Domain switching of barium titanate ceramics induced by surface grinding
Source abstract
Abstract
As-sintered and subsequently ground barium titanate ceramics have been examined by X-ray diffractometry (XRD), scanning electron microscopy (SEM), and their relative permittivity determined. A compressive residual stress of ∼316 MPa parallel to the surface is found in the near surface region of the ground samples. A ferroelectric domain texture with the polar axis normal to the sample surface is developed due to the compressive residual stress. A depth gradient of this texture is observed by varying the penetration depth of the X-ray beam through sample tilting. Because the stressed zone is only confined to the near surface region, no significant difference in relative permittivity is observed between the as-sintered and the ground samples. Comparing with the as-sintered samples, considerable diffuseness in tetragonal to cubic phase transition is observed from the ground samples by XRD during heating. This implies that internal stresses can also cause diffuse phase transition.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Ferroelectric and Piezoelectric Materials · Advanced ceramic materials synthesis · Metal and Thin Film Mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (32)
Show source-provided references
1. Valot · Ferroelectrics · 1995 · 172 · 23510.1080/00150199508018481 ↗
2. Arlt · J. Mater. Sci. · 1990 · 25 · 265510.1007/BF00584864 ↗
3. Arlt · J. Appl. Phys. · 1985 · 58 · 161910.1063/1.336051 ↗
4. Buessem · J. Am. Ceram. Soc. · 1966 · 49 · 3610.1111/j.1151-2916.1966.tb13145.x ↗
5. Buessem · J. Am. Ceram. Soc. · 1966 · 49 · 3310.1111/j.1151-2916.1966.tb13144.x ↗
6. Bowman · J. Am. Ceram. Soc. · 1991 · 74 · 269010.1111/j.1151-2916.1991.tb06825.x ↗
7. Chan · J. Am. Ceram. Soc. · 1991 · 74 · 80710.1111/j.1151-2916.1991.tb06929.x ↗
8. Srinivasan · J. Am. Ceram. Soc. · 1989 · 72 · 209810.1111/j.1151-2916.1989.tb06038.x ↗
9. Kitano · J. Am. Ceram. Soc. · 1989 · 72 · 85410.1111/j.1151-2916.1989.tb06232.x ↗
10. Kitano · J. Am. Cream. Soc. · 1988 · 71 · c38210.1111/j.1151-2916.1988.tb06399.x ↗
11. Li · J. Am. Ceram. Soc. · 1988 · 71 · c36210.1111/j.1151-2916.1988.tb05943.x ↗
12. Virkar · J. Am. Ceram. Soc. · 1986 · 69 · c22410.1111/j.1151-2916.1986.tb07341.x ↗
13. Cullity · 2001
14. Hu · J. Am. Ceram. Soc. · 1986 · 69 · 59410.1111/j.1151-2916.1986.tb04814.x ↗
15. Chou · Acta Mater. · 2000 · 48 · 356910.1016/S1359-6454(00)00133-6 ↗
16. Mendelson · J. Am. Ceram. Soc. · 1969 · 52 · 44310.1111/j.1151-2916.1969.tb11975.x ↗
17. Lu · J. Am. Ceram. Soc. · 1990 · 73 · 356210.1111/j.1151-2916.1990.tb04258.x ↗
18. Kirby · J. Am. Ceram. Soc. · 1991 · 74 · 184110.1111/j.1151-2916.1991.tb07797.x ↗
19. Noyan · 1987
20. Balart · Mater. Sci. Eng. A · 2004 · 367 · 13210.1016/j.msea.2003.10.239 ↗
21. Guo · Wear · 2004 · 256 · 39310.1016/S0043-1648(03)00443-5 ↗
22. Schuster · Z. Metallkd. · 2003 · 94 · 810.3139/146.030934 ↗
23. Cheng · Int. J. Fatigue · 2003 · 25 · 125910.1016/j.ijfatigue.2003.08.020 ↗
24. Torres · Int. J. Fatigue · 2002 · 24 · 87710.1016/S0142-1123(01)00205-5 ↗
25. Menig · Scripta Mater. · 2001 · 45 · 97710.1016/S1359-6462(01)01063-6 ↗
26. Behnken · Mater. Sci. Eng. A · 2000 · 300 · 4110.1016/S0921-5093(00)01791-3 ↗
27. Österle · Mater. Sci. Eng. A · 1999 · 262 · 30810.1016/S0921-5093(98)01018-1 ↗
28. Wang · J. Mater. Process. Technol. · 1998 · 73 · 6410.1016/S0924-0136(97)00213-6 ↗
29. Immelmann · Mater. Sci. Eng. A · 1997 · 238 · 28710.1016/S0921-5093(97)00080-4 ↗
30. Eigenmann · Nucl. Instrum. Meth. B · 1995 · 97 · 9210.1016/0168-583X(94)00410-2 ↗
31. Cullity · 2001
32. Smolenskii · Ferroelectrics · 1984 · 53 · 29