article·2012-01-01Open access

Microstructure and barrier performance of Ta/Ti-Al integrated film used as a barrier layer for Cu metallization

Zhao Qing-xun

Open full text

Abstract

Cu(120nm)/Ta(5nm)/Ti-Al(5nm)/Si heterostructures were deposited on(001) Si substrates using radio frequency magnetron sputtering method.Microstructure of the samples and barrier performance of Ta(5nm)/Ti-Al(5nm) integrated film were investigated using atomic force microscopy(AFM),X-ray diffraction(XRD),and four probe method.No obvious impurity peaks can be found for the 850℃ annealed sample,indicating no evident reaction or inter diffusion happened at the interfaces of the sample during the high temperature annealing.Compared with 800℃ annealed sample,much rougher surface with sharp increase in root mean square roughness(RMS),coupled with a sudden increase in sheet resistance,implies Ta(5nm)/Ti-Al(5nm) integrated film cannot be used as a barrier up to annealing temperature of 850℃.Due to the good adhesion between Ta and Cu and good chemical stability of Ti-Al,Ta(5nm)/Ti-Al(5nm) integrated film has very good barrier performance at temperature lower than 800℃.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Copper Interconnects and Reliability · Semiconductor materials and interfaces · Electronic Packaging and Soldering Technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.