Laser-Annealing and Solid-Phase Epitaxy of Selenium Thin-Film Solar Cells
Source abstract
Abstract
Selenium has resurged as a promising photovoltaic material in solar cell research due to its wide direct bandgap of 1.95 eV, making it a suitable candidate for a top cell in tandem photovoltaic devices. However, the optoelectronic quality of selenium thin-films has been identified as a key bottleneck for realizing high-efficiency selenium solar cells. In this study, we present an approach for crystallizing selenium thin-films using laser-annealing as an alternative to the conventionally used thermal annealing strategy. By laser-annealing through a semitransparent substrate, a buried layer of high-quality selenium crystallites is formed and used as a growth template for solid-phase epitaxy. The resulting selenium thin-films feature larger and more preferentially oriented grains with a negligible surface roughness in comparison to thermally annealed selenium thin-films. We fabricate photovoltaic devices using this strategy and demonstrate a record ideality factor of n = 1.37, a record fill factor of FF = 63.7%, and a power conversion efficiency of PCE = 5.0%. The presented laser-annealing strategy is universally applicable and is a promising approach for crystallizing a wide range of photovoltaic materials where high temperatures are needed while maintaining a low substrate temperature.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Chalcogenide Semiconductor Thin Films · Quantum Dots Synthesis And Properties · Advanced Semiconductor Detectors and Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
SurfCat, DTU Physics, Technical University of Denmark, DK-2800 Kgs. Lyngby, Denmark
DTU Nanolab, National Center for Nano Fabrication and Characterization, Technical University of Denmark, DK-2800 Kgs. Lyngby, Denmark
Funding
Danmarks Frie Forskningsfond
References (26)
Show source-provided references
1. 10.1038/nenergy.2017.14010.1038/nenergy.2017.140 ↗
2. 10.1002/ijch.20140021010.1002/ijch.201400210 ↗
3. 10.1088/2515-7655/abebca10.1088/2515-7655/abebca ↗
4. 10.1039/D2FD00132B10.1039/D2FD00132B ↗
5. 10.1016/j.mattod.2020.09.00210.1016/j.mattod.2020.09.002 ↗
6. 10.1007/s11426-022-1332-310.1007/s11426-022-1332-3 ↗
7. 10.1039/C8TC05873C10.1039/C8TC05873C ↗
8. 10.1002/solr.20210011110.1002/solr.202100111 ↗
9. 10.1021/acsaem.1c0170010.1021/acsaem.1c01700 ↗
10. 10.1038/s41467-017-00582-910.1038/s41467-017-00582-9 ↗
11. 10.1002/aenm.20180276610.1002/aenm.201802766 ↗
12. 10.1002/adma.20170514810.1002/adma.201705148 ↗
13. 10.1021/acsnano.6b0381510.1021/acsnano.6b03815 ↗
14. 10.1039/D2TA07729A10.1039/D2TA07729A ↗
15. 10.1016/0022-3697(68)90075-910.1016/0022-3697(68)90075-9 ↗
16. 10.1016/0022-3093(74)90153-710.1016/0022-3093(74)90153-7 ↗
17. 10.1143/JJAP.24.L53610.1143/JJAP.24.L536 ↗
18. 10.1039/C9EE02324K10.1039/C9EE02324K ↗
19. 10.1109/JPHOTOV.2019.293040910.1109/JPHOTOV.2019.2930409 ↗
20. 10.1088/0022-3719/11/1/01610.1088/0022-3719/11/1/016 ↗
21. 10.1039/D0CP00511H10.1039/D0CP00511H ↗
22. 10.1021/acsenergylett.9b0161910.1021/acsenergylett.9b01619 ↗
23. 10.1016/j.tsf.2009.09.16210.1016/j.tsf.2009.09.162 ↗
24. Nishinaga, T. Handbook of Crystal Growth: Bulk Crystal Growth, 2nd ed. Elsevier Inc., 2014; Vol. 2, pp 317–363.
25. 10.1038/s41560-023-01255-210.1038/s41560-023-01255-2 ↗
26. 10.1039/D0EE00291G10.1039/D0EE00291G ↗