO3–BaTiO3 lead-free piezoelectric ceramics exhibit excellent piezoelectric properties, but its piezoelectric property with high thermal stability is the major obstacle limiting the potential application. In this study, the KNbO3 (KN) was adopted to 0.875(Bi0.5Na0.5)TiO3-0.125BaTiO3 (BNT-12.5BT) by conventional solid-state reaction to enhance the piezoelectric properties in high temperature. The results of X-ray diffraction (XRD) indicate that KN has diffused into BNT-12.5BT lattices to form a pure perovskite structure and not exert a severe disturbance on the ferroelectric tetragonal lattice. The depolarization temperature Td is maintained at a high level. For piezoelectric properties, at KN modification x = 0.01, the piezoelectric coefficient (d33) increases to 147 pC/N from 135 pC/N for unmodified composition. Meanwhile, the d33 will increase to 187 pC/N until the depolarization temperature (185 °C) arrives, showing the excellent temperature stability of the piezoelectric properties to meet the actual demand.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Ferroelectric and Piezoelectric Materials · Multiferroics and related materials · Microwave Dielectric Ceramics Synthesis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (29)
Show source-provided references
1. Transferring lead-free piezoelectric ceramics into application10.1016/j.jeurceramsoc.2014.12.013 ↗
2. Composition-induced phase evolution and high strain response in Ba(Zn1/3Nb2/3)O3-modified (Bi0.5Na0.5)TiO3-based lead-free ferroelectrics10.1039/C8RA00653A ↗
3. Average vs. local structure and composition-property phase diagram of K0.5Na0.5NbO3-Bi0.5Na0.5TiO3 system10.1016/j.jeurceramsoc.2016.11.024 ↗
4. Relaxor ferroelectric BaTiO3-Bi(Mg2/3Nb1/3)O3 ceramics for energy storage application10.1111/jace.13325 ↗
5. Giant strain of 0.65% obtained in B-site complex cations (Zn1/3Nb2/3)4+-modified BNT-7BT ceramics10.1016/j.jallcom.2018.12.210 ↗
6. Integrated hybrid life cycle assessment and supply chain environmental profile evaluations of lead-based (lead zirconate titanate) versus lead-free (potassium sodium niobate) piezoelectric ceramics10.1039/C6EE02429G ↗
7. BaTiO3-based piezoelectrics: fundamentals, current status, and perspectives10.1063/1.4990046 ↗
8. Piezoelectric properties in (K0.5Bi0.5)TiO3-(Na0.5Bi0.5)TiO3-BaTiO3 lead-free ceramics10.1109/TUFFC.2007.336 ↗
9. The improved pyroelectric properties, high depolarization temperature and excellent thermal stability in lead-free (1−x)(Bi0.5Na0.5)TiO3-xBa(Ni0.5Nb0.5)O3 ceramics10.1088/2053-1591/aafcd0 ↗
10. Semiconductor/relaxor 0-3 type composites without thermal depolarization in (Bi0.5Na0.5)TiO3-based lead-free piezoceramics10.1038/ncomms7615 ↗
11. Microstructure and suppressed thermal depolarisation behaviours of lead-free Na0.5Bi0.5TiO3:ZnO ferroelectric composite ceramics10.1080/17436753.2017.1374317 ↗
12. Structural stability and depolarization of manganese-doped (Bi0.5Na0.5)1−xBaxTiO3 relaxor ferroelectrics10.1063/1.4898322 ↗
13. Effect of Co2O3 additive on structure and electrical properties of 85(Bi1/2Na1/2)TiO3-12(Bi1/2Na1/2)TiO3-3BaTiO3 lead-free piezoceramics10.1111/j.1551-2916.2009.03183.x ↗
14. Effect of CoO additive on structure and electrical properties of (Na0.5Bi0.5)0.93Ba0.07TiO3 ceramics prepared by the citrate method10.1016/j.actamat.2007.10.014 ↗
15. Effect of KNbO3 addition on diffuse phase transition and dielectric properties of Bi0.5Na0.5TiO3 ceramics10.1080/10584587.2018.1444884 ↗
16. Energy-storage properties of Bi0.5Na0.5TiO3-BaTiO3-KNbO3 ceramics fabricated by wet-chemical method10.1016/j.jeurceramsoc.2016.07.011 ↗
17. Preparation and electrical properties of Bi0.5Na0.5TiO3–BaTiO3–KNbO3 lead-free piezoelectric ceramics10.1016/j.jallcom.2010.12.190 ↗
18. Tuning optical and dielectric properties of calcium copper titanate CaxCu3-xTi4O12 nanopowders10.1039/C4RA15222K ↗
19. Tunable investigation optical, electrical and magnetic behaviors of Gd3+ substituted lanthanum strontium manganite La0.5-x Sr0.5GdxMnO3 nanopowders facilely synthesized through citrate precursor technique10.1016/j.jallcom.2017.11.373 ↗
20. Effects of long- and short-range ferroelectric order on the electrocaloric effect in relaxor ferroelectric ceramics10.1103/PhysRevApplied.11.044032 ↗
21. Enhanced thermal stability, hardening of piezoelectric property, and mediated electromechanical response in (Bi0.5Na0.5)TiO3 -based piezoceramics via composite approach10.1016/j.ceramint.2018.06.145 ↗
22. Scaling behavior of dynamic hysteresis in relaxor ferroelectric 0.67Pb(Mg1/3Nb2/3)O3–0.33PbTiO3 ceramics
23. Giant electrostrain accompanying structural evolution in lead-free NBT-based piezoceramics10.1039/C7TC05359B ↗
24. Enhanced piezoelectric properties and strain response in ⟨001⟩ textured BNT-BKT-BT ceramics10.1016/j.matdes.2017.10.003 ↗
25. Relaxor phase evolution and temperature-insensitive large strain in B-site complex ions modified NBT-based lead-free ceramics10.1007/s10853-017-1517-4 ↗
26. Linear-like lead-free relaxor antiferroelectric (Bi0.5Na0.5)TiO3–NaNbO3 with giant energy-storage density/efficiency and super stability against temperature and frequency10.1039/C8TA12232F ↗
27. Piezoelectric and Ferroelectric Properties of (Bi,Na)TiO3-(Bi,Li)TiO3-(Bi,K)TiO3 ceramics for accelerometer application
28. Ji · 2012
29. Polarization reversal via a transient relaxor state in nonergodic relaxors near freezing temperature10.1016/j.jmat.2019.06.004 ↗