Improving the Thermal Stability of NMC 622 Li-Ion Battery Cathodes through Doping During Coprecipitation
Source abstract
Abstract
(NMC) cathodes can increase the capacity, but additional stability is needed to improve safety and longevity characteristics. In order to achieve this improved stability, Mg and Zr were added during the coprecipitation to uniformly dope the final cathode material. These dopants reduced the capacity of the material to some extent, depending on the concentration and calcination temperature. However, these dopants can impart substantial stabilization. It was found that the degree of stabilization is strongly dependent on the calcination temperature of the material. In addition, we used synchrotron X-ray diffraction during thermal breakdown to better understand why the different dopants impact the thermal stability and confirm the stabilization effects of the dopants.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Advancements in Battery Materials · Advanced Battery Materials and Technologies · Advanced Battery Technologies Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Applied Materials Division, Argonne National Laboratory, 9700 S. Cass Ave., Lemont, Illinois 60439, United States
Chemical Sciences and Engineering Division, Argonne National Laboratory, 9700 S. Cass Ave., Lemont, Illinois 60439, United States
A123 Systems, LLC., 200 West Street Waltham, Massachusetts 02451, United States
Funding
A123 Systems LLC
References (35)
Show source-provided references
1. 10.1002/adma.20180056110.1002/adma.201800561 ↗
2. 10.1021/acs.jpcc.7b0612210.1021/acs.jpcc.7b06122 ↗
3. 10.1002/adma.20170557510.1002/adma.201705575 ↗
4. 10.1021/acs.chemmater.8b0382710.1021/acs.chemmater.8b03827 ↗
5. 10.1021/am506712c10.1021/am506712c ↗
6. 10.3390/en1109219110.3390/en11092191 ↗
7. 10.1016/j.applthermaleng.2018.09.01610.1016/j.applthermaleng.2018.09.016 ↗
8. 10.1016/j.matlet.2019.03.06410.1016/j.matlet.2019.03.064 ↗
9. 10.1016/j.jpowsour.2005.09.04710.1016/j.jpowsour.2005.09.047 ↗
10. 10.1016/j.electacta.2015.09.15110.1016/j.electacta.2015.09.151 ↗
11. 10.1039/c4dt01611d10.1039/c4dt01611d ↗
12. 10.1016/j.electacta.2004.07.03810.1016/j.electacta.2004.07.038 ↗
13. 10.1149/2.004302jes10.1149/2.004302jes ↗
14. 10.1016/j.jelechem.2019.02.05110.1016/j.jelechem.2019.02.051 ↗
15. 10.1038/s41598-018-21345-610.1038/s41598-018-21345-6 ↗
16. 10.1016/j.electacta.2015.11.09310.1016/j.electacta.2015.11.093 ↗
17. 10.1016/j.electacta.2016.01.03910.1016/j.electacta.2016.01.039 ↗
18. 10.1021/cm101716310.1021/cm1017163 ↗
19. 10.1021/acs.chemmater.7b0293010.1021/acs.chemmater.7b02930 ↗
20. 10.1039/c5cp03228h10.1039/c5cp03228h ↗
21. 10.1016/j.ceramint.2017.05.12910.1016/j.ceramint.2017.05.129 ↗
22. 10.1016/j.jpowsour.2018.06.07210.1016/j.jpowsour.2018.06.072 ↗
23. 10.1021/acsami.9b1390610.1021/acsami.9b13906 ↗
24. 10.1039/c5ee01254f10.1039/c5ee01254f ↗
25. 10.1149/2.0461906jes10.1149/2.0461906jes ↗
26. 10.1021/acsami.9b0038910.1021/acsami.9b00389 ↗
27. 10.1149/2.0651903jes10.1149/2.0651903jes ↗
28. 10.1016/j.electacta.2018.07.18310.1016/j.electacta.2018.07.183 ↗
29. 10.1021/acsami.8b0239610.1021/acsami.8b02396 ↗
30. 10.1021/acsenergylett.8b0080510.1021/acsenergylett.8b00805 ↗
31. 10.1002/adfm.20180882510.1002/adfm.201808825 ↗
32. 10.1002/aenm.20170202810.1002/aenm.201702028 ↗
33. 10.1021/acsami.7b1468410.1021/acsami.7b14684 ↗
34. 10.1107/s002188981300353110.1107/s0021889813003531 ↗
35. 10.1080/08957959.2015.105983510.1080/08957959.2015.1059835 ↗