Mica-Based Multilayer Nanocoating as a Highly Effective Flame Retardant and Smoke Suppressant
Source abstract
Abstract
Highly flammable polyurethane foam (PUF) remains a key risk factor associated with bedding and upholstered furniture, contributing to the yearly destruction of property and loss of lives. In an attempt to tackle this issue and develop a more benign flame retardant for PUF, a mica-based nanocomposite was deposited using layer-by-layer assembly. Chitosan (CH) and poly(acrylic acid) (PAA) were used to stabilize high-aspect-ratio mica. Foam treated with eight bilayers of CH- and PAA-stabilized mica preserves the porous foam structure, prevents melt dripping, and self-extinguishes during a 10 s torch test, while uncoated foam is completely consumed. When exposed to 35 kW/m2 heat flux during cone calorimetry, the peak heat release rate is reduced by 54% and less-volatile molecules are released during combustion, resulting in a 76% reduction in the total smoke release. This multilayer coating serves as an environmentally benign template for flame-retarding PUF and various other three-dimensional substrates.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Flame retardant materials and properties · Fire dynamics and safety research · Polymer composites and self-healing
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Department of Mechanical Engineering, Texas A&M University, 3123 TAMU, College Station, Texas 77843, United States
Department of Chemistry, Texas A&M University, 3255 TAMU, College Station, Texas 77843, United States
Department of Chemical Engineering, Texas A&M University, 3122 TAMU, College Station, Texas 77843, United States
References (28)
Show source-provided references
1. Marketsandmarkets. Polyurethane Foam Market—Global Forecast to 2023. https://www.marketsandmarkets.com/Market-Reports/polyurethane-foams-market-1251.html (accessed January, 2020).
2. Ahrens M. · 2011
3. 10.1038/s41578-019-0164-610.1038/s41578-019-0164-6 ↗
4. Joshi M. · Indian J. Fibre Text. Res. · 2006 · 31 · 202
5. 10.1680/gmat.12.0000210.1680/gmat.12.00002 ↗
6. 10.1038/s41428-017-0015-510.1038/s41428-017-0015-5 ↗
7. 10.1007/s10853-017-1390-110.1007/s10853-017-1390-1 ↗
8. 10.1021/acs.chemrev.6b0062710.1021/acs.chemrev.6b00627 ↗
9. 10.1021/cr400531v10.1021/cr400531v ↗
10. 10.1016/j.polymdegradstab.2018.03.01310.1016/j.polymdegradstab.2018.03.013 ↗
11. 10.1021/am201791510.1021/am2017915 ↗
12. 10.1021/acsami.8b1022710.1021/acsami.8b10227 ↗
13. 10.1039/C4TA03541K10.1039/C4TA03541K ↗
14. 10.1016/j.polymdegradstab.2011.05.01910.1016/j.polymdegradstab.2011.05.019 ↗
15. 10.1016/j.polymdegradstab.2008.11.01910.1016/j.polymdegradstab.2008.11.019 ↗
16. 10.1007/s10973-017-6448-410.1007/s10973-017-6448-4 ↗
17. 10.1021/am301173710.1021/am3011737 ↗
18. 10.1016/j.compscitech.2016.07.00710.1016/j.compscitech.2016.07.007 ↗
19. 10.1021/jp300759n10.1021/jp300759n ↗
20. 10.1021/la802752g10.1021/la802752g ↗
21. 10.1016/S0301-7516(98)00040-410.1016/S0301-7516(98)00040-4 ↗
22. 10.1002/mame.20180053110.1002/mame.201800531 ↗
23. 10.1016/j.polymdegradstab.2015.10.00810.1016/j.polymdegradstab.2015.10.008 ↗
24. 10.1002/adfm.20170328910.1002/adfm.201703289 ↗
25. 10.1021/am504455k10.1021/am504455k ↗
26. 10.1021/la501946f10.1021/la501946f ↗
27. 10.1680/jgrma.17.0002510.1680/jgrma.17.00025 ↗
28. 10.1007/s10853-014-8800-410.1007/s10853-014-8800-4 ↗