Dielectric properties of nanocrystalline Pb0.8Sr0.2TiO3 thin films at different annealing temperature
Source abstract
Abstract
Nanocrystalline Pb0.8Sr0.2TiO3 (PST20) thin films have been synthesized by metallo-organic decomposition (MOD) technique and deposited on Pt/Ti/SiO2/Si substrates at different annealing temperatures of 550–750 °C. The X-ray diffraction (XRD) confirms the distorted tetragonal perovskite phase in PST20 films. The average grain's size varies from 35 nm to 46 nm as the annealing temperature increases from 650 °C to 750 °C as revealed by atomic force microscopy. At 550 °C, the film shows low crystallization with incomplete perovskite structure. The study of dielectric properties of PST20 films is aimed at electrically tunable applications and to observe ferroelectric behaviors of PST20 films. The film annealed at 650 °C shows large dielectric constant and higher tunability than the films annealed at 550 °C and 750 °C. The values of dielectric constant and tan δ at 1 MHz are 272 and 0.005, respectively, and tunability is ∼66% for PST20 film annealed at 650 °C. The dispersionless dielectric properties are observed up to high frequency ∼8 MHz. The results suggest that the growth of uniform, dense and nano-sized grains in PST film makes it suitable for higher frequency device applications and electrically tunable devices.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Ferroelectric and Piezoelectric Materials · Dielectric properties of ceramics · Multiferroics and related materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (20)
Show source-provided references
1. Matsumoto · Thin Solid Films · 2005 · 476 · 7310.1016/j.tsf.2004.09.017 ↗
2. Wang · Appl. Phys. Lett. · 2004 · 84 · 76510.1063/1.1645331 ↗
3. Wang · Appl. Phys. Lett. · 2007 · 91 · 25290810.1063/1.2827583 ↗
4. Negi · Integr. Ferroelectr. · 2007 · 92 · 9710.1080/10584580701748497 ↗
5. Verma · Appl. Phys. Lett. · 2008 · 92 · 15290210.1063/1.2906359 ↗
6. Liu · Appl. Phys. Lett. · 2006 · 89 · 16312210.1063/1.2364454 ↗
7. Knauss · Appl. Phys. Lett. · 1996 · 69 · 2510.1063/1.118106 ↗
8. Li · Appl. Phys. Lett. · 2007 · 90 · 26290610.1063/1.2752532 ↗
9. Yang · Appl. Phys. Lett. · 2007 · 90 · 24290810.1063/1.2748080 ↗
10. Shao · J. Appl. Phys. · 2006 · 100 · 03610210.1063/1.2218268 ↗
11. Gust · J. Am. Ceram. Soc. · 2001 · 8410.1111/j.1151-2916.2001.tb00794.x ↗
12. Cole · J. Appl. Phys. · 2000 · 93 · 921810.1063/1.1569392 ↗
13. Karaki · Jpn. J. Appl. Phys. Part 1 · 2002 · 41 · 676110.1143/JJAP.41.6761 ↗
14. Chu · Sensors Actuat. A · 2001 · 89 · 21010.1016/S0924-4247(00)00536-7 ↗
15. Pintilie · Phys. Rev. B · 2007 · 75 · 10410310.1103/PhysRevB.75.104103 ↗
16. Cullity · 1967
17. Pontes · Appl. Phys. A · 2005 · 80 · 87510.1007/s00339-003-2335-x ↗
18. Kim · Thin Solid Films · 2004 · 447 · 65110.1016/j.tsf.2003.09.037 ↗
19. Tyunina · Phys. Rev. B · 2001 · 63 · 22410210.1103/PhysRevB.63.224102 ↗
20. Chattopadhyay · Phys. Rev. B · 1995 · 52 · 1317710.1103/PhysRevB.52.13177 ↗