journal article·2000-08

Emulsion processing of SOFC materials Ca0.3La0.7CrO3, Sr0.16La0.84CrO3, and Sr0.2La0.8MnO3

J. Ovenstone, C. B. Ponton

Journal of Materials Science· Volume 35· Issue 16
Publisher page

Abstract

A novel preparation route to the perovskite materials Ca0.3La0.7CrO3, Sr0.16La0.84CrO3, and Sr0.2La0.8MnO3 is described. The method produces the phase pure perovskite phases after calcination at 700°C for 2 hours. The powders produced are unagglomerated, and consist of hollow spherical particles 0.15 μm in diameter. EDX has shown that the careful control of reaction conditions is vital to control the phase composition, and that small changes in stoichiometry result in the production of unsinterable powder.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Magnetic and transport properties of perovskites and related materials · Advancements in Solid Oxide Fuel Cells · Thermal Expansion and Ionic Conductivity

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (15)

Show source-provided references
1. G. M. Christie, P. H. Middleton and B. C. H. Steele, J. Europ. Ceram. Soc. 14 (1994) 163.10.1016/0955-2219(94)90104-X ↗
2. M. R. Deguire, S. E. Dorris, R. B. Poeppel, S. Morisette and U. Balachandran, J. Mater. Res. 8(9) (1993) 2327.10.1557/JMR.1993.2327 ↗
3. P. H. Duvigneaud, P. Picate and F. Cambier, J. Europ. Ceram. Soc. 14 (1994) 359.10.1016/0955-2219(94)90073-6 ↗
4. K. Fukaya, S. Hayashi and H. Saito, J. Mater. Sci. Lett. 7 (1988) 457.10.1007/BF01730687 ↗
5. R. Koc and H. U. Anderson, J. Mater. Sci. 27 (1992) 5837.10.1007/BF01119747 ↗
6. N. Sakai, T. Kawada, H. Yokokawa and M. Dokiya, J. Ceram. Soc. Jap. 101(11) (1993) 1195.10.2109/jcersj.101.1195 ↗
7. N. Sakai, T. Kawada, H. Yokokawa, M. Dokiya and I. Kojima, J. Am. Ceram. Soc. 76(3) (1993) 609.10.1111/j.1151-2916.1993.tb03649.x ↗
8. Y. Takeda, Y. Sasaki, T. Ichikawa, N. Imanishi, O. Yamamoto, N. Mori and T. Abe, Solid State Ionics 72 (1994) 257.10.1016/0167-2738(94)90156-2 ↗
9. A. Chakraborty, P. Siyathadevi and H. S. Maiti, Mater. Lett. 20 (1994) 63.10.1016/0167-577X(94)90149-X ↗
10. J. H. Kuo, H. U. Anderson and D. M. Sparlin, J. Solid State Chem. 87 (1989) 52.10.1016/0022-4596(89)90053-4 ↗
11. N. Q. Minh, J. Am. Ceram. Soc. 76(3) (1993) 563.10.1111/j.1151-2916.1993.tb03645.x ↗
12. D. B. Meadowcroft and J. M. Wimmer, Ceram. Bull. 58 (1979) 610.
13. D. B. Meadowcroft, Brit. J. Appl. Phys. 2(2) (1969) 1225.
14. R. Arshady, Colloid Polym. Sci. 270 (1992) 717.10.1007/BF00776142 ↗
15. S. D. Ramamurthi, Z. Xu and D. A. Payne, J. Am. Ceram. Soc. 73 (1990) 2760.10.1111/j.1151-2916.1990.tb06761.x ↗