Preparation and Characterization of Pb(Zr, Ti)O3Thin Films by Metalorganic Chemical vapor Deposition Using a Solid Delivery System
Source abstract
Abstract
Pb(Zr, Ti)O3(PZT) thin films were deposited on Pt/SiO2/Si substrates by metalorganic chemical vapor deposition using solid delivery system. The effects of deposition parameters such as the substrate temperature, the concentration of Pb precursor in the precursor mixtures, and the reactor pressure on the structural and electrical properties of PZT thin films were investigated. To obtain single-phase PZT thin films, the optimal range of the substrate temperature should be between 600 and 650 °C. The PbO content in PZT thin films was proportional to the fraction of Pb in the precursor mixture below 550 °C, but it was independent of the fraction of Pb in the mixture above 600 °C. With the increment of the reactor pressure, Zr contents in PZT thin films were increased, and the Pb/(Zr + Ti) ratio became more stoichiometric so that the ferroelectric properties were improved.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Ferroelectric and Piezoelectric Materials · Acoustic Wave Resonator Technologies · Microwave Dielectric Ceramics Synthesis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (12)
Show source-provided references
1. 10.1063/1.33742310.1063/1.337423 ↗
2. Jones · Chem. Vap. Deposition · 1998 · 4 · 210.1002/(SICI)1521-3862(199810)04:05<169::AID-CVDE169>3.0.CO;2-6 ↗
3. 10.1557/JMR.1999.027710.1557/JMR.1999.0277 ↗
4. 10.1111/j.1151-2916.1995.tb08805.x10.1111/j.1151-2916.1995.tb08805.x ↗
5. 10.1038/374627a010.1038/374627a0 ↗
6. Shin · J. Korean Phys. Soc. · 1998 · 32 · S1529
7. 10.1116/1.58138710.1116/1.581387 ↗
8. Moulson · 1990 · 283
9. 10.1063/1.11055210.1063/1.110552 ↗
10. 10.1557/S088376940004606610.1557/S0883769400046066 ↗
11. 10.1063/1.34161310.1063/1.341613 ↗
12. Kim · 1996 · 433 · 213